Mechanical Properties Metric English Comments
Shear Strength 82.7 MPa

@Temperature 21.1 °C
12000 psi

@Temperature 70.0 °F
In-Plane, Dry; ASTM D790
Renegade Materials Corporation MVK-14 Polyimide FreeForm™ T650-35 8HS Carbon Fabric
MVK-14 polyimide prepregs are a more affordable and easier-to-process, non-carcinogenic alternative to PMR-15 and other older polyimide chemistries. MVK-14 offers a more durable alternative to high-..
Shear Strength 82.7 MPa

@Temperature 82.0 °C
12000 psi

@Temperature 180 °F
Short Beam, Wet
Hexcel® HexPly® 8551-7 Epoxy Matrix, AS4 Fiber
Information provided by HexCel