Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 121 °C | 250 °F | ISO 306/A50 |
Premix Thermoplastics PRE-ELEC® PE 1297 Conductive Thermoplastic Compound PRE-ELEC® PE 1297 is a conductive thermoplastic compound based on PE-HD. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELEC® PE.. |
|||
Vicat Softening Point | 121 °C | 250 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics GELOY HRA170D ASA+PC (Europe-Africa-Middle East) GELOY HRA170D resin is a PC-ASA blend with permanent antistatic behavior. It is typically used in applications that require antidust properties and high impact retention. Geloy HRA170D resin is typi.. |
|||
Vicat Softening Point | 121 °C | 250 °F | Compression Molded; ASTM D1525 |
NOVA Chemicals Surpass® RMs539-U Octene sMDPE Rotational Molding Film Features: Octene copolymerExceptional low temperature impact propertiesOutstanding stiffnessBroad processing windowSuperior whiteness for improved part appearanceEasy mold releaseNSF listed for Stan.. |
|||
Vicat Softening Point | 121 °C | 250 °F | Compression Molded; ASTM D1525 |
NOVA Chemicals Surpass® RMs539-UG Octene sMDPE Rotational Molding Film Features: Octene copolymerExceptional low temperature impact propertiesOutstanding stiffnessBroad processing windowSuperior whiteness for improved part appearanceEasy mold releaseNSF listed for Stan.. |
|||
Vicat Softening Point | 121 °C | 250 °F | ASTM D1525 |
Chevron Phillips HiD® 9326 HDPE Natural Pipe Resin
(discontinued **) Resin Type: Linear Copolymer; PE3408 Pipe Resin; ASTM D 3350 Classification: 335440A; ASTM D 4976 Classification: PE 235, A 56606Applications:Base Resin for use in Oil Patch and Industrial Pipe Appl.. |
|||
Vicat Softening Point | 121 °C | 250 °F | ASTM D1525 |
Chevron Phillips HiD® 9638 HDPE Sheeting and Blown Film Resin
(discontinued **) Resin Type: Sheeting Resin for the Geomembrane Market; ASTM D 4976 Classification: PE 225, A 56507Applications:Cast Geomembrane Applications, Notion and Millinery Bags, Heavy Duty Shipping Sacks, In.. |
|||
Vicat Softening Point | 121 °C | 250 °F | ASTM D1525 |
NOVA Chemicals Sclair® 16A Butene HDPE Film Resin
(discontinued **) Film Properties. Features: Low gel, good barrier properties.Applications: Merchandising bags, lamination, co-extrusion.Data provided by the manufacturer. |
|||
Vicat Softening Point | 121 - 212 °C | 250 - 414 °F | Average value: 154 °C Grade Count:16 |
Overview of materials for Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Glass Filled". Each property range of values repor.. |
|||
Vicat Softening Point | 121 °C | 250 °F | ASTM D1525 |
LyondellBasell Alathon® ETP H4745 High Density Polyethylene ApplicationsALATHON H 4745 is a new, multi-purpose, high-flow resin featuring enhanced cold temperature impact performance, enhanced processability and thermal stability for fast cycling and exhibit.. |
|||
Vicat Softening Point | 121 °C | 250 °F | ASTM D1525 |
LyondellBasell Alathon® ETP H4837 High Density Polyethylene ApplicationsALATHON H 4837 is a high-flow “freezer†grade resin that exhibits enhanced cold temperature impact performance, enhanced processability and thermal stability, with good color a.. |
|||
Vicat Softening Point | 121 °C | 250 °F | ASTM D1525 |
Ineos T50-3600 HDPE Ineos T50-3600 is a high density polyethylene copolymer of narrow molecular weight distribution used primarily for high speed injection molding of thin-walled articles. It is characterized by a hig.. |
|||
Vicat Softening Point | 121 °C | 250 °F | ISO 306 |
Iran Petrochemical (PCC) MF3713 High Density Polyethylene MF3713 is a high molecular weight high density polyethylene.Applications: bags, products for use in property modification.Information provided by Iran Petrochemical Commercial Co. |
|||
Vicat Softening Point | 121 °C | 250 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Xenoy® 6620U PBT+PC PBT+PC, Unfilled, Impact Modified, UV stabilized. Outstanding low temperature impact performance and chemical resistance. |
|||
Vicat Softening Point | 121 °C | 250 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics XYLEX X8409AC PC+POLYESTER PC + Polyester, Injection (Blow) Molding, or Extrusion Blow molding grade, Chemical Resistance and Transparency |
|||
Vicat Softening Point | 121 °C | 250 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics XYLEX X8409AC PC+POLYESTER (Europe-Africa-Middle East) PC + Polyester, Injection (Blow) Molding, or Extrusion Blow molding grade, Chemical Resistance and Transparency |
|||
Vicat Softening Point | 121 °C | 250 °F | B/50; ISO R306 |
