Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 95.0 °C @Load 1.00 kg |
203 °F @Load 2.20 lb |
ISO 306/A |
Polimeri Europa Clearflex® H&T CLH 150 Linear Low Density Polyethylene Clearflex H&T CLH 150 is a linear low density polyethylene resin, with antioxidants, suitable for cast film extrusion.Stretch films obtained from Clearflex H&T CLH 150 show good optical properties, .. |
|||
Vicat Softening Point | 95.0 °C @Load 1.00 kg |
203 °F @Load 2.20 lb |
ASTM D1525B |
SABIC PS 325 High Impact Polystyrene for Injection Molding Product Description: High Impact Polystyrene PS 325 is manufactured by continuous mass polymerization of styrene monomer. An elastomer is incorporated during polymerization to achieve impact resis.. |
|||
Vicat Softening Point | 95.0 °C | 203 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Cycoloy® C2800 PC+ABS (Europe-Africa-Middle East) Non-chlorinated and non-brominated flame retardant PC+ABS offering balanced flow and impact properties for various applications. |
|||
Vicat Softening Point | 95.0 °C | 203 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Cycoloy® FXC630SK PC+ABS (Asia Pacific) PC+ABS, ECO-conforming flame retardant with diamond sparkle appearance. |
|||
Vicat Softening Point | 95.0 °C | 203 °F | ASTM D1525 |
ExxonMobil LL 6100 Injection Molding Resin
(discontinued **) LL 6100 is a narrow molecular weight butene copolymer designed for applications that require easy processability. This resin offers outstanding toughness and tear resistance in freezer applications .. |
|||
Vicat Softening Point | 95.0 °C | 203 °F | ASTM D1525 |
Eastman 1810E Polyethylene
(discontinued **) Polyethylene 1810E contains no additives. It is suggested for general purpose extrusion applications requiring good stress crack resistance or electrical properties. It is used in applications suc.. |
|||
Vicat Softening Point | 95.0 °C | 203 °F | ASTM D1525 |
Eastman 1924P Polyethylene
(discontinued **) Low-density polyethylene 1924P is a resin in the boardstock coating industry for use in breadboard, cupstock, and liquid packaging board. This material has an excellent combination of low neck-in, .. |
|||
Vicat Softening Point | 95.0 °C | 203 °F | ASTM D1525 |
Eastman E6838-922F Polyethylene
(discontinued **) E6838-922F is a low density formulation with medium slip and medium antiblock. Outstanding optical properties make this material an excellent choice for food packaging applications.List of Applicat.. |
|||
Vicat Softening Point | 95.0 °C | 203 °F | ASTM D1525/A |
Gichem GILAC G160 Acrylonitrile Butadiene Styrene
(discontinued **) ABS very high fluidity, good resilience. Medium-High Injection speed.Information provided by GICHEM Gruppo Industriale Chimico |
|||
Vicat Softening Point | 95.0 °C | 203 °F | ASTM D1525 |
LyondellBasell Petrothene® NA340141 Low Density Polyethylene ApplicationsPETROTHENE NA 340 is a LDPE/EVA copolymer resin designed for quality bags and special film applications requiring clarity and excellent impact strength. Typical applications include hea.. |
|||
Vicat Softening Point | 95.0 °C | 203 °F | ISO 306B |
Lucite International Diakon® CRG812 Acrylic Polymer, Toughened Compound The Diakon® impact PMMA series offer the best combination of impact, chemical and heat resistance and provide rigidity and surface hardness. The grades in the Diakon® series can be processed b.. |
|||
Vicat Softening Point | 95.0 °C | 203 °F | ISO 306A |
Lucite International Diakon® ST35G6 Toughened Acrylic Polymer The Diakon® impact PMMA series offer the best combination of impact, chemical and heat resistance and provide rigidity and surface hardness. The grades in the Diakon® series can be processed b.. |
|||
Vicat Softening Point | 95.0 °C | 203 °F | ISO 306B |
Lucite International Diakon® ST35G8 Toughened Acrylic Polymer The Diakon® impact PMMA series offer the best combination of impact, chemical and heat resistance and provide rigidity and surface hardness. The grades in the Diakon® series can be processed b.. |
|||
Vicat Softening Point | 95.0 °C | 203 °F | 1000 g; ASTM D1525 |
LG Chemical 40 AF Flame Retardant HIPS High impact, Safety standards: listed with UL CSA, and classified according to IEC 707, Meet requirements for flammability, mechanical and electrical properties, Applications include televisions, VT.. |
|||
Vicat Softening Point | 95.0 °C | 203 °F | resin; ASTM D1525 |
