Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 68.9 MPa @Temperature 210 °C |
10000 psi @Temperature 410 °F |
In-plane, Wet; SACMA SRM 7R-94 |
Renegade Materials Corporation MVK-16 Polyimide FreeForm™ T650-35-3K-UC309-8HS Carbon Fabric MVK-16 is a low-cost polyimide prepreg system developed for long-term, continuous service temperature at 375 – 450°F. MVK-16 exhibits excellent retention of high-temperature mechanical properties .. |
|||
Shear Strength | 68.9 MPa @Temperature 104 °C |
10000 psi @Temperature 220 °F |
0° Short Beam, Dry |
Hexcel® HexPly® 8552 Epoxy Matrix, SGP196-PW Fiber Information provided by HexCel |
|||
Shear Strength | 68.9 MPa @Temperature 25.0 °C |
10000 psi @Temperature 77.0 °F |
0° Short Beam, Wet |
Hexcel® HexPly® 8552 Epoxy Matrix, A280-5H Fiber Information provided by HexCel |
|||
Shear Strength | 69.0 MPa @Temperature 23.0 °C |
10000 psi @Temperature 73.4 °F |
0°, Interlaminar, Conditioning: 23°C; ASTM D2344 |
Hexcel® HexPly® M49 120°C Curing Epoxy Matrix, 6K High Strength Carbon Fiber Designation: C370S5, Satin weave, 5HInformation provided by HexCel |