Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 147 °C | 297 °F | Rate A; 4 mm thick;10.0 mm wide molded rod; ISO 306/A50 |
Premix Thermoplastics PRE-ELEC® ESD 7300 PRE-ELEC ESD 7300 is a static dissipative thermoplastic compound based on PC/PBT. The dissipative property is permanent and built into the polymer chain. PRE-ELEC ESD 7300 has been developed for inj.. |
|||
Vicat Softening Point | 147 °C | 297 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Lexan® 500RS PC (Europe-Africa-Middle East) LEXAN 500RS is a medium viscosity, glass reinforced, flame retardant grade. |
|||
Vicat Softening Point | 147 °C | 297 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Lexan® 505RU PC (Asia Pacific) Lexan* 505RU is a glass reinforced,flame retardant(FR)grade with non brominated and non chlorinated FR systems and UV stablization packages. This product is intended for applications to meet WEEE/Ro.. |
|||
Vicat Softening Point | 147 °C | 297 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Lexan® EXL4016 PC Copolymer 6% GF reinforced opaque polycarbonate-siloxane copolymer, for increased stiffness with good impact strength. Improved release properties. Available in limited colors only.This data was supplied by S.. |
|||
Vicat Softening Point | 147 °C | 297 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Lexan® EXL4016 PC Copolymer (Europe-Africa-Middle East) 6% GF reinforced opaque polycarbonate-siloxane copolymer, for increased stiffness with good impact strength. Improved release properties. Available in limited colors only.This data was supplied by S.. |
|||
Vicat Softening Point | 147 °C | 297 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics Lexan® LUX2619 PC (Europe-Africa-Middle East) Lexan* LUX2619 Polycarbonate resin is an extrusion grade. It is UL94 V-2 rated at 1.5 mm. It was designed for high light reflectance. |
|||
Vicat Softening Point | 147 °C @Load 5.001 kg |
297 °F @Load 11.03 lb |
50°C/h; ISO 306 |
Polykemi AB SCANTEC PC S75R GF30 V0 Polycarbonate, Glass Fiber Reinforced, Flame Retardant Information provided by Polykemi AB |
|||
Vicat Softening Point | 147 °C | 297 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics Lexan® 3412ECR PC (Europe-Africa-Middle East) Lexan* 3412ECR Polycarbonate (PC) resin is a 20% glass fiber filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant GF-PC has an UL-94 V0 rating and is available in v.. |
|||
Vicat Softening Point | 147 °C | 297 °F | |
Dow Isoplast® 2532 Polyurethane (PUR-RT), Clear Amorphous Polymer
(discontinued **) ISOPLAST® 2532 resin is a clear amorphous polymer with the chemical resistance of crystalline resins specially designed for medical applications. Its outstanding properties include clarity, excelle.. |
|||
Vicat Softening Point | 147 °C | 297 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics Lexan® EXL9330S PC Copolymer (Asia Pacific) Opaque PC-Siloxane copolymer with excellent processability. UV stabilized. UL rated V-0/5VA/CTI-PLC-2. Available in limited colors. |
|||
Vicat Softening Point | >= 147 °C | >= 297 °F | |
Kazanorgsintez PC-005 Polycarbonate Production Method: Obtained by means of polycondensation method. Application: Intended for product manufacture by method of extrusion and die-casting.Information Provided by Kazanorgsintez |
|||
Vicat Softening Point | 147 °C @Load 5.10 kg |
297 °F @Load 11.2 lb |
50°C/hr; ASTM D1525 |
LG Chemical Lupoy 1301EP22 Polycarbonate Resin Description: LUPOY PC 1301EP-22 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strengt.. |
|||
Vicat Softening Point | 147 °C @Load 5.10 kg |
297 °F @Load 11.2 lb |
50°C/hr; ASTM D1525 |
LG Chemical Lupoy 1303EP-22 Polycarbonate Resin Description: LUPOY PC 1303EP-22 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strengt.. |
|||
Vicat Softening Point | 147 °C @Load 5.10 kg |
297 °F @Load 11.2 lb |
50°C/hr; ASTM D1525 |
LG Chemical Lupoy NF1005F 03R Polycarbonate Resin Description: LUPOY NF 1005F03R, eco-friendly UL94 V0/1.5 mm, is designed for extrusion products. It combines an excellent physical property balance of heat resistance, transparency and impact streng.. |
|||
Vicat Softening Point | 147 °C | 297 °F | ASTM D1525-97 |
