Polymer Property : Vicat Softening Point = 367 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Vicat Softening Point 186 °C
367 °F
Rate B/50; ISO 306
SABIC Innovative Plastics Valox® V2000DM PBT (Asia Pacific)
Unreinforced, directly metallizable PBT injection molding resin with high flow better release characteristics.
Vicat Softening Point 186 °C
367 °F
Rate B/50; ISO 306
SABIC Innovative Plastics Valox® V2000DM PBT (Europe-Africa-Middle East)
Unreinforced, directly metallizable PBT injection molding resin with high flow better release characteristics.
Vicat Softening Point 186 °C
367 °F
Rate B/50; ISO 306
SABIC Innovative Plastics Valox® V2000DM PBT
Unreinforced, directly metallizable PBT injection molding resin with high flow better release characteristics.
Vicat Softening Point 186 °C
367 °F
ISO 306
Suzhou Hipro Polymers Hiprolon® 11 PFB Colorized Nylon powder
Hiprolon® 11 PFB colorized is a fluid-bed polyamide powder fully comprised of bio-renewable raw materials. It has excellent weather ability, chemical resistance, wear resistance, impact resistanc..
Vicat Softening Point 186 °C
367 °F
ISO 306
Suzhou Hipro Polymers Hiprolon® 211 PES Colorized Nylon powder
Hiprolon® 211 PES colorized electrostatic polyamide powder is fully comprised of bio-renewable raw materials. It has excellent weather ability, chemical resistance, wear resistance, impact resist..
Vicat Softening Point 186 °C
367 °F
ASTM D1525
Lubrizol Isoplast® 101LGF40BLK Engineering Thermoplastic Polyurethane Resin
Available in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Isoplast product line from Dow in 2009.
Vicat Softening Point 186 °C
367 °F
ASTM D1525
Lubrizol Isoplast® 101LGF40NAT Engineering Thermoplastic Polyurethane Resin
Available in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Isoplast product line from Dow in 2009.
Vicat Softening Point 186 °C
367 °F
ASTM D1525
Lubrizol Isoplast® 101LGF60BLK Engineering Thermoplastic Polyurethane Resin
Available in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Isoplast product line from Dow in 2009.
Vicat Softening Point 186 °C
367 °F
ASTM D1525
Lubrizol Isoplast® 101LGF60NAT Engineering Thermoplastic Polyurethane Resin
Available in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Isoplast product line from Dow in 2009.
Vicat Softening Point 186 °C
367 °F
ASTM D1525
Lubrizol Isoplast® 2540 Engineering Thermoplastic Polyurethane Resin for Medical Applications
Features: USP Class VIAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Isoplast product line from Dow in 2009.
Vicat Softening Point 186 °C
367 °F
Covestro Apec® HT KU 1-9357/2 High-Heat Polycarbonate, 20% Glass Fiber
Only opaque colors available, with 20% glass fiber reinforcement, flame retardant.Applications: Lighting, electrical parts.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience..
Vicat Softening Point 186 °C
367 °F
B/120; ISO 306
Eurostar Staramide BG4ST43 PA6, Glass Fiber Filled, Impact Modified, Injection Molded
Staramide BG4ST43 is an Impact Modified and Glass Fiber Reinforced, Polyamide 6, Injection Molding ResinInformation provided by Eurostar.
Vicat Softening Point 186 °C
367 °F
ASTM D1525
Arkema Group ORGASOL® 1002 D Nat 1 Polyamide 6
Information provided by Arkema Group
Vicat Softening Point 186 °C
367 °F
50°C/h 50N; ISO 306
LATI LASULF G/30 30% Glass Reinforced Polysulfone (PSU)  (Unverified Data**)
Description: Lasulf products are composed of polysulfone (PSU). They feature good thermal and mechanical properties such as excellent toughness, even at low temperatures, excellent dimensional stabi..