Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 12.0 - 71.0 kN/m | 68.5 - 405 pli | Average value: 33.9 kN/m Grade Count:5 |
Overview of materials for Polytetrafluoroethylene (PTFE), Glass Filled, Molded This property data is a summary of similar materials in the MatWeb database for the category "Polytetrafluoroethylene (PTFE), Glass Filled, Molded". Each property range of values reported is minimum.. |
|||
Tear Strength | 56.0 - 71.0 kN/m | 320 - 405 pli | NF EN ISO 1421 |
Isoflon Tisoflon® 14 AD Polytetrafluoroethylene Coated Glass Fabric PTFE coated glass fabric one side adhesive TISOFLON® - Standard gradeInformation provided by Isoflon. |
|||
Tear Strength | 56.0 - 71.0 kN/m | 320 - 405 pli | NF EN ISO 1421 |
Isoflon Tisoflon® 14G Polytetrafluoroethylene & Graphite Coated Glass Fabric PTFE + Graphite coated glass fabric TISOFLON® - Black anti-staticInformation provided by Isoflon. |