Ipiranga Petrochem PCC 0710 Polypropylene The production of polypropylene (PP) employs Spheripol technology from Montell / Italy. This technology has been acclaimed all over the world and is known as clean technology, because it does not pr.. |
|||
Vicat Softening Point | 147 °C | 297 °F | ASTM D1525-97 |
Ipiranga Petrochem PH 2610 Polypropylene The production of polypropylene (PP) employs Spheripol technology from Montell / Italy. This technology has been acclaimed all over the world and is known as clean technology, because it does not pr.. |
|||
Vicat Softening Point | 147 °C @Load 5.10 kg |
297 °F @Load 11.2 lb |
50°C/hr; ASTM D1525 |
LG Chemical Lupoy 1201HP-22 Polycarbonate Resin Description: LUPOY PC 1201HP-22 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strengt.. |
|||
Vicat Softening Point | 147 °C | 297 °F | B/50; ISO R306 |
Samsung Cheil Industries Infino® HN-3203G PC, Glass Filled FR Information provided by Samsung Cheil Industries. |
|||
Vicat Softening Point | 147 °C | 297 °F | B/50; ISO R306 |
Samsung Cheil Industries Infino® HN-3203G PC, Glass Filled FR Information provided by Samsung Cheil Industries. |
|||
Vicat Softening Point | 147 °C | 297 °F | 50°C/hr, 50N Load; ASTM D1525 |
Styron CALIBREâ„¢ 201-22 Polycarbonate Information provided by DowThis product line was spun off from Dow Chemical to Styron in 2010. |
|||
Vicat Softening Point | 147 °C @Load 5.10 kg |
297 °F @Load 11.2 lb |
Rate A (50°C/h); ASTM D1525; ISO 360/B50 |
Styron CALIBREâ„¢ 203-22 Polycarbonate Resin Overview: CALIBREâ„¢ 200-22 polycarbonate resins are produced in compliance with the US Food and Drug Administration (FDA) and EU food contact regulations. They provide excellent impact resistanc.. |
|||
Vicat Softening Point | 147 °C | 297 °F | ISO 306/B50 |
Styron CALIBREâ„¢ 301-58 LT Polycarbonate Resin Overview: CALIBREâ„¢ 301-58 LT is a high light transmission, high-flow polycarbonate resin for injection molding applications.Main Characteristics:High light transmissionHigh flow for injection m.. |
|||
Vicat Softening Point | 147 °C | 297 °F | 50°C/hr, 50N Load; ASTM D1525 |
Styron CALIBREâ„¢ 303 EP Polycarbonate Information provided by DowThis product line was spun off from Dow Chemical to Styron in 2010. |
|||
Vicat Softening Point | 147 °C | 297 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics LNP THERMOCOMP Noryl_PX5379 PPE+HIPS (Europe-Africa-Middle East) LNP* Thermocomp* Noryl_PX5379 compound is a 10% GR. UL94 V-1 rated. Halogen free flame retardant. Typical applications are TV chassis, deflection yokes and connectors. |
|||
Vicat Softening Point | 147 °C | 297 °F | B/50; ISO R306 |
Samsung Cheil Industries Infino® VB-3100G PBT/ABS, Glass Filled FR Information provided by Samsung Cheil Industries. |
|||
Vicat Softening Point | 147 °C @Load 1.02 kg |
297 °F @Load 2.25 lb |
ISO 306 |
Borealis BA390TF Polypropylene Copolymer BA390TF is a high molecular weight, low melt flow rate polypropylene block copolymer with very high impact strength. Applications: BA390TF is recommended for foam extrusion, or thermoforming.Inform.. |
|||
Vicat Softening Point | 147 °C | 297 °F | 50°C/h 50N; ISO 306 |
Covestro Makrolon® 1248 Polycarbonate, Impact Grade ISO 7391-PC,MP,(,,)-09-9Formerly Makrolon KU1-1248MVR (300 °C/1.2 kg) 7.0 cm3/10 minFood contact qualityMedium viscosityImpact modifiedInjection molding - Melt temperature 280 - 320 °CAvailable in.. |
|||
Vicat Softening Point | 147 °C @Load 1.02 kg |
297 °F @Load 2.25 lb |
ASTM-D1525 |
Braskem PCD 0140BR HECO Polypropylene Heterophasic Copolymer PCD 0140BR is a low melt flow rate heterophasic copolymer with high impact resistance. This resin was developed for steel pipe coating extrusion. PCD 0140BR is highly protected against thermal aging.. |
|||
Vicat Softening Point | 147 °C | 297 °F | ASTM D1525 |
Alliance Polymers Zythane™ 4060D Thermoplastic Polyurethane Elastomer Zythane™ 4060D is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good .. |
|||
Vicat Softening Point | 147 °C @Load 1.02 kg |
297 °F @Load 2.25 lb |
ISO 306 |
Arkema Group OREVAC® CA 100 Grafted Maleic Anhydride Polypropylene OREVAC® CA 100 is a chemically functionalized polypropylene with a high content of maleic anhydride. Grafting on polypropylene backbone is achieved with a processing technology which allows to opti.. |