Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 80.9 MPa @Temperature 23.0 °C |
11700 psi @Temperature 73.4 °F |
|
Hexcel® HexPly® M65 Bismaleimide Resin, Carbon Tape Form Fiber: IM7-12KInformation provided by HexCel |
|||
Shear Strength | 80.7 MPa @Temperature 25.0 °C |
11700 psi @Temperature 77.0 °F |
Fill Short Beam, Dry |
Hexcel® HexPly® 8552 Epoxy Matrix, A280-5H Fiber Information provided by HexCel |
|||
Shear Strength | 81.0 MPa @Temperature 23.0 °C |
11700 psi @Temperature 73.4 °F |
0º Interlaminar Shear, Conditioning: 23°C; ASTM D2344 |
Hexcel® HexPly® M47 140°C Curing Epoxy Matrix, Unidirectional Carbon Prepreg M46J Fibre 1947 - 38% resin weight with M46J 52.5% fiber volumeInformation provided by HexCel |