Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 20.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
11.1 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics Lexan® 3414R PC (Europe-Africa-Middle East) LEXAN 3414R is a high viscosity, 40% glass reinforced, flame retardant grade, especially designed for applications requiring high rigidity together with high heat resistance. |
|||
CTE, linear, Parallel to Flow | 20.0 - 30.0 µm/m-°C @Temperature 50.0 - 100 °C |
11.1 - 16.7 µin/in-°F @Temperature 122 - 212 °F |
ISO 11359-2 |
Raschig Group AMPLA® 2000 melamine-modified polyester Halogen-free, organically and inorganically filled melamine-modified Polyester molding compound. Low post-shrinkage, very good electrical values, high heat resistance, very good sliding behavior, ve.. |
|||
CTE, linear, Parallel to Flow | 20.0 - 30.0 µm/m-°C @Temperature 50.0 - 100 °C |
11.1 - 16.7 µin/in-°F @Temperature 122 - 212 °F |
ISO 11359-2 |
Raschig Group AMPLA® 2500 melamine-modified polyester Halogen-free, organically and inorganically filled melamine-modified Polyester molding compound. Excellent elasticity and shock resistance, low post-shrinkage, very good electrical values, high heat.. |
|||
CTE, linear, Parallel to Flow | 20.0 µm/m-°C @Temperature 23.0 - 55.0 °C |
11.1 µin/in-°F @Temperature 73.4 - 131 °F |
ISO 11359-1, -2 |
Lanxess Durethan® BKV 130 GIT DUS008 900116 Nylon 6, Impact Modified PA 6, 30% glass fibers, injection molding, impact modified, GIT/WITInformation provided by LANXESS. |
|||
CTE, linear, Parallel to Flow | 20.0 µm/m-°C | 11.1 µin/in-°F | ISO 11359-1/-2 |
Lanxess Durethan® BKV 130 H3.0 101006 Copolyamide, 30% Glass Fiber CoPA, injection molding grade, 30% glass fibers, elastomer-modified, electroplateable, higher notched impact strength and also higher energy absorption under biaxial impact load than BKV 30 H3.0, ev.. |
|||
CTE, linear, Parallel to Flow | 20.0 µm/m-°C | 11.1 µin/in-°F | ISO 11359-1/-2 |
Lanxess Durethan® BKV 140 H2.0 900051 Copolyamide, 40% Glass Fiber CoPA, injection molding grade, 40% glass fibers, elastomer-modified, electroplateable, higher notched impact strength and also higher energy absorption under biaxial impact load than BKV 40, even in.. |
|||
CTE, linear, Parallel to Flow | 20.0 µm/m-°C | 11.1 µin/in-°F | ISO 11359-1/-2 |
Lanxess Pocan® B 4235 000000 PBT, 30% Glass Fiber PBT, 30% glass fibers, injection molding, flame retardant |
|||
CTE, linear, Parallel to Flow | 20.0 µm/m-°C | 11.1 µin/in-°F | ISO 11359-1/-2 |
Lanxess Durethan® BKV 50 H2.0 EF 900116 Nylon 6, 50% Glass Fiber PA 6, injection molding grade, 50% glass fibers, good heat-ageing resistance, low viscosity (easy flow)Application Examples: mirror baseplates |
|||
CTE, linear, Parallel to Flow | 20.0 µm/m-°C @Temperature 23.0 - 85.0 °C |
11.1 µin/in-°F @Temperature 73.4 - 185 °F |
ISO 11359 |
Solvay TECHNYL® A 218G1 V30 Black 34N PA66, 30% glass fiber, DRY Description: Polyamide 66, reinforced with 30% of glass fiber, for injection molding. This grade shows an improved retention of properties after long term ageing in automotive cooling liquids. For 7.. |
|||
CTE, linear, Parallel to Flow | 20.0 µm/m-°C @Temperature 23.0 - 150 °C |
11.1 µin/in-°F @Temperature 73.4 - 302 °F |
ISO 11359-2 |
SABIC Innovative Plastics ULTEM 2310F PEI (Europe-Africa-Middle East) 30% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). Resin is RoHS compliant. UL94 V0 listing. US FDA and European Food Contact approved. Effective June, 2007 this grade will no longer be.. |
