Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 90.0 °C | 194 °F | ASTM D-1525 |
Plaskolite Optix® CP - 41 General Purpose Acrylic Resin OPTIX® general purpose acrylics are available in a variety of performance grades that offer varying melt flow rates, heat resistance, color/opacity and gloss levels.Information provided by Plaskoli.. |
|||
Vicat Softening Point | 90.0 °C | 194 °F | ASTM D-1525 |
Plaskolite West Optix® CA - 41 FDA General Purpose Acrylic Resin Generally unaffected by alkalis, hydrocarbons, non-oxidizing acids, and salt water. Transparent, translucent, opaque, and custom colors in various grades of melt flow rate and heat resistance are av.. |
|||
Vicat Softening Point | 90.0 °C | 194 °F | 50 N - 50°C/h; ISO 306/B |
Polimeri Europa Edistir RK 451G Polystyrene UL94 V-0, polybromobiphenylether (PBBE) free, flame retarded, high impact polystyrene. This grade combines medium flow, heat resistance and good light stability for injection moulding of technical p.. |
|||
Vicat Softening Point | 90.0 °C | 194 °F | 10 N - 50°C/h; ISO 306/A |
Polimeri Europa Edistir SR 550 Polystyrene High impact, easy flow polystyrene with good elasticity at low temperatures.Suitable for injection moulding of large or complex parts with low thickness and high impact strength.
Designation: Thermo.. |
|||
Vicat Softening Point | 90.0 °C @Load 1.00 kg |
194 °F @Load 2.20 lb |
ISO 306/A |
Polimeri Europa Riblene® FL 24 Low Density Polyethylene - Blown Film Extrusion Riblene FL 24 is a low density polyethylene (LDPE) with added slip and antiblocking agents, suitable for blown film extrusion. Riblene FL 24 is characterized by a good balance between processabilit.. |
|||
Vicat Softening Point | 90.0 °C | 194 °F | |
Polycasa Acryl® KR 2015/1 Acrylic, Impact Grade Medium-impact grade with very good flow behavior, especially mechanically stressed parts with long flow paths; e.g. strip light diffusers. Can be extruded into thin tubes, sheet and film.Data was c.. |
|||
Vicat Softening Point | 90.0 °C | 194 °F | |
Dow Pellethane® 2103-90AEN Polyurethane Elastomer, Ether Based
(discontinued **) PELLETHANE® 2103-90AEN is a polytetramethylene glycol ether based polyurethane elastomer featuring superior resilience, low temperature properties, excellent hydrolytic stability, and resistance to.. |
|||
Vicat Softening Point | 90.0 °C | 194 °F | ASTM D1525 |
Eastman 800A Polyethylene
(discontinued **) Polyethylene 800A is a general-purpose low density formulation used for injection molding applications that require good stress-crack resistance. Polyethylene 800E is used in general-purpose extrus.. |
|||
Vicat Softening Point | 90.0 °C | 194 °F | ASTM D1525 |
Eastman Voridian D4053-A Polyethylene
(discontinued **) Voridian polyethylene D4053-A is a low density formulation used for injection molding. It is an outstanding material for molding lids and other container closures because it processes easily on aut.. |
|||
Vicat Softening Point | 90.0 °C | 194 °F | ASTM D1525 |
LyondellBasell Petrothene® NA951000 Low Density Polyethylene ApplicationsPETROTHENE NA 951 is a series of homopolymer resins specially designed for industrial and consumer packaging and liner and bag applications. NA 951 has an excellent balance of processab.. |
|||
Vicat Softening Point | 90.0 °C | 194 °F | ASTM D1525 |
LyondellBasell Petrothene® NA963083 Low Density Polyethylene ApplicationsPETROTHENE NA 963 is a series of resins formulated with special antiblock additive and designed for a wide variety of industrial film applications where high impact strength and excellen.. |
|||
Vicat Softening Point | 90.0 °C @Load 5.00 kg |
194 °F @Load 11.0 lb |
50°C/h; ASTM D1525 |
LG Chemical HIPS 60HRI PS, Impact Modified Description: Injection Molding, PS, General Purpose, Impact ModifiedApplication: TV Sets, Tape Recorders, Vacuum Cleaner, Washing Machine, Air ConditionerCAS: 9003-55-8Information provided by LG Che.. |
|||
Vicat Softening Point | 90.0 °C | 194 °F | ASTM D1525 |
LG Chemical LUTENE FB3000 LDPE Extrusion of Blown Film Description: LUTENE FB3000 is mainly intended for the extrusion of blown film with high mechanical property for the clarity bags in all thickness. LUTENE FB3000 have high mechanical property and ena.. |
|||
Vicat Softening Point | 90.0 °C | 194 °F | ASTM D1525 |
LG Chemical SEETEC BF500 LDPE Characteristics: Good Processability and Good Optical Properties Additives: Antiblocking Agent, Slip AgentApplications: Industrial Film & Food PackageCAS No. 9002-88-4Information provided by LG Chem.. |
|||
Vicat Softening Point | 90.0 °C @Load 5.00 kg |
194 °F @Load 11.0 lb |
|
