Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 22.1 MPa @Temperature 23.9 °C |
3200 psi @Temperature 75.0 °F |
tensile lap, aluminum to aluminum |
Master Bond EP17HT One component epoxy system for bonding, sealing, coating and casting Product Description: Master Bond EP17HT is an one component, heat cured epoxy system for bonding, sealing, coating and encapsulating. It features good physical properties, electrical insulation prof.. |
|||
Shear Strength | 22.1 MPa @Temperature 23.9 °C |
3200 psi @Temperature 75.0 °F |
tensile lap, aluminum to aluminum |
Master Bond EP17HT-LO One component epoxy system for bonding, sealing, coating and casting Product Description: Master Bond EP17HT-LO is a one component, heat cured epoxy system for bonding, sealing, coating and encapsulating. It features good physical properties, electrical insulation pr.. |
|||
Shear Strength | 22.1 MPa @Temperature 23.9 °C |
3200 psi @Temperature 75.0 °F |
Cure cycle: 3 days @ RT, with Aced Etched 6061-T6 Aluminum |
Zyvex Performance Materials Epovex™ Nano-Engineered Composite Epoxy Adhesive Liquid Epovex® Adhesive is a carbon nanotube enhanced ambient or elevated temperature cure two-part epoxy adhesive. Used for bonding, laminating, filling or potting, Epovex is ideal for many metals, woods.. |
|||
Shear Strength | 22.1 MPa @Temperature 149 °C |
3200 psi @Temperature 300 °F |
Single Lap Shear (Metal/Metal), 0.03 psf, No conditioning |
Hexcel® Redux® 330M Epoxy film adhesives for the bonding and finishing of composites Redux 330 is a 350°F curing tough film adhesive which is ideally suited to structural bonding, composite to composite bonding, surface finishing, electromagnetic shielding and lightning strike appl.. |
|||
Shear Strength | 22.1 MPa @Temperature 24.0 °C |
3200 psi @Temperature 75.2 °F |
Overlap |
3M Scotch-Weld™ EC2216 Structural Adhesive High Performance, Very flexible bondsInformation provided by 3M |