Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 21.0 µm/m-°C @Temperature 20.0 °C |
11.7 µin/in-°F @Temperature 68.0 °F |
ISO data |
BASF Capron® HPN 9233G 33% Glass-Filled Nylon 6 (Dry)
(discontinued **) Capron HPN 9233G is a 33% glass reinforced polyamide 6 injection molding compound combining exceptional strength, stiffness and high temperature performance with excellent surface aesthetics. It is.. |
|||
CTE, linear, Parallel to Flow | 21.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
11.7 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP LUBRICOMP 5CL23 FP-V (PVDF) LNP* LUBRICOMP* 5CL23 is a compound based on PVDF resin containing 15% Carbon Fiber, 10% PTFE. Added features include: Wear Resistant. |
|||
CTE, linear, Parallel to Flow | 21.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
11.7 µin/in-°F @Temperature -22.0 - 86.0 °F |
|
Idemitsu Kosan Xarec® WA 212 SPS, 30% Glass Filled Crystalline Polymer, Glass Filled, Impact Modified. Used in Automotive and Industrial applications. |
|||
CTE, linear, Parallel to Flow | 21.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
11.7 µin/in-°F @Temperature -22.0 - 86.0 °F |
|
Idemitsu Kosan Xarec® WA 212LG SPS, 30% Glass Filled |
|||
CTE, linear, Parallel to Flow | 21.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
11.7 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP LUBRICOMP QCL34 PA6.10 LNP* LUBRICOMP* QCL34 is a compound based on Nylon 6/10 resin containing 15% PTFE, 20% Carbon Fiber. Added features of this material include: Wear Resistant, Electrically Conductive. |
|||
CTE, linear, Parallel to Flow | 21.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
11.7 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP Lubricomp RFL38 PA 66 (Europe-Africa-Middle East) LNP* Lubricomp* RFL38 is a compound based on Nylon 66 resin containing Glass Fiber, PTFE.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
CTE, linear, Parallel to Flow | 21.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
11.7 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP LUBRICOMP UFL36AS PPA LNP* LUBRICOMP* UFL36AS is a Polyphthalamide (PPA) base resin containing 30% Glass Fiber, 15% PTFE. Added features of this material are: Heat Stabilized, Wear Resistant. |
|||
CTE, linear, Parallel to Flow | 21.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
11.7 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP STAT-KON AE008XXY ABS LNP* STAT-KON* AE008XXY is a compound based on ABS resin containing 40% Carbon Fiber. Added feature of this material ia: Electrically Conductive. |
|||
CTE, linear, Parallel to Flow | 21.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
11.7 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP STAT-KON AX02747 ABS LNP* STAT-KON* AX02747 is a compound based on ABS resin containing Proprietary Filler(s). Added feature of this material is: Electrically Conductive. |
|||
CTE, linear, Parallel to Flow | 21.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
11.7 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP STAT-KON WEF42I PBT LNP* STAT-KON* WEF42I is a compound based on PBT resin containing 10% Carbon Fiber, 20% Glass Fiber. Added features of this grade include: High Impact, Electrically Conductive. |
|||
CTE, linear, Parallel to Flow | 21.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
11.7 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP THERMOCOMP WX05502 Polyester Elastomer LNP THERMOCOMP* WX05502 is a compound based on Polyester, TP resin containing Flame Retardant, Glass Fiber, Mineral. Added features of this material include: Flame Retardant. |
|||
CTE, linear, Parallel to Flow | 21.0 µm/m-°C @Temperature 20.0 °C |
11.7 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Sumitomo Bakelite North America 52-01 Short-Glass Reinforced Diallyl Phthalate Ortho Resin Isomer (DAP). Used for critical, high-performance military and commercial electrical components where long-term reliability is demanded.Meets the requirements of ASTM D5948 Type SDG.Inf.. |
|||
CTE, linear, Parallel to Flow | 21.0 µm/m-°C @Temperature 20.0 °C |
11.7 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Sumitomo Bakelite North America 52-70-70-VO-P Short-Glass Reinforced Diallyl Phthalate Ortho Resin Isomer (DAP). Used for critical, high-performance military and commercial electrical components where long-term reliability is demanded.Conforms with the requirements of ASTM D5948 Type.. |
|||
CTE, linear, Parallel to Flow | 21.0 µm/m-°C @Temperature 20.0 °C |