Lotte Chemical Titan TITANLENE® LDF200GG Low density polyethylene LDF200GG is a low density polyethylene resin for film extrusion. LDF200GG has medium slip and anti-block additives. LDF200GG meets the U.S. Food and Drug Administration (FDA) criteria for food conta.. |
|||
Vicat Softening Point | 95.0 °C | 203 °F | ASTM D1525 |
Hannam Chemical Hanalac 750 ABS, General Purpose FDA Approved. Good combination of impact strength, rigidity, gloss, heat resistance, processability, and thermal stability. May be injection molded. Its broad range of applications include: elect.. |
|||
Vicat Softening Point | 95.0 °C | 203 °F | 50°C/h; 50N; 10x10x4mm; ISO 306/B50 |
SYNTHOS Forsan® 449 Acrylonitrile Butadiene Styrene (ABS) High flow, high gloss, suitable for electroplating.Applications: General purpose, intricate and thin-walled productsHousehold appliances, vacuum cleaners, heels, toys, fan grilles, etc.Synthos was f.. |
|||
Vicat Softening Point | <= 95.0 °C | <= 203 °F | |
Sibur ABS 1106M Extrusion Grade ABS Plastic With high thermal and light resistance for production of sheets with following pneumatic and vacuum formation of internal parts for refrigerators and other articles of technical purpose. |
|||
Vicat Softening Point | <= 95.0 °C | <= 203 °F | |
Sibur ABS 2802 Extrusion Grade ABS Plastic With high deformation properties and impact strength for production of sheets with following pneumatic and vacuum forming of products of technical purpose. |
|||
Vicat Softening Point | 95.0 °C | 203 °F | B/50; ISO R306 |
Samsung Cheil Industries Starex® AS-0151BS ABS, Unreinforced Anti-static material that can be used in the housing of OA devices, IC, LSI carrier etc.Information provided by Samsung Cheil Industries. |
|||
Vicat Softening Point | 95.0 °C | 203 °F | ISO R-306 |
Samsung Cheil Industries Starex® WR-9750 Extrusion Grade ABS Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Vicat Softening Point | 95.0 °C | 203 °F | ISO 306/B50 |
Styron Magnumâ„¢ 8391 MED Acrylonitrile Butadiene Styrene (ABS) Resin Overview: MAGNUMâ„¢ MED ABS combines an excellent glossy appearance with high flow and medium impact performance. The mass (continuous process) ABS technology of Styron ensures an ABS resin that .. |
|||
Vicat Softening Point | 95.0 °C | 203 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics NORYL PPX PPX7110 PPE+PP (Europe-Africa-Middle East) PPX7110 is an alloy of PP and PPO, providing high impact and good heat resistance. Generic identification acc. ISO11469: >PP+PPE+PS-I |
|||
Vicat Softening Point | 95.0 °C | 203 °F | ASTM D1525 |
Total PSI 945E Polystyrene Polystyrene 945E is a high impact polystyrene designed for applications requiring extra toughness without sacrificing mechanical properties. Excellent falling dart impact combined with the high glos.. |
|||
Vicat Softening Point | 95.0 °C | 203 °F | A50; DIN 53460 |
Lubrizol ESTANE® 58447 Ester Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |
|||
Vicat Softening Point | 95.0 °C | 203 °F | |
Dow ATTANE™ 4201 Ultra Low Density Polyethylene, Blown Film Grade ATTANE® 4201 copolymer is an ultra low density polyethylene having high impact resistance and tear strength in blown films, designed for use in food packaging applications. It complies with FDA reg.. |
|||
Vicat Softening Point | 95.0 °C | 203 °F | |
Dow LDPE 5004I Low Density Polyethylene, Extrusion Coating Grade DOW Polyethylene 5004I extrusion coating resin is a low melt index resin for heavy duty applications such as paperboard coatings, milk cartons and folding cartons, aseptic package coatings, bag line.. |
|||
Vicat Softening Point | 95.0 °C @Load 0.999 kg |
203 °F @Load 2.20 lb |
ISO 306 |
Arkema Group OREVAC® 18334 Grafted Maleic Anhydride Polyethylene OREVAC 18334 is a grafted maleic anhydride polyethylene used in the manufacturing of multilayer oxygen barrier bottle. OREVAC 18334 is mainly used in multi-layer bottle and tank to have good adhesio.. |
|||
Vicat Softening Point | 95.0 °C | 203 °F | |
BASF Elastollan® C-85A Polyester Type Polyurethane Elastomer Processed by extrusion or injection molding. Elastollan C series of products are polyester-based thermoplastic polyurethanes that exhibit very good hydrolytic stability. They also exhibit excellen.. |
|||
Vicat Softening Point | 95.0 °C | 203 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics NORYL RN0612 PPE+HIPS (Europe-Africa-Middle East) Noryl RN0612 is an unfilled Post Consumer recycle (PCR) based injection moldable modified polyphenylene ether resin comprising at least 30% PCR styrenic series resin content. Designed for good dimen.. |