LATI Latene® 7-V2 PP Homopolymer, Flame Retardant Polypropylene homopolymer (PPh) based compound. UL94 V-2 classified, with brominated flame retardants, PBB/PBDE free. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North A.. |
|||
Vicat Softening Point | 90.0 °C | 194 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics NORYL V090 PPE+HIPS (Europe-Africa-Middle East) NORYL V090 is an unfilled, flame retardant material with a Vicat B/120 of 95 °C according ISO 306. NORYL V090 is V0 at 2.0 mm and V1 at 1.6 mm according UL94 and halogen free according VDE/DIN 47.. |
|||
Vicat Softening Point | 90.0 °C | 194 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Noryl V190 PPE+HIPS (Europe-Africa-Middle East) NORYL V190 is an unfilled flame retardant material with a Vicat B/120 of 90°C according ISO 306. NORYL V190 is V1 at 2.0 mm according UL94 and halogen free according VDE/DIN 472 part 815.This dat.. |
|||
Vicat Softening Point | 90.0 °C | 194 °F | VST/B/50; ISO 306 |
Styrolution Luran® S 797 S UV White 33999 Q455 ASA Description: Grade with especially high notched impact strengthApplications: Lighting covers and lawn mower housings.Information provided by STYROLUTION, which is a joint venture between BASF and IN.. |
|||
Vicat Softening Point | 90.0 °C | 194 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics XYLEX FXY330DF PC+POLYESTER (Europe-Africa-Middle East) Polyester+PC alloy. Diffusion Effect. Color package may affect performance. |
|||
Vicat Softening Point | 90.0 °C | 194 °F | ASTM D1525 |
Lubrizol Estane® X-585A-31 Thermoplastic Polyurethane Type: Estane® X585A-31 is a Shore 95A, polyester grade without lubricant thermoplastic polyurethane (TPU). USP Class VI Certified.Uses: Extrusion, Film Blowing.Information Provided by The Lubrizol.. |
|||
Vicat Softening Point | 90.0 °C | 194 °F | ASTM D1525 |
UBE F522 Polyethylene Description: UBE Polyethylene is polymerized at high pressure using a tubular reactor. Production conditions are strictly controlled ensuring the product's superior physical and mechanical prope.. |
|||
Vicat Softening Point | 90.0 °C @Load 1.02 kg |
194 °F @Load 2.25 lb |
50°C per hour; ASTM D1525 |
Total PS CPDS 815 High Flow, Non-Deca Polystyrene Total Petrochemicals Polystyrene 815 is a high heat resistant, high impact Polystyrene for injection molding. It is recommended for the manufacturing of articles which require good dimensional stab.. |
|||
Vicat Softening Point | 90.0 °C | 194 °F | ASTM D1525 |
Lubrizol Estane® CS195A Thermoplastic Polyurethane Type: Estane® CS195A is a Shore 95A, polyester grade, calendering processible thermoplastic polyurethane (TPU). FDA approved (21 CFR 177.2600, 177.1680).Uses: Calendering, Molt roll processing.Inf.. |
|||
Vicat Softening Point | 90.0 °C | 194 °F | B50 (50N); ISO 306 |
Domo 1102J Polypropylene Homopolymer Information provided by Domo. |
|||
Vicat Softening Point | 90.0 °C | 194 °F | |
Dow ATTANE™ 4202 Ultra Low Density Polyethylene, Cast Film Grade ATTANE® 4202 copolymer is an ultra low density polyethylene having excellent tear and puncture resistance with good optics. It is designed for cast films used in food packaging applications. It com.. |
|||
Vicat Softening Point | 90.0 °C | 194 °F | ASTM D1525 |
Dow DNDA-8350 NT 7 Linear Low Density Polyethylene Resin DOW DNDA-8350 NT 7 is produced using UNIPOL™ PE process technology. It is intended for use in general purpose injection molding applications. Information provided by Dow |
|||
Vicat Softening Point | 90.0 °C | 194 °F | ASTM D1525 |
Dow FLEXOMER™ ETS-9078 NT 7 Very Low Density Polyethylene (VLDPE) Resin FLEXOMER™ ETS-9078 NT 7 is intended primarily for slot cast extrusion. This narrow molecular weight distribution resin has outstanding drawdown properties and produces low modulus cast films, high.. |
|||
Vicat Softening Point | 90.0 °C @Thickness 2.00 mm |
194 °F @Thickness 0.0787 in |
molded plaque, cured 20 hr at 100°C; ASTM D1525 |
BASF Elastollan® 1180A10 Wire & Cable Grade Polyurethane Elastomer As with all TPU products this grade must be dried prior to processing.Information provided by BASF Corporation. |
|||
Vicat Softening Point | 90.0 °C | 194 °F | ASTM D1525 |
PlastxWorld CEVIAN® SER23 ABS General purpose and flame retarded ABS with excellent moldability and no plate-out.These are typical values and are not intended for specification purposes. UL approved file No. is E47773. Informat.. |
|||
Vicat Softening Point | 90.0 °C | 194 °F | ASTM D1525 |
Huntsman PE1353 EVA Film Extrusion
(discontinued **) 3.5% Vinyl Acetate EVA copolymer and FDA compliantFeatures: Excellent balance of optical and strength, toughness and flexibility at low temperatures, and good heat seal characteristic.Applications: .. |