Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 29.0 MPa @Temperature 71.1 °C |
4200 psi @Temperature 160 °F |
Short-Beam, Wet; ASTM D2344 |
Park Electrochemical Nelcote® E-761 Epoxy Prepreg, 285 Kevlar® Reinforced Nelcote® E-761 is a versatile self-adhesive epoxy matrix for use in aerospace and commercial application where ease of processing and cost are key considerations.Key Features and Benefits:Controlle.. |
|||
Shear Strength | 28.96 MPa @Temperature 21.1 °C |
4200 psi @Temperature 70.0 °F |
90 min @ 350°F, Spring Clamp Pressure, FPL Acid Etched 6061-T6; ASTM D1002 |
Zyvex Performance Materials Aroply™ 350 Nano-Engineered Composite Film Adhesive Aroply™ 350 Film Adhesive is a versatile, heat curing carbon-nanotube modified epoxy structural film adhesive available in a variety of film weights on a supported carrier. Cured adhesive character.. |