Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 75.2 MPa @Temperature 21.1 °C |
10900 psi @Temperature 70.0 °F |
Short-Beam, Dry; Vacuum/Oven Cured; ASTM D2344 |
Park Electrochemical Nelcote® E-765 Epoxy Prepreg, T300 6K 5HS Reinforced Nelcote® E-765 is a tough 250°F cure prepreg system designed to replace 350°F cure systems in aircraft structural applications. FAA-approved Design Allowable Databases are available upon request... |
|||
Shear Strength | 75.2 MPa @Temperature 21.1 °C |
10900 psi @Temperature 70.0 °F |
Inter-laminar, Wet; SACMA SRM 7R-94 |
Renegade Materials Corporation MVK-16 Polyimide FreeForm™ T650-35-3K-UC309-8HS Carbon Fabric MVK-16 is a low-cost polyimide prepreg system developed for long-term, continuous service temperature at 375 – 450°F. MVK-16 exhibits excellent retention of high-temperature mechanical properties .. |
|||
Shear Strength | 75.2 MPa @Temperature 25.0 °C |
10900 psi @Temperature 77.0 °F |
0° Short Beam, Wet |
Hexcel® HexPly® 8552 Epoxy Matrix, A193-PW Fiber Information provided by HexCel |
|||
Shear Strength | 75.2 MPa @Temperature 23.0 °C |
10900 psi @Temperature 73.4 °F |
|
Hexcel® HexPly® 954-2A Curing Cyanate Resin, S-2 Glass Fiber Reinforced 8 Harness Satin Fabric Information provided by HexCel |
|||
Shear Strength | 75.0 MPa @Temperature 132 °C |
10900 psi @Temperature 270 °F |
Short Beam |
Hexcel® HexPly® F263 Epoxy Resin, T3T095 Carbon Tape Hexcel designation: T_095-12"-F263; Various fibersInformation provided by HexCel |