Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 50.0 kN/m | 285 pli | Die B, post cured- 8 hours at 200°C; ASTM D624 |
Multibase SILASTIC® Q7-4850 Dow-Corning Biomedical Grade Liquid Silicone Rubber Information provided by Multibase |
|||
Tear Strength | 50.0 kN/m | 285 pli | Die C, 2 in/min; ASTM D1004 |
PolyOne Geon™ Vinyl Flexible 90034 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Tear Strength | 50.0 kN/m | 285 pli | Die C, 2 in/min; ASTM D1004 |
PolyOne Geon™ Vinyl Flexible 90037 Polyvinyl Chloride, Flexible (PVC, Flexible) Automotive OEM approval(s).Information provided by PolyOne |
|||
Tear Strength | 50.0 kN/m | 286 pli | B-type, Vulcanized |
KKPC KOSYN 1507H Styrene Butadiene Rubber Styrene Butadiene RubberCharacteristics: KOSYN SBR, a useful synthetic rubber, is a copolymer made from butadiene and styrene by cold emulsion polymerization. It has superior abrasion resistance and.. |
|||
Tear Strength | >= 50.0 kN/m | >= 285 pli | DIN 53507 |
Karina 701D48/1-A-IS Black PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tear Strength | >= 50.0 kN/m | >= 285 pli | DIN 53507 |
Karina 722-48/1-A-IS Black PVC Compound Heavy metal free PVC compound recommended for extrusion of automobile profilesInformation provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tear Strength | 50.0 kN/m | 285 pli | Die B |
Momentive Performance Materials Siloprenâ„¢ LSR 2661 Liquid Silicone Rubber - Non Post Cure / Low Compression Set This LSR elastomer is a specialty grade, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera.. |
|||
Tear Strength | 50.0 kN/m | 285 pli | ISO 34B |
Huntsman AVALON® 65 AE Thermoplastic Polyurethane Introduction: AVALON 65 AE is a polyester based thermoplastic polyurethane for injection molding. AVALON 65 AE is part of the AVALON Soft Range and offers a premium soling material for casual, sport.. |
|||
Tear Strength | 50.0 kN/m | 286 pli | B-type, Vulcanized |
KKPC KOSYN 1502W Styrene Butadiene Rubber Styrene Butadiene RubberCharacteristics: KOSYN SBR, a useful synthetic rubber, is a copolymer made from butadiene and styrene by cold emulsion polymerization. It has superior abrasion resistance and.. |
|||
Tear Strength | 50.0 kN/m | 285 pli | |
Trelleborg R650 Natural Rubber Polyisoprene All information provided by Trelleborg |
|||
Tear Strength | 50.0 kN/m | 285 pli | ASTM D624 |
ELASTO UK Dryflex® 500850S SEBS Based Material, Unfilled Qualities, 85A Hardness, Translucent The 500-seriesis very favorable when transparency and good scratch resistance are required, as well as when there are high surface finish requirements. Unfilled grades have excellent flow and mecha.. |
|||
Tear Strength | 50.0 kN/m | 285 pli | ASTM D624 |
ELASTO UK Dryflex® 502850S SEBS Based Material, Unfilled Qualities, 85A Hardness, Black The 500-seriesis very favorable when transparency and good scratch resistance are required, as well as when there are high surface finish requirements. Unfilled grades have excellent flow and mecha.. |
|||
Tear Strength | 50.0 kN/m | 285 pli | ASTM D624 |
ELASTO UK Dryflex® 600900S SEBS Based Material, Filled Qualities, 90A Hardness, Natural The most significant features of the 600-series are the improved heat stability, the sound reduction and that the material enables an easy and secure pigmenting for the customer. A filled material .. |
|||
Tear Strength | 50.0 kN/m | 285 pli | ASTM D624 |
ELASTO UK Dryflex® 602900S SEBS Based Material, Filled Qualities, 90A Hardness, Black The most significant features of the 600-series are the improved heat stability, the sound reduction and that the material enables an easy and secure pigmenting for the customer. A filled material .. |
|||
Tear Strength | 50.0 kN/m | 285 pli | ASTM D624 |
