Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 155 °C | 311 °F | B; STN EN ISO 306 |
Plastcom SLOVALEN PC 59 GF 13 Compounded Polypropylene Homopolymer, 13% Chemically Coupled Glass Fiber FeaturesCompounded homopolymer PP, with the content of 13% chemically coupled glass fiber and modifier of mechanical properties. Increased strength in comparison with unfilled PP. Use in all indus.. |
|||
Vicat Softening Point | 155 °C | 311 °F | B; STN EN ISO 306 |
Plastcom SLOVALEN PH 49 GF 50 Polypropylene Homopolymer, 50% Glass Fiber FeaturesModified homopolymer PP for injection moulding, chemically reinforced with 50% glass fiber, contains the modifier of mechanical properties. Increased strength in comparison with unfilled PP.. |
|||
Vicat Softening Point | 155 °C | 311 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Lexan® HPH4504 PPC High heat specialty polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 of USP Class VI). EtO, steam, gamma and e-beam steril.. |
|||
Vicat Softening Point | 155 °C | 311 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Lexan® HPH4504H PPC (Europe-Africa-Middle East) High heat specialty polycarbonate with enhanced autoclavability. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 of USP Class VI). EtO, .. |
|||
Vicat Softening Point | 155 °C | 311 °F | ASTM D1525 |
PolyMirae Moplen HP521M IPP/WQBF Grade Polypropylene Moplen HP521M is the polypropylene homopolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen HP521M is suitable for core resin of co-extrusion CPP film. Moplen .. |
|||
Vicat Softening Point | 155 - 165 °C | 311 - 329 °F | Average value: 161 °C Grade Count:12 |
Overview of materials for Acetal Copolymer, Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Carbon Fiber Filled". Each property range of values reported is minimum and maximum va.. |
|||
Vicat Softening Point | 155 °C | 311 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Lexan® HPH4404 PPC+PC High heat specialty polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam, gamma and e-beam steril.. |
|||
Vicat Softening Point | 155 °C | 311 °F | |
EVALCA EVAL® LC-E105A Ethylene Vinyl Alcohol Copolymer Resin
(discontinued **) 44 mol % Ethylene.Data provided by EVALCA. Applications: Cast film, melt phase forming, solid phase pressure forming, tubes, coex coating. EVOH is used in packaging applications because of its out.. |
|||
Vicat Softening Point | 155 °C | 311 °F | For EP-E105 |
EVALCA EVAL® LC-E151B Ethylene Vinyl Alcohol Copolymer Resin
(discontinued **) 44 mol % Ethylene.Data provided by EVALCA. Applications: Melt phase forming, solid phase pressure forming, blow molding, tubes EVOH is used in packaging applications because of its outstanding gas.. |
|||
Vicat Softening Point | 155 °C | 311 °F | For EP-E105 |
EVALCA EVAL® G110 Ethylene Vinyl Alcohol Copolymer Resin
(discontinued **) 48 mol % Ethylene.Data provided by EVALCA. EVOH is used in packaging applications because of its outstanding gas barrier properties.EVAL™ is now produced as a part of the Kuraray product line. |
|||
Vicat Softening Point | 155 °C | 311 °F | DIN ISO 306 |
Lehmann & Voss LUVOCOM® 80-0837 Polyacetal-copolymer, with PTFE, lubricant modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Emergency running property, gl.. |
|||
Vicat Softening Point | 155 °C | 311 °F | ASTM D1525 |
Mapal Plastics Maplon Type K OPAQLON COO1 Polypropylene Sheet Maplon Catalog No. L050-C001K0101 is an extremely opaque white sheet. Sheet surface is smoothly embossed with similar finish on both sides..Main advantages: High opacity, High rigidity high thermal .. |
|||
Vicat Softening Point | 155 °C @Load 1.00 kg |
311 °F @Load 2.20 lb |
ASTM D1525 |
LG Chemical SEETEC M1425 Polypropylene Impact Copolymer Features: SEETEC M1425 is a heterophasic polypropylene copolymer for injection molding applications. SEETEC M1425 exhibits a very high stiffness and a good impact strength. SEETEC M1425 meets the FD.. |
|||
Vicat Softening Point | 155 °C | 311 °F | ISO 306/A |
Iran Petrochemical (PCC) Moplen Z 30 S Polypropylene Moplen Z 30S is a high melt flow homopolymer for the production of low denier BCF, CF, and staple fibers at medium to high spinning speeds. Moplen Z30S offers a high homogeneity, stable extrusion a.. |
|||
Vicat Softening Point | 155 °C @Load 5.00 kg |
311 °F @Load 11.0 lb |
