Polymer Property : Tear Strength = 64.0 pli Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tear Strength 11.2 kN/m
64.0 pli
Die B; DCBP Cure
Shin-Etsu Silicones KE-571U Silicone Elastomer
KE571U is one of a series of easy processing, general purpose grade silicone rubber bases. It can be used in a variety of applications requiring finishing by molding or extruding with extending fill..
Tear Strength 11.2 kN/m
64.0 pli
Dow Corning SILASTIC® 37085-V SILICONE RUBBER BLACK
50 Durometer, peroxide cured, low compression set Silicone Rubber CompoundInformation provided by Dow Corning
Tear Strength 11.2 kN/m
64.0 pli
73°F, Die C; ASTM D624
ExxonMobil Santoprene® 8291-55PA Thermoplastic Elastomer  (discontinued **)
A soft, colorable, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is especially formulated to bond to PA-6 and blends thereof for applications where hard/s..