Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 165 °C | 329 °F | ASTM D1525 |
Multibase Nylex™ 2185 Polyamide + PP Forms: PelletsInformation provided by Multibase |
|||
Vicat Softening Point | 165 °C | 329 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics Lexan® 3413R PC 30% GR, provides improved mechanical properties and UL94V-1 rated at 0.058"". Internal mold release added. |
|||
Vicat Softening Point | 165 °C | 329 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics Lexan® 3414R PC (Asia Pacific) 40% GR, provides improved mechanical properties and UL94V-1 rated at 0.058"". Internal mold release added. |
|||
Vicat Softening Point | 165 °C | 329 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Lexan® HPH4704 PPC High heat specialty polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam, gamma and e-beam steril.. |
|||
Vicat Softening Point | 165 °C | 329 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics Lexan® 3412R PC (Asia Pacific) 20% GR, provides improved mechanical properties and UL94 V-1 rated at 0.058"". Internal mold release added. |
|||
Vicat Softening Point | 165 °C | 329 °F | DIN ISO 306 |
Lehmann & Voss LUVOCOM® 1850/TF/30 PBT, with PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteri.. |
|||
Vicat Softening Point | 165 °C | 329 °F | DIN ISO 306 |
Lehmann & Voss LUVOCOM® 80/CF/10/BK Polyacetal-copolymer, with carbon fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Electrically conductive, suitable for continuous discharging of statically .. |
|||
Vicat Softening Point | 165 °C @Load 5.00 kg |
329 °F @Load 11.0 lb |
|
LATI Latigray 82-04 CX/90 PA 12 Radiopaque compound based on Polyamide 12 (PA12). Special mineral filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria.. |
|||
Vicat Softening Point | 165 °C @Load 5.00 kg |
329 °F @Load 11.0 lb |
|
LATI Latimass 82-02 D030 PA12 Specific density compound based on Polyamide 12 (PA12). Special filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria T.. |
|||
Vicat Softening Point | 165 °C @Load 5.00 kg |
329 °F @Load 11.0 lb |
|
LATI Latimass 82-03 D080 PA12 Specific density compound based on Polyamide 12 (PA12). Special filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria T.. |
|||
Vicat Softening Point | 165 °C | 329 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Noryl PX7446 PPE+PS This data was supplied by SABIC-IP for the Americas region. |
|||
Vicat Softening Point | 165 °C | 329 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics NORYL V02570 PPE+HIPS Noryl* V02570 is a 25% milled fiber reinforced, injection moldable grade. Designed for good dimensional stability and low warpage, this resin also uses non-chlorinated, non-brominated FR additives t.. |
|||
Vicat Softening Point | 165 °C | 329 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics NORYL V02570 PPE+HIPS (Asia Pacific) Noryl* V02570 is a 25% milled fiber reinforced, injection moldable grade. Designed for good dimensional stability and low warpage, this resin also uses non-chlorinated, non-brominated FR additives t.. |
|||
Vicat Softening Point | 165 °C | 329 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Valox® HX312C PBT (Europe-Africa-Middle East) Unreinforced PBT with release. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food contact compliant. EtO and stea.. |
|||
Vicat Softening Point | 165 °C | 329 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Valox® IQ325HP PBT (Asia Pacific) FDA compliant PBT resin, using chemically recycled post consumer PET Bottles. Fit to food contact applications. |
|||
Vicat Softening Point | 165 °C | 329 °F | VST/A/50; ISO 306 |
Styrolution Terblend® N NM-13 ABS+PA (Conditioned) Description: Terblend® N NM-13 is ABS/PA blend combining excellent impact strength at low temperatures with easy processability and good surface appearance.Information provided by STYROLUTION, wh.. |
|||
Vicat Softening Point | 165 °C | 329 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Valox® IQ325HP PBT (Europe-Africa-Middle East) FDA compliant PBT resin, using chemically recycled post consumer PET Bottles. Fit to food contact applications. |
|||
Vicat Softening Point | 165 °C | 329 °F | Rate A/50; ISO 306 |
SABIC Innovative Plastics Valox® IQ357U PBT+PC (Europe-Africa-Middle East) Valox* Resin IQ357U: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified and UV stabilized resin. |
|||
Vicat Softening Point | 165 °C | 329 °F | ASTM-D1525 |
Polyram RamTal PM340S4 Acetal, 20% Glass beads Reinforced 20% Glass beads reinforced polyacetal for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Vicat Softening Point | 165 °C | 329 °F | A (10N); ISO 306 |
Borealis Xmod™ K65G2 20% Glass Fiber Reinforced Polypropylene Compound Xmod K65G2 is a 20% glass fiber reinforced grade intended for injection molding. Xmod K65G2 has been developed especially for the car industry, to be used UTB parts. Xmod K65G2 offers good balance.. |
|||
Vicat Softening Point | 165 °C | 329 °F | B/50; ISO 306 |
Eurostar Staramide BST44 PA6, Impact Modified, Injection Molded BST44 is a Low Temperature Impact Modified Polyamide 6 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
Vicat Softening Point | 165 °C | 329 °F | under 1 daN; ASTM D1525 |
Arkema Group Pebax® 7033 Polyether Block Amide (PEBA) Information provided by Arkema Group |
|||
Vicat Softening Point | 165 °C | 329 °F | under 1 daN; ASTM D1525 |
Arkema Group Pebax® 7233 Polyether Block Amide (PEBA) Information provided by Arkema Group |
|||
Vicat Softening Point | 165 °C | 329 °F | 50°C/hr; 50N |
Arkema Group Rilsan® AUM 50 NOIR T6LD Nylon 12, 50% Glass Bead Filled (Conditioned) Designation ISO 1874-PA12,MHLR,16-020,GB50Rigid grad with glass beads filler (50%) for injection molding. Available color: black. Reinforced light and heat stabilizing agents. Mold-release agent.Goo.. |
|||
Vicat Softening Point | 165 °C | 329 °F | 50°C/hr; 50N |
Arkema Group Rilsan® AZM 23 T6LD Nylon 12, 23% Glass Fiber Filled (Conditioned) Designation ISO 1874-PA12,MHLR,16-050,GF23Rigid grade with glass fiber filler (23%) for injection molding. Available colors: black and natural. Reinforced light and heat stabilizing agent. Mold-rele.. |
|||
Vicat Softening Point | 165 °C | 329 °F | 50°C/hr; 50N |
Arkema Group Rilsan® AZM 30 O TLD Nylon 12, 30% Glass Fiber Filled (Conditioned) Designation ISO 1874-PA12,MHLR,16-050,GF30Rigid grade with glass fiber (30%) for injection molding. Available color: natural. Light and heat stabilizing agent. Mold-release agent.High rigidity. High.. |
|||
Vicat Softening Point | 165 - 210 °C | 329 - 410 °F | Average value: 183 °C Grade Count:5 |
Overview of materials for Polybutylene Terephthalate (PBT), PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), PTFE Filled". Each property range of values reported is minimum and ma.. |
|||
Vicat Softening Point | 165 °C | 329 °F | Rate A/50; ISO 306 |
SABIC Innovative Plastics Valox® VX3608C PBT (Europe-Africa-Middle East) VALOX VX3608C is an impact modified, flame retardant PBT+PC injection moulding resin. Application: electrical enclosures. This grade is 3607U with reduced oxygen index.This data was supplied by SABI.. |