Polymer Property : Vicat Softening Point = 280 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Vicat Softening Point 280 - 320 °C
536 - 608 °F
Average value: 307 °C Grade Count:3
Overview of materials for Polyaryletherketone (PAEK), Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyaryletherketone (PAEK), Carbon Fiber Filled". Each property range of values reported is minimum and ..
Vicat Softening Point 280 °C
536 °F
DIN ISO 306
Lehmann & Voss LUVOCOM® 1105-7198/BK PEEK, with PTFE
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Chemical and hydrolysis resistance parts, non flammable.Improved friction and wear behavio..
Vicat Softening Point 280 °C
536 °F
DIN ISO 306
Lehmann & Voss LUVOCOM® 1105-7741 PEEK, with mineral filler, lubricant modified
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Dynamic stressed parts at high movement velocity.Chemical and hydrolysis resistance parts,..
Vicat Softening Point 280 °C
536 °F
DIN ISO 306
Lehmann & Voss LUVOCOM® 1t-7370 Polyamide 6/6T, with carbon fiber, toughness-modified
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Reduced moment of inertia compared with metal parts.Electrically conductive..
Vicat Softening Point 280 °C
536 °F
DIN ISO 306
Lehmann & Voss LUVOCOM® 2205-7123 Blend based on polyaryl ether ketone, with carbon fiber, PTFE, lubricant modified
Applications: High dimensionally stable precision parts, high continuous use temperature.Especially suitable for medical parts, superheated steam sterilizable, hydrolysis resistanceChemical and hydr..
Vicat Softening Point 280 °C
536 °F
DIN ISO 306
Lehmann & Voss LUVOTECH® GS 46 Polyamide 46, lubricant modified, heat stabilized
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Emergency running property.Isotropic shrinkage characteristics.Highly dimensionally stable at e..
Vicat Softening Point 280 °C
536 °F
DIN ISO 306
Lehmann & Voss LUVOCOM® 1105/GR/15/TF/15-2 PEEK, with PTFE, lubricant modified
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Dynamic stressed parts at high movement velocity.Chemical and hydrolysis resistance parts,..
Vicat Softening Point 280 °C
536 °F
DIN ISO 306
Lehmann & Voss LUVOCOM® 1105/MS/15/TF/15 PEEK, with PTFE, lubricant modified
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Dynamic stressed parts at high movement velocity.Chemical and hydrolysis resistance parts,..
Vicat Softening Point 280 °C
536 °F
DIN ISO 306
Lehmann & Voss LUVOCOM® 1105-7740 PEEK, lubricant modified, heat stabilized
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Dynamic stressed parts at high movement velocity.Chemical and hydrolysis resistance parts,..
Vicat Softening Point 280 °C

@Load 5.00 kg
536 °F

@Load 11.0 lb
LATI Laramid G/60 PPA, 60% Glass Fiber Reinforced
Semi-aromatic polyamide (PPA) based compound. Glass fibers. Very good thermal properties. Good chemical resistance. Low moisture absorption.Availability: Africa & Middle East; Asia Pacific; Europe; ..
Vicat Softening Point 280 °C
536 °F
DIN ISO 306
Lehmann & Voss LUVOCOM® 1105/TF/20/NAT PEEK, with PTFE
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Chemical and hydrolysis resistance parts, non flammable.Improved friction and wear behavio..
Vicat Softening Point 280 °C
536 °F
50°C/h 50N; ISO 306
DSM Stanyl® TE350 Nylon 46 (European and Asian Grade) (Dry)  (discontinued **)
Stanyl is a high performance polyamide providing unmatched performance and value across an amazingly broad range of automotive and electronic applications. Stanyl offers:Highest mechanical propertie..
Vicat Softening Point 280 °C
536 °F
DIN ISO 306
Lehmann & Voss LUVOCOM® 1105-7825 PEEK, with PTFE
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Chemical and hydrolysis resistance parts, non flammable.Improved friction and wear behavio..
Vicat Softening Point 280 °C

@Load 5.00 kg
536 °F

@Load 11.0 lb
LATI Latilub 88/50-30GRT PEEK, Graphite/PTFE Filled
Self-lubricating product based on Polyetheretherketone (PEEK). Graphite / PTFE.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Indu..