Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 74.0 °C @Load 1.00 kg |
165 °F @Load 2.20 lb |
ISO 306/A |
Polimeri Europa Clearflex® MQ B0 Very Low Density Polyethylene Clearflex MQ B0 is a linear polyethylene, with antioxidants, characterized by a very low density (VLDPE).The resin shows an excellent balance between flexibility and impact resistance.Main Applicati.. |
|||
Vicat Softening Point | 74.0 °C @Load 5.10 kg |
165 °F @Load 11.2 lb |
ISO 306 |
SABIC P6006 Black High Density Polyethylene for Pipes Product Description: P6006 is a black compound high density (class MRS 8 - PE 80) polyethylene with bimodal distribution of molecular mass. It is specifically designed for Pressure Pipe applicatio.. |
|||
Vicat Softening Point | 74.0 °C | 165 °F | |
Eastman Eastapak 7352 PET
(discontinued **) Unreinforced Low IV. ISO data as provided by the manufacturer, Eastman Chemical.This product is discontinued; 2003. |
|||
Vicat Softening Point | 74.0 °C | 165 °F | ASTM D1525 |
DuPont™ Surlyn® 1601B Sodium Ionomer Resin for Blown and Cast Film
(discontinued **) Surlyn® 1601B is an ionomer resin available for use in conventional blown and cast film extrusion and coextrusion equipment designed to process polyethylene resins. Applications: Meat, poultry, se.. |
|||
Vicat Softening Point | 74.0 °C | 165 °F | |
LyondellBasell Lupolen® 5031 L HDPE, Injection Molding Grade Easy flow, injection molding grade for closures, aerosol pumps, spray nozzles for spray cans, small automotive parts such as the caps on lead/acid batteries, knobs, barrels for writing instruments a.. |
|||
Vicat Softening Point | 74.0 - 76.0 °C @Load 5.00 kg |
165 - 169 °F @Load 11.0 lb |
ISO R306 |
Fainplast Compounds RI 528/H Rigid PVC, Antishock Injection Molding Road drains |
|||
Vicat Softening Point | 74.0 °C | 165 °F | ASTM D1525 |
LyondellBasell Plexar® PX3216 Extrudable Tie-Layer Resin, Anhydride Modified LLDPE Plexar® tie-layers are chemically modified resins used to bond unlike materials, primarily in packaging and industrial applications. Common adherents include polyethylene resins and copolymers, s.. |
|||
Vicat Softening Point | >= 74.0 °C | >= 165 °F | ASTM D 1525 |
Karina 801-10/88-CR White PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Vicat Softening Point | >= 74.0 °C | >= 165 °F | ASTM D 1525 |
Karina 822-18/599-CRB-LMP Gray PVC Compound Heavy metal free PVC compound.Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Vicat Softening Point | >= 74.0 °C | >= 165 °F | ASTM D 1525 |
Karina E 835-35/1-ERYB-AS Ivory PVC Compound Rigid ivory PVC compound with anti-UV protection, developed for extrusion profile under 8700x0220 sample analysis.Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Vicat Softening Point | 74.0 °C | 165 °F | ASTM D1525 |
UBE V210 Polyethylene Description: UBE Polyethylene is polymerized at high pressure using a tubular reactor. Production conditions are strictly controlled ensuring the product's superior physical and mechanical prope.. |
|||
Vicat Softening Point | 74.0 °C | 165 °F | A50; ISO 306 |
Lubrizol ESTANE® GP65AE Ester Based Thermoplastic Polyurethane Type: Estane® GP 65AE is an aromatic polyester-based thermoplastic polyurethane (TPU).Appearance: Translucent spherical pelletsUses: Injection molding partsAvailable in EuropeInformation provided b.. |
|||
Vicat Softening Point | 74.0 °C | 165 °F | |
Eastman Eastar 6763 PETG Copolyester ISO data as provided by the manufacturer, Eastman Chemical |
|||
Vicat Softening Point | 74.0 °C | 165 °F | |
Eastman Eastar EN058 PET Copolymer ISO data as provided by the manufacturer, Eastman Chemical |
|||
Vicat Softening Point | 74.0 °C | 165 °F | ASTM D1525 |
Eastman Eastman Embrace Copolyester for Extrusion/Cast Film Applications:Flexible packagingIV containersLabels to fit high contour containersShrink packagingWrap around designKey Attributes:Excellent clarityExcellent printabilityGood chemical resistanceGood .. |
|||
Vicat Softening Point | 73.9 °C | 165 °F | ASTM D1525 |
