Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 42.0 - 123 °C | 108 - 253 °F | Average value: 93.7 °C Grade Count:101 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Unreinforced, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Unreinforced, Flame Retardant". Each property range of values rep.. |
|||
Vicat Softening Point | 42.0 °C | 108 °F | ASTM D1525 |
Hannam Chemical Hanalac HFA-700 ABS |
|||
Vicat Softening Point | 42.0 °C | 108 °F | ASTM D1525 |
DuPont Bynel® E418 Anhydride-Modified Ethylene Vinyl Acetate Adhesive Resin Bynel® Series 3800 resins are anhydride-modified ethylene vinyl acetate polymers. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process p.. |
|||
Vicat Softening Point | 42.0 °C | 108 °F | ASTM D1525 and ISO 306/A |
ExxonMobil Exact™ 9361 Ethylene-based Plastomer Resin Product Description: Exact 9361 plastomer is an ethylene butene copolymer produced using ExxonMobil Chemical's EXXPOL™ Technology, exhibiting both plastic and elastomeric properties.Key Features:P.. |
|||
Vicat Softening Point | 42.0 °C | 108 °F | |
Dow Primacor® 5980I Ethylene Acrylic Acid (EAA) PRIMACOR® 5980I dispersible polymer is an ethylene acrylic acid copolymer (20 wt % comonomer) which is dispersible in aqueous alkali and amines. Excellent adhesion to metallic, cellulosic, glass an.. |
|||
Vicat Softening Point | 42.2 °C | 108 °F | ASTM D1525 |
Dow Primacor® 5986 Ethylene acrylic acid copolymer Low heat seal temperature High gloss, excellent clarity Excellent grease and oil resistance and excellent product resistance for flexible packaging applications Complies with U.S. FDA 21 CFR 177.131.. |
|||
Vicat Softening Point | 42.0 °C | 108 °F | B (50N); ISO 306 |
Borealis Daplen™ PB4432 TPO Compound Daplen PE4432 is a 10% mineral and elastomer modified polypropylene compound intended for injection molding. Daplen PE4432 is a material with excellent impact /stiffness ratio. Thanks to its low th.. |
|||
Vicat Softening Point | 42.0 °C | 108 °F | ASTM D1525 |
DuPont Elvax® 250 Ethylene-Vinyl Acetate Copolymer Resin Elvax resins offer a unique combination of processing and performance characteristics. They provide outstanding toughness and resilience and maintain flexibility over a broad temperature range with.. |