Mechanical Properties Metric English Comments
Shear Strength 31.0 MPa

@Temperature 177 °C
4500 psi

@Temperature 350 °F
Short-Beam, Dry, Autoclave; ASTM D2344
Park Electrochemical Nelcote® E-746 Epoxy Prepreg, 3k 5HS Carbon Reinforced
Nelcote® E-746 is a modified epoxy resin system designed to retain excellent mechanical properties after extended exposure to high temperature. E-746 has a proven history in many demanding aerospac..
Shear Strength 31.0 MPa

@Temperature 177 °C
4500 psi

@Temperature 350 °F
Short-Beam, Dry, Autoclave with Post-Cure; ASTM D2344
Park Electrochemical Nelcote® E-746 Epoxy Prepreg, 581 Quartz Reinforced
Nelcote® E-746 is a modified epoxy resin system designed to retain excellent mechanical properties after extended exposure to high temperature. E-746 has a proven history in many demanding aerospac..
Shear Strength 31.0 MPa

@Temperature -55.0 °C
4500 psi

@Temperature -67.0 °F
Lap Shear, Cured at 250°C for 60 min at 30 psi MMM-A-132 and MIL-A-25463.
Hexcel® Redux® 382H (0.06 psf) Film Adhesive
Redux 382H is a 250°F curing modified epoxy film adhesive available in both supported and unsupported versions. Redux 382H is a versatile adhesive system suitable for bonding a wide variety of subs..
Shear Strength 31.0 MPa

@Temperature 21.1 °C
4500 psi

@Temperature 70.0 °F
Lap Shear
Hexcel® Redux® 609 (0.04 psf) Adhesive film for bonding metallic and composite components
Redux 609 is a 250°F curing modified epoxy film adhesive containing a cottom scrim for easy handling and glue-line thickness control. It is available at standard areal weights of 0.06 psf and 0.04 ..
Shear Strength 31.0 MPa

@Temperature 48.9 °C
4500 psi

@Temperature 120 °F
Lap Shear
Hexcel® Redux® 609 (0.04 psf) Adhesive film for bonding metallic and composite components
Redux 609 is a 250°F curing modified epoxy film adhesive containing a cottom scrim for easy handling and glue-line thickness control. It is available at standard areal weights of 0.06 psf and 0.04 ..
Shear Strength 31.0 MPa

@Temperature 48.9 °C
4500 psi

@Temperature 120 °F
Lap Shear
Hexcel® Redux® 609 (0.06 psf) Adhesive film for bonding metallic and composite components
Redux 609 is a 250°F curing modified epoxy film adhesive containing a cottom scrim for easy handling and glue-line thickness control. It is available at standard areal weights of 0.06 psf and 0.04 ..
Shear Strength 31.0 MPa

@Temperature 21.1 °C
4500 psi

@Temperature 70.0 °F
Tensile Shear, Redux 775 Liquid & Powder (P:L Ration = 1.3:1)
Hexcel® Redux® 775 Vinyl phenolic structural adhesive
Redux 775 was adopted as the world's first metal-to-metal bonding process to be officially approved for use in the manufacture of aircraft primary structures in 1943. It is available either as a fil..
Shear Strength 31.0 MPa

@Temperature 24.0 °C
4500 psi

@Temperature 75.2 °F
Aluminum Overlap
3M Scotch-Weld™ 2214 Hi-Dense Epoxy Adhesive
3M™ Scotch-Weld™ Adhesive 2214 Hi-Dense is a deareted version of Scotch-Weld adhesive 2214 regular for use where a very dense, void free bondline is required. One part 250°F (121°C) curing 100% ..
Shear Strength 31.0 MPa

@Temperature 82.0 °C
4500 psi

@Temperature 180 °F
Aluminum Overlap
3M Scotch-Weld™ 2214 Hi-Dense Epoxy Adhesive
3M™ Scotch-Weld™ Adhesive 2214 Hi-Dense is a deareted version of Scotch-Weld adhesive 2214 regular for use where a very dense, void free bondline is required. One part 250°F (121°C) curing 100% ..
Shear Strength 31.0 MPa

@Temperature 82.0 °C
4500 psi

@Temperature 180 °F
Aluminum Overlap
3M Scotch-Weld™ 2214 Non-Metallic Filled Epoxy Adhesive
3M™ Scotch-Weld™ Non-Metallic Filled is a non-metal filled version of Scotch-Weld adhesive 2214 regular. One part 250°F (121°C) curing 100% solids, 3M™ Scotch-Weld™ Epoxy Adhesive 2214 is a pa..
Shear Strength 31.0 MPa

@Temperature 82.0 °C
4500 psi

@Temperature 180 °F
Overlap
3M Scotch-Weld™ 1386 One-Part Epoxy Adhesives and Metal Primer
High Temperature strength and Impact resistanceInformation provided by 3M
Shear Strength 31.0 MPa

@Temperature 24.0 °C
4500 psi

@Temperature 75.2 °F
Aluminum Overlap
3M Scotch-Weld™ 2214 Regular Epoxy Adhesive
3M™ Scotch-Weld™ Adhesive 2214 Regular is an aluminum filled general purpose product for use in applications where high strength bonds are needed in a temperature range of -53-121°C.One part 250°..
Shear Strength 31.0 MPa

@Temperature 82.0 °C
4500 psi

@Temperature 180 °F
Aluminum Overlap
3M Scotch-Weld™ 2214 Regular Epoxy Adhesive
3M™ Scotch-Weld™ Adhesive 2214 Regular is an aluminum filled general purpose product for use in applications where high strength bonds are needed in a temperature range of -53-121°C.One part 250°..