ExxonMobil Escor™ 5070 Ethylene Acrylic Acid Copolymer Resin Product Description: Escor 5070 is an ethylene acrylic acid copolymer characterized by high melt index and 9% acrylic acid comonomer content. Escor 5070 combines easily processing and adhesion to po.. |
|||
Vicat Softening Point | 74.0 °C | 165 °F | ASTM D1525 |
DuPont™ Surlyn® 1601 Sodium Ionomer Resin for Blown and Cast Film Surlyn® 1601 is an ionomer resin available for use in conventional blown and cast film extrusion and coextrusion equipment designed to process polyethylene resins. Applications: Meat, poultry, sea.. |
|||
Vicat Softening Point | 74.0 °C | 165 °F | ASTM D1525 |
DuPont™ Surlyn® 1601-2 Sodium Ionomer Resin for Blown and Cast Film Surlyn® 1601-2 is an ionomer resin available for use in conventional blown and cast film extrusion and coextrusion equipment designed to process polyethylene resins. Applications: Meat, poultry, s.. |
|||
Vicat Softening Point | 74.0 °C | 165 °F | ASTM D1525 |
DuPont™ Surlyn® 1601-2LM Sodium Ionomer Resin for Blown and Cast Film Surlyn® 1601-2LM (Low Moisture) is an ionomer resin available for use in conventional blown and cast film extrusion and coextrusion equipment designed to process polyethylene resins. Applications:.. |
|||
Vicat Softening Point | 74.0 °C | 165 °F | Rate B, ASTM D1525-70 |
DuPont™ Surlyn® 9520 Ionomer Resin, Zinc Surlyn® 9520 thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with zinc ions. The amount of MAA and neutr.. |
|||
Vicat Softening Point | 74.0 °C | 165 °F | |
Dow AFFINITY™ SM 1300 Polyolefin Plastomer AFFINITY® SM 1300 polyolefin plastomer is an alpha-olefin resin that offers excellent performance in high clarity durable injection molded industrial and consumer goods and compression molded closu.. |
|||
Vicat Softening Point | 74.0 °C | 165 °F | 1kg load; ASTM D1525 |
Eastman Eastar GN077 Copolyester, Natural Eastar Copolyester GN077 is an amorphous resin with good melt strength, chemical resistance, high clarity and gloss. It is an excellent choice for extrusion blow molding small to intermediate size c.. |
|||
Vicat Softening Point | 74.0 °C | 165 °F | JIS-K-6740 |
Denka VINYKON M6000 PVC, M grade for hard injection molding A PVC resin compound offering excellent physical properties and workability. A broad product lineup is available, including hard and soft grades, as well as those for extrusion and injection molding.. |
|||
Vicat Softening Point | 74.0 - 76.0 °C @Load 5.00 kg |
165 - 169 °F @Load 11.0 lb |
ISO R306 |
Fainplast Compounds ARC 30 Rigid PVC, Atoxic for General Purpose Bottles very high antishock |
|||
Vicat Softening Point | 74.0 °C | 165 °F | under 1 daN; ASTM D1525 |
Arkema Group Pebax® 3533 Polyether Block Amide (PEBA) Information provided by Arkema Group |
|||
Vicat Softening Point | 74.0 °C | 165 °F | 50°C/hr; 50N |
Arkema Group Pebax® 3533 SN 01 Polyether Block Amide (PEBA) (Conditioned) POLYETHER BLOCK AMIDE (PEBA) hardness 35 shore D Non plasticized flexible Polyamide Outstanding mechanical properties at low temperature (-40°C) Applications: molded parts for sport goods (softness.. |
|||
Vicat Softening Point | 74.0 °C | 165 °F | 50°C/hr; 50N |
Arkema Group Evatane® 1003 VL 4C Ethylene Vinyl Acetate EVA copolymer made by high pressure tubular process. Anti-UV stabilized grade. Applications Thermal and colorless agricultural film to 180 at 200 µ for greenhouse coverage.ISO data provided by the .. |
|||
Vicat Softening Point | 74.0 °C | 165 °F | 50°C/hr; 50N |
Arkema Group Evatane® 1004 VL 4E Ethylene Vinyl Acetate EVA copolymer made by high pressure tubular process. Anti-UV stabilized grade. Applications Thermal and colorless agricultural film to 180 at 200 µ for greenhouse coverage.ISO data provided by the .. |
|||
Vicat Softening Point | 74.0 °C | 165 °F | |
BASF Procom® D 1187 Polypropylene Data was collected by ISO methods and provided by BASF. |
|||
Vicat Softening Point | 74.0 °C | 165 °F | |
BASF Procom® T20C 556 Polypropylene Uses: car heater casings, electrical and domestic appliance components (e.g. motor housings, dryer drums), industrial and agricultural plant components, textile bobbins.Data was collected by ISO met.. |