Mechanical Properties Metric English Comments
Shear Strength 12.1 MPa

@Temperature 60.0 °C
1750 psi

@Temperature 140 °F
Arovex (abraded), with Arovex Carbon Fiber Epoxy Laminate
Zyvex Performance Materials Epovex™ Nano-Engineered Composite Epoxy Adhesive Paste
Epovex® Adhesive Paste is a carbon nanotube enhanced two part epoxy adhesive thixotropic paste. Used for bonding or filling, Epovex Paste is ideal for many metals, woods, masonry products, and some..
Shear Strength 12.1 MPa

@Temperature 23.0 °C
1750 psi

@Temperature 73.4 °F
Overlap, Polycarbonate
3M Scotch-Weld™ TE030 Polyurethane Reactive Adhesive
3M™ Scotch-Weld™ Polyurethane Reactive Adhesives are a family of one-component, moisture curing, urethane adhesives. These adhesives are applied warm and bond a wide variety of substrates such as ..
Shear Strength 12.1 MPa

@Temperature 23.0 °C
1760 psi

@Temperature 73.4 °F
Overlap, PVC, Substrate Failure
3M Scotch-Weld™ TE030 Polyurethane Reactive Adhesive
3M™ Scotch-Weld™ Polyurethane Reactive Adhesives are a family of one-component, moisture curing, urethane adhesives. These adhesives are applied warm and bond a wide variety of substrates such as ..
Shear Strength 12.1 - 12.4 MPa

@Temperature 23.0 °C
1750 - 1800 psi

@Temperature 73.4 °F
Overlap FR-4/FR-4 (MEK Wiped); ASTM D1002-72
3M Scotch-Weld™ DP270 Black Structural Adhesive
Rigid potting compound, Non-corrosiveInformation provided by 3M
Shear Strength 12.1 - 12.4 MPa

@Temperature 23.0 °C
1750 - 1800 psi

@Temperature 73.4 °F
Overlap FR-4/FR-4 (MEK Wiped); ASTM D1002-72
3M Scotch-Weld™ DP270 Clear Structural Adhesive
Rigid potting compound, Non-corrosiveInformation provided by 3M
Shear Strength 12.1 MPa

@Temperature 23.0 °C
1760 psi

@Temperature 73.4 °F
Overlap, Polycarbonate
3M Scotch-Weld™ TE015 Polyurethane Reactive Adhesive
3M™ Scotch-Weld™ Polyurethane Reactive Adhesives are a family of one-component, moisture curing, urethane adhesives. These adhesives are applied warm and bond a wide variety of substrates such as ..