Polymer Property : Crystallization Temperature = 113 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Crystallization Temperature 113 °C
235 °F
ASTM D3418
ExxonMobil HD 6510 Injection Molding Resin  (discontinued **)
HD 6510 is a narrow molecular weight hexene copolymer designed for good processability and excellent balance of ESCR, Toughness, and Stiffness properties. This resin is ideally suited for a wide ra..
Crystallization Temperature 113 °C
235 °F
ASTM D3418
ExxonMobil HD 6510.17 Injection Molding Resin  (discontinued **)
HD 6510 is a narrow molecular weight hexene copolymer designed for good processability and excellent balance of ESCR, Toughness, and Stiffness properties. This resin is ideally suited for a wide ra..
Crystallization Temperature 113 °C
235 °F
ASTM D2117
SCG Chemicals EL-Leneâ„¢ M10 Butene (C4) Rotational Molding Resin
Color compound resin available in pellet / powder formKey Characteristics:High stiffnessGood processingFair impact resistanceTypical Applications: General-purpose products, such as small-to-medium ..
Crystallization Temperature 113 °C
235 °F
ASTM D2117
SCG Chemicals EL-Leneâ„¢ M3804 Butene (C4) Rotational Molding Resin
Natural base resin available in pellet / powder formKey Characteristics:High stiffnessGood processingFair impact resistanceTypical Applications: General-purpose products, such as small-to-medium wa..
Crystallization Temperature 113 °C
235 °F
ASTM D2117
SCG Chemicals EL-Leneâ„¢ M90 Butene (C4) Rotational Molding Resin
Color compound resin available in pellet / powder formKey Characteristics:High stiffness and toughnessGood ESCRFair processingTypical Applications: Large, thick-wall parts, high-load products, such..
Crystallization Temperature 113 °C
235 °F
ASTM D2117
SCG Chemicals EL-Leneâ„¢ M9001 Butene (C4) Rotational Molding Resin
Natural base resin available in pellet / powder formKey Characteristics:High stiffness and toughnessGood ESCRFair processingTypical Applications: Large, thick-wall parts, high-load products, such a..
Crystallization Temperature 113 °C
235 °F
ASTM D-3418
Chevron Phillips Marlex® HMN TR-938/938G Polyethylene; MDPE
Medium density polyethylene. These hexene copolymers are tailored for rotational molding applications that require: Wide process windows and good flowLong-term UV stabilizationExcellent impact stre..
Crystallization Temperature 113 °C
235 °F
ASTM D-3418
Chevron Phillips Marlex® HMN TR-942/942G Polyethylene; HDPE
High density polyethylene. These hexene copolymers are tailored for rotational molding applications that require: Wide process windows and fair flowLong-term UV stabilizationExcellent impact stren..
Crystallization Temperature 113 °C
235 °F
ASTM D-3418
Chevron Phillips Marlex® HMN TR-945/945G Polyethylene; HDPE
High density polyethylene. These hexene copolymers are tailored for rotational molding applications that require: Wide process windows and excellent flowLong-term UV stabilizationGood impact stren..
Crystallization Temperature 113 °C
235 °F
Equate Test Method
Equate EPDA-5040 HDPE Non-Pressure Gravity Pipe Resin
EPDA-5040 is a high molecular weight high density polyethylene copolymer resin designed for non-pressure gravity pipe applications. It has a good balance of flexibility, ductility, stiffness and tou..
Crystallization Temperature 113 °C
235 °F
Dow Method (DSC)
Dow DNDA-1081 NT 7 Linear Low Density Polyethylene Resin
DOW DNDA-1081 NT 7 is produced using UNIPOL™ PE process technology. It is intended for high-speed injection molding of thin walled parts such as downguaged lids. Information provided by Dow
Crystallization Temperature 113 °C
235 °F
Dow Method (DSC)
Dow DNDA-1082 NT 7 Linear Low Density Polyethylene Resin
DOW DNDA-1082 NT 7 is produced using UNIPOL™ PE process technology. It is intended for high-speed injection molding of thin walled parts such as downguaged lids. Information provided by Dow
Crystallization Temperature 113 °C
235 °F
Dow Method (DSC)
Dow DNDA-1149 NT 7 Linear Low Density Polyethylene Resin
DOW DNDA-1149 NT 7 is produced using UNIPOL™ PE process technology and is intended for high-speed injection molding applications. Information provided by Dow
Crystallization Temperature 113 - 115 °C
235 - 239 °F
Addcomp PRIEX® 20095 Maleic Anhydride Grafted PP homopolymer
Uses: Enhance sealability in bi-oriented polypropylene film packagingIncrease adhesion between metallic or textile wire and polymer coatingAchieve high compatibility between glass or other natural f..
Crystallization Temperature 113 °C
235 °F
Addcomp PRIEX® Ionomer 33101 HDPE
Ionomers will be used toStrengthen rigidity and hardness while maintaining impact resistance in polyolefinsMaintain adhesion even under contaminated conditions especially in fatty substratesReduce t..
Crystallization Temperature 113 - 115 °C
235 - 239 °F
Addcomp PRIEX® 20070 Maleic Anhydride Grafted PP homopolymer
Uses: Enhance sealability in bi-oriented polypropylene film packagingIncrease adhesion between metallic or textile wire and polymer coatingAchieve high compatibility between glass or other natural f..
Crystallization Temperature 113 - 115 °C
235 - 239 °F
ISO 11357-3
Addcomp PRIEX® 20097 Maleic Anhydride Grafted PP homopolymer
Fields of application: Functionalised polypropylene to be used as compatibiliser for polymer blends or coupling agent for glass fibre, wood flour, natural fibres, multilayer films, aluminium foils, ..
Crystallization Temperature 113 °C
235 °F
Addcomp PRIEX® Ionomer 30101 HDPE
Ionomers will be used toStrengthen rigidity and hardness while maintaining impact resistance in polyolefinsMaintain adhesion even under contaminated conditions especially in fatty substratesReduce t..