Mechanical Properties Metric English Comments
Flexural Strength 180 MPa

@Temperature -40.0 °C
26100 psi

@Temperature -40.0 °F
ISO 178
DuPont Performance Polymers Rynite® FR515 BK507 PET  (Unverified Data**)
Rynite® FR515 BK507 is a flame retardant 15% glass reinforced modified polyethtylene terephthalate. Recognized by UL as UL94V-0 at 0.8mm(0.03in). Has a 140C temp index. Excellent balance of electr..
Flexural Strength 180 MPa

@Temperature 175 °C
26100 psi

@Temperature 347 °F
ISO 178
Victrex® PEEK 90HMF20 Polyetheretherketone (PEEK), 20% Carbon Fiber Reinforced
Product Description: High performance thermoplastic material, 20% carbon fiber reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding, very easy flow, color black.T..
Flexural Strength 180 MPa

@Temperature 23.0 °C
26100 psi

@Temperature 73.4 °F
ISO 178
Victrex® PEEK -HT™ G22 PolyEtherKetone, Unreinforced
Product Description:High performance thermoplastic material, unreinforced PolyEtherKetone (PEK), semi crystalline, depth filtered granules for injection moulding, easy flow, FDA food contact complia..
Flexural Strength 180 MPa

@Temperature 125 °C
26100 psi

@Temperature 257 °F
ISO 178
Victrex® ST™ ST45GL30 Polyetherketoneetherketoneketone (PEKEKK), 30% Glass Fiber Reinforced
Product Description:High performance thermoplastic material, 30% glass fibre reinforced PolyEtherKetoneEtherKetoneKetone (PEKEKK), semi crystalline, granules for injection moulding, standard flow, c..
Flexural Strength 180 MPa

@Strain 5.00 %
26100 psi

@Strain 5.00 %
cond., 2 mm/min; ISO 178-A
Lanxess Durethan® BKV 35 H3.0 000000 Nylon 6, Glass Fiber Reinforced
PA 6, 35% glass fibers, injection molding, heat-aging stabilizedInformation provided by LANXESS.
Flexural Strength 180 MPa

@Temperature 23.0 °C
26100 psi

@Temperature 73.4 °F
Practical Use (Water Absorption 2.0%); ASTM-D790
Toyobo GLAMIDE® T-403 Nylon-6
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Flexural Strength 180 MPa

@Temperature 23.0 °C
26100 psi

@Temperature 73.4 °F
Absolute Drying; ASTM-D790
Toyobo GLAMIDE® T-521 Nylon-6
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Flexural Strength 180 MPa

@Temperature 80.0 °C
26100 psi

@Temperature 176 °F
Absolute Drying; ASTM-D790
Toyobo GLAMIDE® TY-791GT 6T-Nylon
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Flexural Strength 180 MPa

@Temperature 23.0 °C
26100 psi

@Temperature 73.4 °F
Absolute Drying; ASTM-D790
Toyobo GLAMIDE® T-401 Nylon-6
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..