ELASTO UK Dryflex® 660900S SEBS Based Material, Semi-Filled Qualities, 90A Hardness, Natural The 660-series is recommended when the properties of the produced detail requires the advantages of the 500-series in combination with the 600-series. A semi-filled material can therefore combine t.. |
|||
Tear Strength | 50.0 kN/m | 285 pli | ASTM D624 |
ELASTO UK Dryflex® 662900S SEBS Based Material, Semi-Filled Qualities, 90A Hardness, Black The 660-series is recommended when the properties of the produced detail requires the advantages of the 500-series in combination with the 600-series. A semi-filled material can therefore combine t.. |
|||
Tear Strength | 50.0 kN/m | 285 pli | Trouser Tear resistance MD; ISO 6383-1 |
EMS-Grivory Grivory® FG 34 NL nat 6023 PA6 Product description: Grilon FG 34 NL natural 6023 is a modified, medium viscosity polyamide 6. Grilon FG 34 NL natural 6023 exhibits following improvements compared to a PA 6: Better gas barrier pro.. |
|||
Tear Strength | 50.0 kN/m | 285 pli | Trouser Tear resistance TD; ISO 6383-1 |
EMS-Grivory Grivory® FG 34 NL nat 6023 PA6 Product description: Grilon FG 34 NL natural 6023 is a modified, medium viscosity polyamide 6. Grilon FG 34 NL natural 6023 exhibits following improvements compared to a PA 6: Better gas barrier pro.. |
|||
Tear Strength | 50.0 kN/m | 285 pli | Trouser Tear resistance TD; ISO 6383-1 |
EMS-Grivory Grivory® FG 40 NL nat 6021 PA6 Product description: Grilon FG 40 NL natural 6021 is a modified, high viscosity polyamide 6. As a result of the modification in comparison to conventional polyamide 6 Grilon FG40 NL natural 6021 off.. |
|||
Tear Strength | 50.0 kN/m | 285 pli | Trouser Tear resistance MD; ISO 6383-1 |
EMS-Grivory Grivory® FG 47 NL nat 6028 PA6 Product description: Grilon FG 47 NL natural 6028 is a modified, high viscosity Polyamide 6, which contains also slip and nucleating agents. Grilon FG 47 NL natural 6028 shows following improvements.. |
|||
Tear Strength | 50.0 kN/m | 285 pli | Trouser Tear resistance TD; ISO 6383-1 |
EMS-Grivory Grivory® FG 47 NL nat 6028 PA6 Product description: Grilon FG 47 NL natural 6028 is a modified, high viscosity Polyamide 6, which contains also slip and nucleating agents. Grilon FG 47 NL natural 6028 shows following improvements.. |
|||
Tear Strength | 50.0 kN/m | 285 pli | DIN ISO 34-1/Bb |
BASF Elastollan S 60 A SPF TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with excellent mechanical properties and wear resistance, good damping characteristics and a high resilience performance.Typical Applicat.. |
|||
Tear Strength | 50.0 - 70.0 kN/m | 285 - 399 pli | TM-019K |
AorTech Biomaterials Elast-Eon™ E5-325 Biomedical Polyurethane Pellets Elast-Eon™ 5-325 is a polyurethane with a 32.5% hard segment content and a mixed polyether/siloxane soft segment. It comes in pellet form. The pellets are colorless to yellowish and are soluble in .. |
|||
Tear Strength | >= 50.0 kN/m | >= 285 pli | ISO 34 |
Austin Novel Materials Texalan® 370A Polyester-based TPU Description: Good abrasion resistance, tensile strength, oil resistance which can be used in injection, extrusion purpose.Information from Dawnentech |
|||
Tear Strength | 50.0 - 70.0 kN/m | 285 - 399 pli | TM-019K |
AorTech Biomaterials Elast-Eon™ E5-325 Biomedical Polyurethane Pellets Elast-Eon™ 5-325 is a polyurethane with a 32.5% hard segment content and a mixed polyether/siloxane soft segment. It comes in pellet form. The pellets are colorless to yellowish and are soluble in .. |
|||
Tear Strength | 50.0 kN/m | 285 pli | DIN ISO 34-1/Bb |
BASF Elastollan B 60 A WHA TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with excellent mechanical properties, outstanding wear resistance, high tensile strength, good damping and resilience performance and sup.. |