Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 25.5 MPa @Temperature 26.7 °C |
3700 psi @Temperature 80.0 °F |
ASTM D732 |
Greene Tweed Avalon® 1 PTFE Products made from Avalon® thermoplastics are constructed from proprietary high-performance reinforced PTFE material. Greene, Tweeds Avalon thermoplastics, available in grades ranging from virgin.. |
|||
Shear Strength | 25.5 MPa @Temperature 23.9 °C |
3700 psi @Temperature 75.0 °F |
Arovex (abraded) (+7 days water soak), with Arovex Carbon Fiber Epoxy Laminate |
Zyvex Performance Materials Epovex™ Nano-Engineered Composite Epoxy Adhesive Paste Epovex® Adhesive Paste is a carbon nanotube enhanced two part epoxy adhesive thixotropic paste. Used for bonding or filling, Epovex Paste is ideal for many metals, woods, masonry products, and some.. |
|||
Shear Strength | 25.5 MPa @Temperature 23.9 °C |
3700 psi @Temperature 75.0 °F |
Cure cycle: 3 days @ RT, with Aced Etched 6061-T6 Aluminum |
Zyvex Performance Materials Epovex™ Nano-Engineered Composite Epoxy Adhesive Paste Epovex® Adhesive Paste is a carbon nanotube enhanced two part epoxy adhesive thixotropic paste. Used for bonding or filling, Epovex Paste is ideal for many metals, woods, masonry products, and some.. |
|||
Shear Strength | 25.5 MPa @Temperature 24.0 °C |
3700 psi @Temperature 75.2 °F |
Overlap |
3M Scotch-Weld™ 1469 One-Part Epoxy Adhesives and Metal Primer High Temperature strength and Low ViscosityInformation provided by 3M |
|||
Shear Strength | 25.5 MPa @Temperature 82.0 °C |
3700 psi @Temperature 180 °F |
Overlap |
3M Scotch-Weld™ 1469 One-Part Epoxy Adhesives and Metal Primer High Temperature strength and Low ViscosityInformation provided by 3M |
|||
Shear Strength | 25.5 MPa @Temperature -43.0 °C |
3700 psi @Temperature -45.4 °F |
with Scotch-Weld EW-5000; ASTM D1002-10 |
3M Scotch-Weld™ EC-2815 B/A FR Epoxy Adhesive 3M Scotch-Weld Epoxy Adhesive EC-2815 B/A FR is a two-component epoxy adhesive with cure at room temperature or with additional heat to form a tough, impact-resistant bond. It has excellent adhesion.. |