Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 186 °C | 367 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Valox® V2000DM PBT (Asia Pacific) Unreinforced, directly metallizable PBT injection molding resin with high flow better release characteristics. |
|||
Vicat Softening Point | 186 °C | 367 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Valox® V2000DM PBT (Europe-Africa-Middle East) Unreinforced, directly metallizable PBT injection molding resin with high flow better release characteristics. |
|||
Vicat Softening Point | 186 °C | 367 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Valox® V2000DM PBT Unreinforced, directly metallizable PBT injection molding resin with high flow better release characteristics. |
|||
Vicat Softening Point | 186 °C | 367 °F | ISO 306 |
Suzhou Hipro Polymers Hiprolon® 11 PFB Colorized Nylon powder Hiprolon® 11 PFB colorized is a fluid-bed polyamide powder fully comprised of bio-renewable raw materials. It has excellent weather ability, chemical resistance, wear resistance, impact resistanc.. |
|||
Vicat Softening Point | 186 °C | 367 °F | ISO 306 |
Suzhou Hipro Polymers Hiprolon® 211 PES Colorized Nylon powder Hiprolon® 211 PES colorized electrostatic polyamide powder is fully comprised of bio-renewable raw materials. It has excellent weather ability, chemical resistance, wear resistance, impact resist.. |
|||
Vicat Softening Point | 186 °C | 367 °F | ASTM D1525 |
Lubrizol Isoplast® 101LGF40BLK Engineering Thermoplastic Polyurethane Resin Available in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Isoplast product line from Dow in 2009. |
|||
Vicat Softening Point | 186 °C | 367 °F | ASTM D1525 |
Lubrizol Isoplast® 101LGF40NAT Engineering Thermoplastic Polyurethane Resin Available in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Isoplast product line from Dow in 2009. |
|||
Vicat Softening Point | 186 °C | 367 °F | ASTM D1525 |
Lubrizol Isoplast® 101LGF60BLK Engineering Thermoplastic Polyurethane Resin Available in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Isoplast product line from Dow in 2009. |
|||
Vicat Softening Point | 186 °C | 367 °F | ASTM D1525 |
Lubrizol Isoplast® 101LGF60NAT Engineering Thermoplastic Polyurethane Resin Available in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Isoplast product line from Dow in 2009. |
|||
Vicat Softening Point | 186 °C | 367 °F | ASTM D1525 |
Lubrizol Isoplast® 2540 Engineering Thermoplastic Polyurethane Resin for Medical Applications Features: USP Class VIAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Isoplast product line from Dow in 2009. |
|||
Vicat Softening Point | 186 °C | 366 °F | ASTM D1525 |
Lubrizol ISOPLAST™ 2560 Engineering Thermoplastic Polyurethane Resin for Medical Applications Features: USP Class VIAvailable in Americas, Europe, Middle East, Africa, India and AsiaAvailableInformation provided by LubrizolLubrizol acquired the Isoplast product line from Dow in 2009. |
|||
Vicat Softening Point | 186 °C | 367 °F | |
Covestro Apec® HT KU 1-9357/2 High-Heat Polycarbonate, 20% Glass Fiber Only opaque colors available, with 20% glass fiber reinforcement, flame retardant.Applications: Lighting, electrical parts.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience.. |
|||
Vicat Softening Point | 186 °C | 367 °F | B/120; ISO 306 |
Eurostar Staramide BG4ST43 PA6, Glass Fiber Filled, Impact Modified, Injection Molded Staramide BG4ST43 is an Impact Modified and Glass Fiber Reinforced, Polyamide 6, Injection Molding ResinInformation provided by Eurostar. |
|||
Vicat Softening Point | 186 °C | 367 °F | ASTM D1525 |
Arkema Group ORGASOL® 1002 D Nat 1 Polyamide 6 Information provided by Arkema Group |
|||
Vicat Softening Point | 186 °C | 367 °F | 50°C/h 50N; ISO 306 |
LATI LASULF G/30 30% Glass Reinforced Polysulfone (PSU)
(Unverified Data**) Description: Lasulf products are composed of polysulfone (PSU). They feature good thermal and mechanical properties such as excellent toughness, even at low temperatures, excellent dimensional stabi.. |