Mechanical Properties Metric English Comments
Shear Modulus 0.950 GPa

@Temperature 100 °C
138 ksi

@Temperature 212 °F
ISO 6721
BASF Ultrason E 6020 P PES
Ultrason E 6020 P is an unfilled, injection molding PES grade. Polyethersulfone flakes of high molecular weight and good solubility in typical solvents (N-Methylpyrrolidone, Dimethylacetamide, Dichl..
Shear Modulus 0.950 GPa

@Temperature 50.0 °C
138 ksi

@Temperature 122 °F
ISO 6721
BASF Ultrason S 2010 G4 20% Glass Filled PSU
Ultrason S 2010 G4 is a 20% glass reinforced, medium viscosity injection molding PSU grade with high rigidity and strength.
Shear Modulus 0.950 GPa

@Temperature 50.0 °C
138 ksi

@Temperature 122 °F
ISO 6721
BASF Ultrason S 2010 G6 30% Glass Filled PSU
Ultrason S 2010 G6 is a 30% glass reinforced, medium viscosity injection molding PSU grade with high rigidity and strength.
Shear Modulus 0.950 GPa

@Temperature 50.0 °C
138 ksi

@Temperature 122 °F
ISO 6721
BASF Ultrason S 2010 PSU
Ultrason S 2010 is an unreinforced, medium viscosity standard injection molding PSU grade. It flows readily and offers outstanding heat resistance and dimensional stability. It conforms to FDA req..
Shear Modulus 0.950 GPa

@Temperature 100 °C
138 ksi

@Temperature 212 °F
ISO 6721
BASF Ultrason® E 2010 C6 30% Carbon Filled
Carbon fibers and Ultrason® two partners with good properties. The combination of carbon fibers with the amorphous high-temperature plastic Ultrason® guarantees mechanical properties for temperatu..
Shear Modulus 0.950 GPa

@Temperature 100 °C
138 ksi

@Temperature 212 °F
ISO 6721
BASF Ultrason E 1010 PES
Ultrason E 1010 is an unreinforced, low viscosity injection molding PES grade. It flows readily and offers outstanding heat resistance and dimensional stability.
Shear Modulus 0.950 GPa

@Temperature 100 °C
138 ksi

@Temperature 212 °F
ISO 6721
BASF Ultrason E 2010 G4 20% Glass Filled PES
Ultrason E 2010 G4 is a 20% glass reinforced, medium viscosity injection molding PES grade with high rigidity and strength.
Shear Modulus 0.950 GPa

@Temperature 100 °C
138 ksi

@Temperature 212 °F
ISO 6721
BASF Ultrason E 2010 G6 30% Glass Filled PES
Ultrason E 2010 G6 is a 30% glass reinforced, medium viscosity injection molding PES grade with high rigidity and strength.
Shear Modulus 0.950 GPa

@Temperature 100 °C
138 ksi

@Temperature 212 °F
ISO 6721
BASF Ultrason E 2010 PES
Ultrason E 2010 is an unreinforced, medium viscosity standard injection molding PES grade. It flows readily and offers outstanding heat resistance and dimensional stability. It conforms to FDA req..
Shear Modulus 0.950 GPa

@Temperature 100 °C
138 ksi

@Temperature 212 °F
ISO 6721
BASF Ultrason E 3010 PES
Ultrason E 3010 is an unfilled, higher viscosity injection molding and extrusion PES grade, tougher and with improved chemical resistance.
Shear Modulus 0.950 GPa

@Temperature 50.0 °C
138 ksi

@Temperature 122 °F
ISO 6721
BASF Ultrason S 3010 PSU
Ultrason S 3010 is an unreinforced, higher viscosity injection molding and extrusion PSU grade, tougher and with improved chemical resistance. It conforms to FDA requirements of 21 CFR 177.1655.
Shear Modulus 0.950 GPa

@Temperature 100 °C
138 ksi

@Temperature 212 °F
ISO 6721
BASF Ultrason E 2020 P PES
Ultrason E 2020 P is an unfilled, injection molding PES grade. Polyethersulfone flakes, for solvent based processes; product is soluble e.g. in N-Methylpyrrolidone and N,N-Dimethylacetamide.