Polymer Property : Heat of Fusion = 54.0 J/g Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Heat of Fusion 54.0 - 60.0 J/g
23.2 - 25.8 BTU/lb
Crystallization Heat; ASTM D3417
Solvay Specialty Polymers Solef® 6008 Polyvinylidene Fluoride (PVDF)  (Unverified Data**)
Solef® 6008 PVDF homopolymer is a low-viscosity PVDF resin and is typically processed by injection molding.Information provided by Solvay Specialty Polymers.
Heat of Fusion 54.0 - 60.0 J/g
23.2 - 25.8 BTU/lb
Crystallization Heat; ASTM D3417
Solvay Specialty Polymers Solef® 6010 Polyvinylidene Fluoride (PVDF)  (Unverified Data**)
Solef® 6010 PVDF homopolymer has medium viscosity and is typically processed by extrusion.Information provided by Solvay Specialty Polymers.
Heat of Fusion 54.0 J/g
23.2 BTU/lb
Crystallization Heat
Solvay Specialty Polymers Solef® 1015/0078 PVDF Homopolymer  (discontinued **)
Key features of this grade: Plasticized, Offshore, Piping, Formulated. Recommended processing is extrusion. Available as granules.General information about SOLEF® PVDF: SOLEF® PVDF is a fluorina..
Heat of Fusion 54.0 J/g
23.2 BTU/lb
ASTM D3417
Arkema Group Pebax® 7033 Polyether Block Amide (PEBA)
Information provided by Arkema Group