Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 10.34 MPa @Temperature 177 °C |
1500 psi @Temperature 350 °F |
2 hr soak, 90 min @ 350°F, Spring Clamp Pressure, FPL Acid Etched 6061-T6; ASTM D1002 |
Zyvex Performance Materials Aroply™ 350 Nano-Engineered Composite Film Adhesive Aroply™ 350 Film Adhesive is a versatile, heat curing carbon-nanotube modified epoxy structural film adhesive available in a variety of film weights on a supported carrier. Cured adhesive character.. |