|||
CTE, linear, Parallel to Flow | 20.0 µm/m-°C @Temperature 23.0 - 150 °C |
11.1 µin/in-°F @Temperature 73.4 - 302 °F |
ISO 11359-2 |
SABIC Innovative Plastics ULTEM CRS5311 PEI (Europe-Africa-Middle East) 30% Glass fiber filled, enhanced flow Polyetherimide copolymer (Tg 225C) with enhanced chemical resistance to strong acids, bases, aromatics, and ketones. Resin is RoHS compliant. UL94 V0 and 5VA li.. |
|||
CTE, linear, Parallel to Flow | 20.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
11.1 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP THERMOCOMP DF0079 PC (Europe-Africa-Middle East) LNP* Thermocomp* DF0079 is a compound based on Polycarbonate resin containing Glass Fiber, Flame Retardant. Added features of this material include: Flame Retardant. |
|||
CTE, linear, Parallel to Flow | 20.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
11.1 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics Valox® 430 PBT (Europe-Africa-Middle East) VALOX 430 is 33% glass reinforced, impact modified PBT injection moulding resin. |
|||
CTE, linear, Parallel to Flow | 20.0 µm/m-°C | 11.1 µin/in-°F | ISO 11359-1/-2 |
Covestro Desmopan® DP 3970D Polyurethane, 20% Glass Filled injection molding grade20 % Glass fiber reinforcedgood heat resistancelow coefficent of linear thermal expansionApplicationAutomotive engineeringInjection molded engineering partsPreprocessingMax. W.. |
|||
CTE, linear, Parallel to Flow | 20.0 µm/m-°C @Temperature 20.0 °C |
11.1 µin/in-°F @Temperature 68.0 °F |
ISO 11359-1/-2 |
DSM Akulon® K224-LG6 Nylon 6-30% Glass Reinforced (European and Asian Grade) (Dry) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
CTE, linear, Parallel to Flow | 20.0 µm/m-°C @Temperature 20.0 °C |
11.1 µin/in-°F @Temperature 68.0 °F |
ISO 11359-1/-2 |
DSM Akulon® S223-G4U (Dry) 23% Glass Reinforced Nylon 66 (North America) Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis.. |
|||
CTE, linear, Parallel to Flow | 20.0 µm/m-°C | 11.1 µin/in-°F | ISO 11359-1/-2 |
EMS-Grivory Grivory® BG-30/2 PA6-GF30 Product description: Grilon BG-30/2 is a heat stabilized, normal viscosity PA6 injection molding grade with 30% glass fibers. Grilon BG-30/2 has the following important properties: High stiffnessGoo.. |
|||
CTE, linear, Parallel to Flow | 20.0 µm/m-°C @Temperature 20.0 °C |
11.1 µin/in-°F @Temperature 68.0 °F |
ISO 11359-1/-2 |
DSM Stanyl® TE250F6 (DAM) Nylon 46 30% Glass Reinforced, Heat Stabilized, Flame Retardant (North America) Information provided by DSM Engineering Plastics. |
|||
CTE, linear, Parallel to Flow | 20.0 µm/m-°C | 11.1 µin/in-°F | ISO 11359-1/-2 |
EMS-Grivory Grivory® EBGM-30 HX PA666-GF30 Product description: Grilon EBGM-30 HX is a specially heat stabilized PA66+PA6 injection molding grade with 30% glass fibers. Grilon EBGM-30 HX has the following important properties: High heat resi.. |
|||
CTE, linear, Parallel to Flow | 20.0 µm/m-°C | 11.1 µin/in-°F | ISO 11359-1/-2 |
EMS-Grivory Grivory® GVL-4H nat PA*-GF40 Product description: Grivory GVL-4H black is based on a combination of a heat stabilized semi-crystalline Polyamide with a partially aromatic Polyamide and 40% long glass fibers. Grivory GVL-4H blac.. |
|||
CTE, linear, Parallel to Flow | 20.0 µm/m-°C | 11.1 µin/in-°F | ISO 11359-1/-2 |
