Mechanical Properties Metric English Comments
Shear Strength 75.8 MPa

@Temperature 177 °C
11000 psi

@Temperature 350 °F
In-plane, Wet; SACMA SRM 7R-94
Renegade Materials Corporation MVK-16 Polyimide FreeForm™ T650-35-3K-UC309-8HS Carbon Fabric
MVK-16 is a low-cost polyimide prepreg system developed for long-term, continuous service temperature at 375 – 450°F. MVK-16 exhibits excellent retention of high-temperature mechanical properties ..
Shear Strength 75.8 MPa

@Temperature 71.0 °C
11000 psi

@Temperature 160 °F
Short Beam, 1/2 hr
Hexcel® HexPly® F515 Epoxy Resin, T2C120 Carbon Tape
Hexcel designation: TXX120-12"-F515; Fiber: Toho® G30/500Information provided by HexCel