Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 82.7 MPa @Temperature 21.1 °C |
12000 psi @Temperature 70.0 °F |
In-Plane, Dry; ASTM D790 |
Renegade Materials Corporation MVK-14 Polyimide FreeForm™ T650-35 8HS Carbon Fabric MVK-14 polyimide prepregs are a more affordable and easier-to-process, non-carcinogenic alternative to PMR-15 and other older polyimide chemistries. MVK-14 offers a more durable alternative to high-.. |
|||
Shear Strength | 82.7 MPa @Temperature 82.0 °C |
12000 psi @Temperature 180 °F |
Short Beam, Wet |
Hexcel® HexPly® 8551-7 Epoxy Matrix, AS4 Fiber Information provided by HexCel |