EMS-Grivory Grivory® HT2V-3H PA6T/66-GF30 Product description: Grivory HT2V-3H is a 30 % glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamde. Polymer designation acc. to ISO: .. |
|||
CTE, linear, Parallel to Flow | 20.0 µm/m-°C | 11.1 µin/in-°F | ISO 11359-1/-2 |
EMS-Grivory Grivory® TSGL-40/4 nat PA666-GF40 Product description: Grilon TSGL-40/4 natural is based on a heat stabilized semi-crystalline Polyamide PA66+PA6 and 40% long glass fibers. Grilon TSGL-40/4 natural is characterized by the following .. |
|||
CTE, linear, Parallel to Flow | 20.0 µm/m-°C | 11.1 µin/in-°F | ISO 11359-1/-2 |
EMS-Grivory Grivory® TSGZ-30 PA666-GF30 Product description: Grilon TSGZ-30 is a heat stabilized, normal viscosity, and impact modified PA66 + PA6 injection molding grade with 30% glass fibers. Grilon TSGZ-30 has the following important p.. |
|||
CTE, linear, Parallel to Flow | 20.0 µm/m-°C @Temperature -40.0 - 23.0 °C |
11.1 µin/in-°F @Temperature -40.0 - 73.4 °F |
ISO 11359-1/-2 |
DuPont Performance Polymers Rynite® FR530 BK507 Polyethylene Terephthalate (PET)
(Unverified Data**) 30% Glass Reinforced Flame Retardant Polyethylene Terephthalate Rynite FR530 BK507 is a 30% glass reinforced flame retardant modified polyethylene terephthalate resin.Information provided by DuPont .. |
|||
CTE, linear, Parallel to Flow | 20.0 µm/m-°C @Temperature -40.0 - 23.0 °C |
11.1 µin/in-°F @Temperature -40.0 - 73.4 °F |
DAM; ISO 11359-1/-2 |
DuPont Performance Polymers Zytel® HTN 51G35HSLR BK420 Polyphthalamide (PPA)
(Unverified Data**) 35% Glass Reinforced PPA High Performance Polyamide Zytel HTN51G35HSLR BK420 is a 35% glass reinforced heat stabilized lubricated high performance polyamide resin with improved hydrolysis resistance.. |
|||
CTE, linear, Parallel to Flow | 20.0 µm/m-°C @Temperature -40.0 - 23.0 °C |
11.1 µin/in-°F @Temperature -40.0 - 73.4 °F |
DAM; ISO 11359-1/-2 |
DuPont Performance Polymers Zytel® HTN FR52G30BL BK337 Polyphthalamide (PPA)
(Unverified Data**) 30% Glass Reinforced Flame Retardant PPA High Performance Polyamide Zytel HTNFR52G30BL BK337 is a 30% glass reinforced flame retardant lubricated high performance polyamide resin that has been devel.. |
|||
CTE, linear, Parallel to Flow | 20.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
11.1 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
Eurostar Staramide ACF3 PA66, 15% Carbon Fiber Reinforced, Heat stabilized, Injection Molding Staramide ACF3 is a 15% Carbon Fiber Reinforced Polyamide 66, Injection Molding ResinInformation provided by Eurostar. |
|||
CTE, linear, Parallel to Flow | 20.0 µm/m-°C @Temperature 20.0 °C |
11.1 µin/in-°F @Temperature 68.0 °F |
ISO 11359-1/-2 |
DSM Akulon® S223-G6 Nylon 66-30% Glass Reinforced (European and Asian Grade) (Dry) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
CTE, linear, Parallel to Flow | 20.0 - 25.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
11.1 - 13.9 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-1/-2 |
BASF Ultramid® B3EG6 30% Glass Filled PA6 (Dry) Ultramid B3EG6 is a 30% glass fiber reinforced injection molding PA6 grade. It conforms to FDA requirements of 21 CFR 177.1500. |
|||
CTE, linear, Parallel to Flow | 20.0 µm/m-°C | 11.1 µin/in-°F | ISO 11359-1/-2 |
EMS-Grivory Grivory® GVX-5 H nat PA*-GF50 Product description: Grivory GVX-5H natural is a 50% glass-fiber reinforced engineering thermoplastic material based on a combination of semi-crystalline polyamide with partially aromatic copolyamid.. |