Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Modulus | 0.800 GPa @Temperature 200 °C |
116 ksi @Temperature 392 °F |
|
Akro-Plastic Akromid® T1 GF 50 (3101) PPA Dry, 50% Glass Filled The new AKROMID® T is characterized primarily by high heat resistance and the lowest moisture absorption of the three PA grades, making it particularly well-suited in the automotive sector for high.. |
|||
Shear Modulus | 0.800 GPa @Temperature 175 °C |
116 ksi @Temperature 347 °F |
ISO 6721 |
BASF Ultrason S 2010 G4 20% Glass Filled PSU Ultrason S 2010 G4 is a 20% glass reinforced, medium viscosity injection molding PSU grade with high rigidity and strength. |
|||
Shear Modulus | 0.800 GPa @Temperature 175 °C |
116 ksi @Temperature 347 °F |
ISO 6721 |
BASF Ultrason S 2010 G6 30% Glass Filled PSU Ultrason S 2010 G6 is a 30% glass reinforced, medium viscosity injection molding PSU grade with high rigidity and strength. |
|||
Shear Modulus | 0.800 GPa @Temperature 175 °C |
116 ksi @Temperature 347 °F |
ISO 6721 |
BASF Ultrason S 2010 PSU Ultrason S 2010 is an unreinforced, medium viscosity standard injection molding PSU grade. It flows readily and offers outstanding heat resistance and dimensional stability. It conforms to FDA req.. |
|||
Shear Modulus | 0.800 GPa @Temperature 175 °C |
116 ksi @Temperature 347 °F |
ISO 6721 |
BASF Ultrason S 3010 PSU Ultrason S 3010 is an unreinforced, higher viscosity injection molding and extrusion PSU grade, tougher and with improved chemical resistance. It conforms to FDA requirements of 21 CFR 177.1655. |
|||
Shear Modulus | 0.800 GPa @Temperature 50.0 °C |
116 ksi @Temperature 122 °F |
ISO 6721 |
BASF Ultrason® P 3010 PPSU Unreinforced Polyphenylsulfone Description: Medium viscosity injection-molding and extrusion grade with good toughness and chemical resistance (stress crack resistance), resistant against superheated steam. The property profile m.. |
|||
Shear Modulus | 0.799 GPa @Temperature 120 °C |
116 ksi @Temperature 248 °F |
DAM; Dynamic; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 73G45L NC010 Nylon 6
(Unverified Data**) 45% Glass Reinforced Polyamide 6Zytel 73G45L NC010 is a 45% glass fiber reinforced polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers |