Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 108 °C | 227 °F | ASTM D-1525 |
Plaskolite Optix® CA - 1000 E High Impact Grade Acrylic Resin OPTIX® impact-modified grades offer 7 to 10 times the impact resistance of general purpose polymers while maintaining optical clarity.Information provided by Plaskolite, Inc. |
|||
Vicat Softening Point | 108 °C | 227 °F | ASTM D-1525 |
Plaskolite Optix® CA - 1000 E-2 High Impact Grade Acrylic Resin OPTIX® impact-modified grades offer 7 to 10 times the impact resistance of general purpose polymers while maintaining optical clarity.Information provided by Plaskolite, Inc. |
|||
Vicat Softening Point | 108 °C | 226 °F | ASTM D-1525 |
Plaskolite Optix® CA - 927 High Impact Grade Acrylic Resin OPTIX® impact-modified grades offer 7 to 10 times the impact resistance of general purpose polymers while maintaining optical clarity.Information provided by Plaskolite, Inc. |
|||
Vicat Softening Point | 108 °C | 226 °F | ASTM D-1525 |
Plaskolite West Optix® CA - 927 High Impact Acrylic Resin Optix® impact-modified grades exhibit 7 to 10 times the impact strength of general purpose grades and maintaining the superior optical properties. Each grade is offered in a grade(G) that resists g.. |
|||
Vicat Softening Point | 108 °C | 226 °F | Rate A, ASTM D1525 |
Plaskolite West Optix® CA-927 HF Clear Impact Modified Acrylic Resin Impact modified acrylic resin, injection molding gradeApplications: A high flow, impact-modified acrylic resin for injection molding. This resin offers impact strengths up to seven times those of g.. |
|||
Vicat Softening Point | 108 °C | 226 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Cycolac® G366 ABS (Europe-Africa-Middle East) CYCOLAC G366 is a "new technology" grade of ABS exhibiting outstanding property balance, a good flow, medium impact, medium to high heat resistant and an excellent stability during injection mouldin.. |
|||
Vicat Softening Point | 108 °C | 226 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Cycoloy® C3650 PC+ABS Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering high impact and excellent extrusion and thermoforming characteristics. Halogen free according .. |
|||
Vicat Softening Point | 108 °C | 226 °F | 5 kg load; ISO 306 |
Eastman EASTALLOY Polymer DA105, Natural Alloy
(discontinued **) General: All ISO tests are run @ 4-mm thickness with the exception of Impact Resistance, which is run @ 2-mm thickness. Comments: Properties reported here are typical of average lots. Eastman ma.. |
|||
Vicat Softening Point | 108 °C | 226 °F | |
Eastman Eastalloy DA111 PC+PET Copolyester/Polycarbonate
(discontinued **) ISO data as provided by the manufacturer, Eastman Chemical |
|||
Vicat Softening Point | 108 °C | 226 °F | ASTM D1525 |
Global 120-PC-Natural Acrylonitrile Styrene, General Purpose Grade Description-transparent, natural, medium impact resistance, high hardness, high heat resistance, good chemical resistanceApplications-automotive, electrical parts, household goodsInformation provide.. |
|||
Vicat Softening Point | 108 °C @Load 1.00 kg, Thickness 3.17 mm |
226 °F @Load 2.20 lb, Thickness 0.125 in |
ASTM D1525 |
IRPC Polimaxx Polene 330PC Styrene Acrylonitrile APPLICATIONS: INJECTION MOLDING, HOUSEHOLD PRODUCTS : SANITARY WARE, AUTOPART APPLICATION : LAMP ELECTRICAL APPLIANCES : ELECTRICAL FAN |
|||
Vicat Softening Point | 108 °C @Load 5.00 kg |
226 °F @Load 11.0 lb |
50°C/h; ASTM D1525 |
LG Chemical XR404HJ ABS, Heat Resistance, Curl Fit Feature: Injection Molding, Heat Resistance, Curl FitApplication: Automotives Interior Housing (P/W Switch Housing Etc)CAS No. 25120-20-1, 9003-56-9 and 25747-74-7Information provided by LG Chemica.. |
|||
Vicat Softening Point | 108 °C | 226 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics XYLEX X7300 PC+POLYESTER PC+POLYESTER unreinforced alloy. High flow, chemically resistant with excellent optical quality. UV-stabilized. |
