Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 114 °C | 237 °F | 10 N - 120°C/h; ISO 306/A120 |
Polimeri Europa Sinkral® C 442 ABS Resin Sinkral C 442 is a heat resistant injection molding grade offering good flow and impact resistance together with excellent thermal stability during processing. Designation: Thermoplastic ISO 2580-AB.. |
|||
Vicat Softening Point | 114 °C | 237 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Cycoloy® CX1440 PC+ABS CYCOLOY CX1440 is a general purpose PC+ABS blend specially developped for thin wall applications requiring weld line strength and high flow with a good balance of properties |
|||
Vicat Softening Point | 114 °C | 237 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Cycoloy® CX1440 PC+ABS (Europe-Africa-Middle East) CYCOLOY CX1440 is a general purpose PC+ABS blend specially developped for thin wall applications requiring weld line strength and high flow with a good balance of propertiesThis data was supplied by.. |
|||
Vicat Softening Point | 114 °C | 237 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Cycoloy® CX5430 PC+ABS Cycoloy* resin CX5430 is a general purpose PC/ABS blend developed for thin wall applications requiring weld line strength, high flow and impact together with a good balance of other properties. |
|||
Vicat Softening Point | 114 °C | 237 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Lexan® BPL1000 PC Lexan* BPL1000 Polycarbonate (PC) resin is an injection moldable grade featuring high flow and good impact peroformance. It contains non-chlorinated and non-brominated flame retardant systems with U.. |
|||
Vicat Softening Point | 114 °C | 237 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Lexan® BPL1000 PC (Asia Pacific) Lexan* BPL1000 Polycarbonate (PC) resin is an injection moldable grade featuring high flow and good impact peroformance. It contains non-chlorinated and non-brominated flame retardant systems with U.. |
|||
Vicat Softening Point | 114 °C | 237 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics Lexan® FST3403 PC Copolymer (Asia Pacific) Lexan* FST3403 resin is a high flow PC Copolymer Resin, suitable for injection molding. This halogen-free flame retardant resin is EN45545 R6 HL3 compliant and an ideal candidate for train interior .. |
|||
Vicat Softening Point | 114 °C | 237 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Lexan® ML7677 PC (Asia Pacific) Transparent Polycarbonate in limited colors. Excellent processability, super high flow, flame retardant, UL rated V-1 at 2.0mm |
|||
Vicat Softening Point | 114 °C | 237 °F | Rate B/50; ASTM D 1525 |
SABIC Innovative Plastics Lexan® ML7677A PC (Asia Pacific) Commercial grade for Polycarbonate in only nature color. Excellent processability, super high flow, flame retardant, UL rated V-1 at 2.0mm.This data was supplied by SABIC-IP for the Asia Pacific reg.. |
|||
Vicat Softening Point | 114 °C | 237 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Lexan® ML7686 PC (Asia Pacific) Transparent Polycarbonate in limited colors. Excellent processability, super high flow. UL rated V-2 at 1.5mm. |
|||
Vicat Softening Point | 114 °C @Load 1.00 kg |
237 °F @Load 2.20 lb |
ISO 306/A |
Polimeri Europa Clearflex® RM 50 U Linear Medium Density Polyethylene Clearflex RM 50 U is a linear medium density polyethylene resin, with antioxidants and UV stabilizers, suitable for rotomolding applications.Items manufactured with Clearflex RM 50 U show good mecha.. |
|||
Vicat Softening Point | 114 °C | 237 °F | Rate A; 4 mm thick;10.0 mm wide molded rod; ISO 306/A50 |
Premix Thermoplastics PRE-ELEC® PPE 1461
(discontinued **) PRE-ELEC PPE 1461 is a conductive thermoplastic compound based on modified polyphenylene ether (PPE). Conductivity is achieved by using special conductive carbon black. In addition to a low electric.. |
|||
Vicat Softening Point | 114 °C | 237 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics Lexan® FST3403 PC Copolymer (Europe-Africa-Middle East) Lexan* FST3403 resin is a high flow PC Copolymer Resin, suitable for injection molding. This halogen-free flame retardant resin is EN45545 R6 HL3 compliant and an ideal candidate for train interior .. |
|||
Vicat Softening Point | 114 °C | 237 °F | ASTM D1525 |
Eastman M3016-P Polyethylene
(discontinued **) M3016-P is suggested for applications such as spiral-wound can linings, release paper, and photographic paper. M3016-P Has been found to exhibit good barrier properties, temperature resistance, and.. |
|||
Vicat Softening Point | 114 °C | 237 °F | ISO 306 |
Total Lacqtene® 2006 TN 35 HDPE pipe coating
