Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 21.4 MPa @Temperature 23.9 °C |
3100 psi @Temperature 75.0 °F |
Cure cycle: 7 days @ RT (+7 days ethyl alcohol soak), with Aced Etched 6061-T6 Aluminum |
Zyvex Performance Materials Epovex™ Nano-Engineered Composite Epoxy Adhesive Paste Epovex® Adhesive Paste is a carbon nanotube enhanced two part epoxy adhesive thixotropic paste. Used for bonding or filling, Epovex Paste is ideal for many metals, woods, masonry products, and some.. |
|||
Shear Strength | 21.4 MPa @Temperature 23.9 °C |
3100 psi @Temperature 75.0 °F |
Cure cycle: 7 days @ RT (+7 days gasoline soak) , with Aced Etched 6061-T6 Aluminum |
Zyvex Performance Materials Epovex™ Nano-Engineered Composite Epoxy Adhesive Paste Epovex® Adhesive Paste is a carbon nanotube enhanced two part epoxy adhesive thixotropic paste. Used for bonding or filling, Epovex Paste is ideal for many metals, woods, masonry products, and some.. |
|||
Shear Strength | 21.4 MPa @Temperature 23.0 °C |
3100 psi @Temperature 73.4 °F |
Overlap, FRP |
3M Scotch-Weld™ TE230 Black Polyurethane Reactive Adhesive 3M™ Scotch-Weld™ Polyurethane Reactive Adhesives are a family of one-component, moisture curing, urethane adhesives. These adhesives are applied warm and bond a wide variety of substrates such as .. |