Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 69.6 MPa @Temperature 21.1 °C |
10100 psi @Temperature 70.0 °F |
Inter-laminar, Dry; SACMA SRM 7R-94 |
Renegade Materials Corporation MVK-16 Polyimide FreeForm™ T650-35-3K-UC309-8HS Carbon Fabric MVK-16 is a low-cost polyimide prepreg system developed for long-term, continuous service temperature at 375 – 450°F. MVK-16 exhibits excellent retention of high-temperature mechanical properties .. |
|||
Shear Strength | 69.6 MPa @Temperature 71.0 °C |
10100 psi @Temperature 160 °F |
Short Beam, 1/2 hr |
Hexcel® F515 Epoxy Resin, TXX200 Carbon Tape STD MOD FiberInformation provided by HexCel |