Samsung Cheil Industries Infino® HP-1011 PC/ABS, Unreinforced Material with superior flowability and small gas generation that can be used in the exterior material of mobile phonesInformation provided by Samsung Cheil Industries. |
|||
Vicat Softening Point | 121 °C | 250 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Valox® V3900WX PBT+PC PBT/PC blend - Unreinforced - Flame Retardant. This is a UV-stabilized grade designed for outdoor enclosure applications requiring UL 746C F1 weatherability performance. |
|||
Vicat Softening Point | 121 °C | 250 °F | Loading 1, Rate A; ASTM D1525 |
Chevron Phillips Marlex® 9005 HDPE Injection Molding Resin Resin Type: Hexene CopolymerCharacteristics: Moderate flowExcellent impact strengthExcellent ESCRGood warpage resistanceApplications: Industrial partsSeatsFood and household containersAgricultural p.. |
|||
Vicat Softening Point | 121 °C | 250 °F | ASTM D1525 |
ExxonMobil Paxon™ BA50-100 Blow Molding Resin Product Description: BA50-100 is a high molecular weight, high density polyethylene copolymer. This resin has superior stress crack resistance, high impact strength and good rigidity.Availability: .. |
|||
Vicat Softening Point | 121 °C | 250 °F | |
Dow DOWLEX™ IP-40 High Density Polyethylene DOWLEX® IP-40 resin is an improved processing high density resin designed to offer excellent processability and impact resistance required for food container applications. This resin is designed by.. |
|||
Vicat Softening Point | 121 °C | 250 °F | |
Dow HDPE 42047N High Density Polyethylene DOW HDPE 42047N resin is a narrow molecular weight distribution copolymer designed to combine high impact strength and environmental stress crack resistance with excellent processability over a wide.. |
|||
Vicat Softening Point | 121 °C @Load 0.999 kg |
250 °F @Load 2.20 lb |
ISO 306 |
Arkema Group OREVAC® 18510P Grafted Maleic Anhydride Polyethylene OREVAC 18510P is a maleic anhydride grafted polyethylene used in the manufacturing of three layer MDPE or HDPE coating for steel pipeline. It is a powder product. OREVAC 18510P is mainly used in pip.. |
|||
Vicat Softening Point | 121 °C | 250 °F | ISO 306 |
Arkema Group OREVAC® 18750 Maleic Anhydride Modified Polypropylene DescriptionOREVAC 18750 is a coextrusion coating adhesive based on a maleic anhydride modified polypropylene resin. It combines the processability of an extrusion coating resin with the thermal resi.. |
|||
Vicat Softening Point | 121 °C @Load 1.02 kg |
250 °F @Load 2.25 lb |
ISO 306 |
Arkema Group Pebax® Rnew 40R53 SP 01 Polyether Block Amide (PEBA) Polyether block amide Pebax® 40R53 SP 01 is a thermoplastic elastomer made of flexible polyether and rigid polyamide based on renewable resources. This SP grade has been developed to be heat and UV.. |
|||
Vicat Softening Point | 121 °C | 250 °F | 50°C/hr; 50N |
Arkema Group Pebax® MV 1074 SN 01 Polyether Block Amide (PEBA) (Conditioned) POLYETHER BLOCK AMIDE (PEBA) hardness 40 shore D breathable (high permeability to H2O vapor,CO2,O2) permanent antistatic grade Applications: breathable films (medical, textile....) Permanent antista.. |
|||
Vicat Softening Point | 121 °C @Load 1.02 kg |
250 °F @Load 2.25 lb |
ASTM-D1525 |
Braskem Symbios 4102 Polypropylene Terpolymer Braskem Symbios 4102 is a medium melt flow rate terpolymer with a heat seal temperature below 120ºC on its treated face. It is designed for use as a heat sealing layer on bioriented films (BOPP) an.. |
|||
Vicat Softening Point | 121 °C | 250 °F | ASTM D1525 |
ExxonMobil Paxon™ BC50-100 Sheet Extrusion and Blow Molding Resin
(discontinued **) BC50-100 is a high molecular weight, high density polyethylene copolymer. This resin has superior stress crack resistance, high impact strength and good rigidity.Information provided by ExxonMobil .. |
|||
Vicat Softening Point | 121 °C | 250 °F | ISO 306 |
Total Lacqtene® 6002 FLG 42 HDPE film
(discontinued **) LACQTENE® 6002 FLG 42 is a medium density polyethylene resin with hexene as comonomer. This shows a broad molecular weight distribution ensuring outstanding processability. LACQTENE® 6002 FLG 42 h.. |
|||
Vicat Softening Point | 121 °C | 250 °F | ASTM D1525 |
Huntsman Rexell® H2104 Injection Molding LLDPE
(discontinued **) Linear-low high density homopolymer, injection molding, FDA compliant.Features: High flow and short cycle times.Applications: Thin wall containers.FDA Notes: Conforms to FDA regulation 21 CFR 177.15.. |
|||
Vicat Softening Point | 121 °C | 250 °F | ASTM D1525 |
ExxonMobil Paxon™ AG45-004 Blow Molding Resin
(discontinued **) AG45-004 is a blow molding high density polyethylene which offers exceptional stress crack resistance and impact performance. It contains an antistat which permits this resin to be used in all food.. |