|||
Vicat Softening Point | 108 °C @Load 5.10 kg |
226 °F @Load 11.2 lb |
50°C/h; ISO 306 |
Styrolution Novodur® E211 ABS Novodur E211 is a high heat extrusion grade and suitable for blow moldingInformation provided by Styrolution |
|||
Vicat Softening Point | 108 °C | 226 °F | B/50; ISO R306 |
Samsung Cheil Industries Infino® UF-1013 PC, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Vicat Softening Point | 108 °C | 226 °F | VST/A/120; ISO 306 |
Styrolution Polystyrol 158 K GR 2 PS Description: Polystyrol 158 K is a heat resistant, rapid freezing general purpose grade. It is suitable for expanded sheet and film; for blend s with high impact Polystyrol in heat contact applicati.. |
|||
Vicat Softening Point | 108 °C | 226 °F | B/120; ISO R306 |
Samsung Cheil Industries Starex® GR-4010 ABS, 10% Glass Filled Material with 10% GF reinforcement with high stiffness that can be used in refrigerator vegetable boxesInformation provided by Samsung Cheil Industries. |
|||
Vicat Softening Point | 108 °C | 226 °F | B/50; ISO R306 |
Samsung Cheil Industries Starex® SR-0320BM ABS, Unreinforced Heat Resistant Information provided by Samsung Cheil Industries. |
|||
Vicat Softening Point | 108 °C | 226 °F | B/50; ISO R306 |
Samsung Cheil Industries Starex® WR-9370 ASA, Unreinforced Heat Resistant Information provided by Samsung Cheil Industries. |
|||
Vicat Softening Point | 108 °C | 226 °F | B/50; ISO R306 |
Samsung Cheil Industries Starex® WR-9370 ASA, Unreinforced Heat Resistant Information provided by Samsung Cheil Industries. |
|||
Vicat Softening Point | 108 °C | 226 °F | 120°C / 10N; ISO 306-A120 |
Styron EMERGEâ„¢ 7560 Polycarbonate (PC) / Acrylonitrile Butadiene Styrene (ABS) EMERGEâ„¢ PC/ABS 7560 advanced resin is an ignition-resistant PC/ABS blend that contains no chlorine or bromine additives. This resin is suitable for use in a wide variety of applications in the.. |
|||
Vicat Softening Point | 108 °C | 226 °F | |
Styron Magnum™ 2610 ABS, High Gloss MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Vicat Softening Point | 108 °C | 226 °F | |
Styron Magnum™ 555 ABS MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Vicat Softening Point | 108 °C | 226 °F | |
Styron Magnum™ 9010 ABS, High Gloss MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Vicat Softening Point | 108 °C | 226 °F | |
Covestro Bayblend® FR 110 Polycarbonate/ABS Blend Flame retardant grade with antimony, chlorine and bromine free, flame retardant package, good light stability.Applications: Housings for business machines.Information provided by Bayer.As of 1 Septe.. |
|||
Vicat Softening Point | 108 °C @Load 1.00 kg, Thickness 3.17 mm |
226 °F @Load 2.20 lb, Thickness 0.125 in |
ASTM D1525 |
Diamond Polymers ABS 7535 Injection Molding Grade, Very High Impact Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Vicat Softening Point | 108 °C | 226 °F | ASTM D1525 |
Americas Styrenics STYRON® 686E High Heat Crystal Polystyrene Product CharacteristicsExceptional balance between heat resistance, toughness and flowGood dimensional stability and excellent clarityFood Contact CompliantTypical ApplicationsFoamed PS sheets used .. |
|||
Vicat Softening Point | 108 °C | 226 °F | Method B; ASTM D-1525 |
Bhansali Engineering Abstron HR-60 ABS Heat Resistant High, Medium Impact Heat Resistant Grades with good flowInformation provided by Bhansali |
|||
Vicat Softening Point | 108 °C | 226 °F | Rate A, ASTM D1525 |
Plaskolite West Optix® CA-1000 I Clear High Impact Acrylic Resin High impact acrylic resin, injection molding gradeApplications: A high-impact acrylic resin for injection molding. This resin offers impact strengths up to ten times of general-purpose acrylic resi.. |
|||
Vicat Softening Point | 108 °C | 226 °F | |
Styron Magnum™ 9020 ABS, High Gloss MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM AB.. |