Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Strength 71.7 MPa

@Temperature 21.1 °C
10400 psi

@Temperature 70.0 °F
Short-Beam, Dry; Vacuum/Oven Cured; ASTM D2344
Park Electrochemical Nelcote® E-765 Epoxy Prepreg, T300 3K PW Reinforced
Nelcote® E-765 is a tough 250°F cure prepreg system designed to replace 350°F cure systems in aircraft structural applications. FAA-approved Design Allowable Databases are available upon request...
Shear Strength 71.7 MPa

@Temperature 82.2 °C
10400 psi

@Temperature 180 °F
Beam, V-Notched; Wet; Autoclave Cured; ASTM D5379-93
Park Electrochemical Nelcote® E-765 Epoxy Prepreg, T300 6K 5HS Reinforced
Nelcote® E-765 is a tough 250°F cure prepreg system designed to replace 350°F cure systems in aircraft structural applications. FAA-approved Design Allowable Databases are available upon request...
Shear Strength 71.7 MPa

@Temperature 71.1 °C
10400 psi

@Temperature 160 °F
0° Short Beam, Wet
Hexcel® HexPly® 8552 Epoxy Matrix, A193-PW Fiber
Information provided by HexCel
Shear Strength 71.7 MPa

@Temperature 23.0 °C
10400 psi

@Temperature 73.4 °F
Hexcel® HexPly® 954-2A Curing Cyanate Resin, Quartz Fiber Reinforced 8 Harness Satin Fabric
Information provided by HexCel
Shear Strength 72.0 MPa

@Temperature 24.0 °C
10400 psi

@Temperature 75.2 °F
Short Beam
Hexcel® HexPly® F263 Epoxy Resin, F3T584 Carbon Fabric
Hexcel designation: F3T584-42"-F263; Fiber: T300 CelionInformation provided by HexCel
Shear Strength 72.0 MPa

@Temperature 132 °C
10400 psi

@Temperature 270 °F
Short Beam
Hexcel® HexPly® F263 Epoxy Resin, T3T145 Carbon Tape
Hexcel designation: T_145-12"-F263; Various fibersInformation provided by HexCel
Shear Strength 72.0 MPa

@Temperature -54.0 °C
10400 psi

@Temperature -65.2 °F
Short Beam
Hexcel® HexPly® F263 Epoxy Resin, W3T282 Carbon Fabric
Hexcel designation: W3T282-42"-F263; Fiber: T300 CelionInformation provided by HexCel
Shear Strength 71.7 MPa

@Temperature 71.0 °C
10400 psi

@Temperature 160 °F
Short Beam, 1/2 hr
Hexcel® HexPly® F515 Epoxy Resin, T5A120 Carbon Tape
Hexcel designation: TXX120-12"-F515; Fiber: IM6Information provided by HexCel
Shear Strength 71.7 MPa

@Temperature 232 °C
10400 psi

@Temperature 450 °F
Short Beam; 424 Hrs
Hexcel® HexPly® F650 Bismaleimide Resin with T300 Fiber
Thermal Aging at 232°C; Composition T300 Fiber, 6K, UD Tape - 148 g/m2; Laminate Physicals: 32.7% Resin content, 60.0% Fiber volumeInformation provided by HexCel
Shear Strength 72.0 MPa

@Temperature 177 °C
10400 psi

@Temperature 351 °F
IM7 (12K); [+/- 45°]2s; In Plane; Wet condition
Hexcel® HexPly® M65 Bismaleimide Resin, Carbon Tape Form
Fiber: IM7-12KInformation provided by HexCel
Shear Strength 71.7 MPa

@Temperature 177 °C
10400 psi

@Temperature 351 °F
Autoclave Cured; [+/- 45°]2s
Hexcel® HexPly® F652 Bismaleimide Resin, Carbon Tape Form
Material Description: T6T145; Fiber: T300-6KInformation provided by HexCel