Polymer Property : Shear Strength = 2880 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Strength 19.9 MPa

@Temperature 23.9 °C
2880 psi

@Temperature 75.0 °F
Cure cycle: 7 days @ RT (+7 days ethyl alcohol soak), with Aced Etched 6061-T6 Aluminum
Zyvex Performance Materials Epovex™ Nano-Engineered Composite Epoxy Adhesive Liquid
Epovex® Adhesive is a carbon nanotube enhanced ambient or elevated temperature cure two-part epoxy adhesive. Used for bonding, laminating, filling or potting, Epovex is ideal for many metals, woods..