(discontinued **) LACQTENE® 2006 TN 35 is a medium density polyethylene produced by the gas phase polymerization process with hexene as comonomer. LACQTENE® 2006 TN 35 may be used for pipe and sheet extrusion (flex.. |
|||
Vicat Softening Point | 114 °C | 237 °F | ASTM D1525 |
NOVA Chemicals Sclair® 8405 UV8D, 8405G UV8D MDPE Rotational Molding Resin
(discontinued **) Features: Good ESCR, high impact strength.Applications: Spray tanks.Data provided by the manufacturer. |
|||
Vicat Softening Point | 114 °C @Load 5.00 kg |
237 °F @Load 11.0 lb |
50°C/h; ASTM D1525 |
LG Chemical XR409H ABS, Heat Resistance Feature: Injection Molding, Heat ResistanceApplication: Automotives Interior Housing (Switch Panel Housing etc)CAS No. 25120-20-1, 9003-56-9, 25747-74-7, and 31621-07-5Information provided by LG Ch.. |
|||
Vicat Softening Point | 114 °C | 237 °F | ASTM D1525 |
Micropol Microlin ML27 Linear Polyethylene Rotational Molding Powder Information provided by Micropol Limited |
|||
Vicat Softening Point | 114 °C | 237 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics NORYL WCV072 PPE+PP (Asia Pacific) Flexible, halogen free mPPE extrusion grade material for applications such as automotive wire insulation. Low specific gravity with good flame retardant and very good scrape abrasion resistance. De.. |
|||
Vicat Softening Point | 114 °C | 237 °F | 50°C/hr, 50N; ISO 306 |
Teijin Multilon T-3713 Standard PC/ABS Polymer Alloy General grade of PC/ABS polymer alloy, having improved impact strength and heat resistance compared with a heat resistant ABS and flame retardant m-PPE and also having higher flowability compared wi.. |
|||
Vicat Softening Point | 114 °C | 237 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Noryl NH3060 PPE+HIPS NH3060 resin is a modified PPE + PS blend with an excellent balance of non-chlorinated non-brominated flame retardance, hydrolytic stability, impact and heat resistance, good flow, and low specific .. |
|||
Vicat Softening Point | 114 °C | 237 °F | ISO 306 |
Borealis Bormed™ TD109CF Polypropylene Copolymer Bormed™ TD109CF is a propylene alpha olefin copolymer. This grade is suitable for the manufacturing of unoriented films on cast and tubular quench film lines. Applications: lamination films, food.. |
|||
Vicat Softening Point | 114 °C | 237 °F | 10 N; ISO 306 |
Borealis Borseal™ TD115BF Terpolymer for BOPP Film Borseal TD115BF is a C2/C4 terapolymer film resin.Borseal TD115BF is especially developed for use as sealing layers in coextruded BOPP film (manufactured on Stenter frame and double bubble film proc.. |
|||
Vicat Softening Point | 114 °C | 237 °F | ISO 306 |
Unipetrol PE HD LITEN® SB/SL 20 HDPE Made for blow molding, tubular film and special applications.Information provided by Unipetrol RPA |
|||
Vicat Softening Point | 114 °C | 237 °F | A50; ISO 306 |
Lubrizol ESTANE® GP92AT Ether Based Thermoplastic Polyurethane Type: Estane® GP 92AT is an aromatic polyether-based thermoplastic polyurethane (TPU).Appearance: Translucent spherical pelletsUses: Injection molding partsAvailable in EuropeInformation provided b.. |
|||
Vicat Softening Point | 114 °C | 237 °F | 10 N; ISO 306A |
Borealis Borseal™ TD210BF Terpolymer for BOPP Film Borseal TD210BF is a C2/C4 terapolymer film resin especially developed for use as sealing layers in coextruded BOPP film (manufactured on stenter frame and double bubble film process).Borseal TD210B.. |
|||
Vicat Softening Point | 114 °C | 237 °F | ExxonMobil Method |
ExxonMobil Pax-Plus™ 3204 Blown Film Resin Pax-Plus 3204 is a rubber modified high density polyethylene film resin which is used primarily in film requiring good impact strength. It is specially formulated to provide easy tear in the machin.. |
|||
Vicat Softening Point | 114 - 127 °C | 237 - 261 °F | Average value: 119 °C Grade Count:4 |
Overview of materials for Medium Density Polyethylene (MDPE), Extruded This property data is a summary of similar materials in the MatWeb database for the category "Medium Density Polyethylene (MDPE), Extruded". Each property range of values reported is minimum and max.. |
|||
Vicat Softening Point | 114 °C | 237 °F | ASTM D1525 |
ExxonMobil LL 6407 Injection Molding Resin
(discontinued **) LL 6100 is a narrow molecular weight butene copolymer designed for applications that require outstanding environmental stress crack resistance. This resin offers good processability with minimal wa.. |
|||
Vicat Softening Point | 114 °C | 237 °F | under 1 daN; ASTM D1525 |
Arkema Group Pebax® MX 1205 Polyether Block Amide (PEBA) Typical application: Impact modifierInformation provided by Arkema Group |