|
LATI Latiohm 90/13-09 PD01 G/10 PPOm, 10% Glass Fiber Reinforced Semiconductive/dissipative product based on Modified Polyphenylene Oxide (PPOm). Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation prov.. |
|||
Vicat Softening Point | 155 °C | 311 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics NORYL V0150B PPE+HIPS Noryl* V0150B is an unfilled, injection moldable modified polyphenylene ether resin.. Designed for high heat resistance and thin wall FR performance, this resin delivers a UL94 V0 rating at 1.5 mm a.. |
|||
Vicat Softening Point | 155 °C | 311 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics NORYL V03550 PPE+HIPS (Asia Pacific) Noryl* V03550 is a 35% milled fibre reinforced, injection moldable grade. Designed for good dimensional stability and low warpage, this resin also uses non-chlorinated, non-brominated FR additives t.. |
|||
Vicat Softening Point | 155 °C | 311 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Valox® VX4910 ASA+PBT (Europe-Africa-Middle East) 10% Glass reinforced nucleated PBT/ASA with excellent mechanical properties high dimensional stability, and low density. |
|||
Vicat Softening Point | 155 °C | 311 °F | Rate A/50; ISO 306 |
SABIC Innovative Plastics NORYL GFN3V PPE+HIPS (Europe-Africa-Middle East) NORYL GFN3V is a 30 % glass fibre reinforced material with a HDT/A of 145C according ISO 75. NORYL GFN3V has been approved for potable water applications up to 85C by the UK WFBS according BS 6920 i.. |
|||
Vicat Softening Point | 155 °C | 311 °F | ISO 306 |
Unipetrol PP MONSTEN® GB 506 Polypropylene Impact Copolymer Applications include injection molding and thermoforming. Basic stabilization. Impact copolymer.Information provided by Unipetrol RPA |
|||
Vicat Softening Point | 155 °C | 311 °F | ASTM D1525 |
Engineered Plastics EPPC 1214C Polycarbonate Clear injection grade. Property values below represent typical values. Information provided by Engineered Plastics Corporation. |
|||
Vicat Softening Point | 155 °C | 311 °F | 10 N; ASTM D1525 |
Braskem H 503 Injection Molding Polypropylene Description: H 503 is a low melt flow rate additivated homopolyme used for general purposes. It is designed for injection molding, raffia extrusion, bioriented film and general extrusion. This produ.. |
|||
Vicat Softening Point | 155 °C @Load 1.02 kg |
311 °F @Load 2.25 lb |
ASTM D1525 |
Carmel Olefins CAPILENE® T 77 A Polypropylene Homopolymer CAPILENE® T 77 A is a high melt flow rate polypropylene homopolymer for injection molding with nucleation and antistatic additivation. It exhibits good stiffness, combined with good thermal stabili.. |
|||
Vicat Softening Point | 155 °C @Load 1.02 kg |
311 °F @Load 2.25 lb |
ASTM D1525 |
Carmel Olefins CAPILENE® U 77 AV Polypropylene Homopolymer CAPILENE® U 77 AV is a high melt flow rate polypropylene homopolymer controlled rheology, designed for injection molding of products with long flow length. It is specially formulated with antistati.. |
|||
Vicat Softening Point | 155 °C | 311 °F | -1kg; ASTM D1525 |
Braskem H 117 Injection Molding Polypropylene Description: H 117 is a ultra-high melt flow rate homopolymer. This product is suitable to high productivity on thin-walled parts. H 117 features an excellent stiffness, thermal resistance, low warp.. |
|||
Vicat Softening Point | 155 °C | 311 °F | 50 N; ISO 306 |
Azoty Tarnow™ TARNOFORM 300 GB2 POM 10% glass beads filled grade with increased stiffness and hardness with lowered shrinkageInformation provided by Zakłady Azotowe w Tarnowie-Moscicach S.A. |
|||
Vicat Softening Point | 155 °C | 311 °F | ISO 306 |
Polyram RamOfin PPC343T4 Polypropylene, 20% Mineral Filled 20% Mineral filled, UV stabilized, heat stabilized polypropylene for injection molding applications.Information provided by Polyram. |
|||
Vicat Softening Point | 155 °C | 311 °F | B |
Plastcom SLOVALEN PH 91 C 20 PP, 20% mineral filling FeaturesModified homopolymer and copolymer PP for injection moulding with the contenct of 20% microground, chemically modified talc. Increased strength, rigidity and thermal application up to 100°C.. |
|||
Vicat Softening Point | 155 °C | 311 °F | -1kg; ASTM D1525 |
Braskem H 510 Bioriented Film Polypropylene Applications: Bioriented films for conversion; adhesive tapes; textile and food packing. Information provided by Braskem |