Mechanical Properties Metric English Comments
Shear Modulus 0.0250 GPa

@Temperature 200 °C
3.63 ksi

@Temperature 392 °F
ISO 6721
BASF Ultrason S 2010 G4 20% Glass Filled PSU
Ultrason S 2010 G4 is a 20% glass reinforced, medium viscosity injection molding PSU grade with high rigidity and strength.
Shear Modulus 0.0250 GPa

@Temperature 200 °C
3.63 ksi

@Temperature 392 °F
ISO 6721
BASF Ultrason S 2010 G6 30% Glass Filled PSU
Ultrason S 2010 G6 is a 30% glass reinforced, medium viscosity injection molding PSU grade with high rigidity and strength.
Shear Modulus 0.0250 GPa

@Temperature 200 °C
3.63 ksi

@Temperature 392 °F
ISO 6721
BASF Ultrason S 2010 PSU
Ultrason S 2010 is an unreinforced, medium viscosity standard injection molding PSU grade. It flows readily and offers outstanding heat resistance and dimensional stability. It conforms to FDA req..
Shear Modulus 0.0250 GPa

@Temperature 200 °C
3.63 ksi

@Temperature 392 °F
ISO 6721
BASF Ultrason S 3010 PSU
Ultrason S 3010 is an unreinforced, higher viscosity injection molding and extrusion PSU grade, tougher and with improved chemical resistance. It conforms to FDA requirements of 21 CFR 177.1655.