11.7 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Sumitomo Bakelite North America 73-70-70 C-P /73-70-70 VO-P Short-Glass Reinforced Diallyl Phthalate Ortho Resin Isomer (DAP). Used for critical, high-performance military and commercial electrical components where long-term reliability is demanded.Meets the requirements of ASTM D5948 Type SDG-F.I.. |
|||
CTE, linear, Parallel to Flow | 21.0 µm/m-°C @Temperature 20.0 °C |
11.7 µin/in-°F @Temperature 68.0 °F |
ASTM E-831 |
Sumitomo Bakelite North America RX® 1-520/RX® 1310 Short-Glass Reinforced Diallyl Phthalate Short glass fiber reinforced, non-flame retardant, diallyl ortho-phthalate molding compound which meets the requirements of ASTM D5948 Type SDG.Information provided by Vyncolit, a Sumitomo Bak Group.. |
|||
CTE, linear, Parallel to Flow | 21.0 µm/m-°C @Temperature 20.0 °C |
11.7 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Sumitomo Bakelite North America 52-20-30 Short-Glass Reinforced Diallyl Phthalate Ortho Resin Isomer (DAP). Used for critical, high-performance military and commercial electrical components where long-term reliability is demanded.Information provided by Sumitomo Bak North Americ.. |
|||
CTE, linear, Parallel to Flow | 21.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
11.7 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP VERTON RV00AESC PA 66 (Europe-Africa-Middle East) LNP* VERTON* RV00AESC is a compound based on PA 66 resin containing Long Glass Fiber. Added features include; Easy Molding, Heat Stabilized. |
|||
CTE, linear, Parallel to Flow | 21.0 µm/m-°C @Temperature -40.0 - 23.0 °C |
11.7 µin/in-°F @Temperature -40.0 - 73.4 °F |
DAM; ISO 11359-1/-2 |
DuPont Performance Polymers Zytel® 77G43L BK031 Nylon 612
(Unverified Data**) 43% Glass Reinforced Polyamide 612Information provided by DuPont Performance Polymers |
|||
CTE, linear, Parallel to Flow | 21.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
11.7 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
Eurostar Staramide AG8 PA66, 40% Glass Fiber Reinforced, Injection Molding Staramide AG8 is a 40% Glass Fiber Reinforced Polyamide 66, Injection Molding ResinInformation provided by Eurostar. |
|||
CTE, linear, Parallel to Flow | 21.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
11.7 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
Eurostar Staramide BG7H PA6, 35% Glass Fiber Filled, Heat Stabilized, Injection Molded Staramide BG7H is a Heat Stabilized, 35% Glass Fiber Reinforced, Polyamide 6, Injection Molding ResinInformation provided by Eurostar. |
|||
CTE, linear, Parallel to Flow | 21.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
11.7 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
Eurostar Staramide BG7HU PA6, 35% Glass Fiber Filled, Heat and UV Stabilized, Injection Molded Staramide BG7H is a Heat and UV Stabilized, 35% Glass Fiber Reinforced, Polyamide 6, Injection Molding ResinInformation provided by Eurostar. |
|||
CTE, linear, Parallel to Flow | 21.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
11.7 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
Eurostar Starflam AFR470X2 PA66, 35% Glass Filled, Injection Molded AFR470X2 is a Red Phosphorous, Flame Retardant, Glass Fiber Reinforced, Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive suppli.. |
|||
CTE, linear, Parallel to Flow | 21.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
11.7 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
Eurostar Staramide PF007 PA6, 35% Glass Fiber Filled, Injection Molded Staramide PF007 is a 35% Glass Fiber Reinforced, Polyamide 6 Injection Molding ResinInformation provided by Eurostar. |
|||
CTE, linear, Parallel to Flow | 21.0 µm/m-°C | 11.7 µin/in-°F | ISO 11359 |
BASF Ultramid® 8233G HS 33% Glass Filled PA6 (Dry) Ultramid 8233G HS is a heat stabilized, 33% glass fiber reinforced nylon 6 molding compound offering excellent strength, stiffness, high temperature performance and dimensional stability. It is also.. |
|||
CTE, linear, Parallel to Flow | 21.0 - 23.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
11.7 - 12.8 µin/in-°F @Temperature 73.4 - 176 °F |
DIN 11359-1/-2 |
BASF Ultramid® FRee A3U40G5 25% Glass Filled PA66 FR (Dry) Description: Flame retardant without halogens and red phosphorus, 25% glass fiber reinforced injection-molding grade; light colorable; outstanding mechanical and electrical properties.Information pr.. |
|||
CTE, linear, Parallel to Flow | 21.0 µm/m-°C @Temperature 20.0 °C |
11.7 µin/in-°F @Temperature 68.0 °F |
ISO data |
BASF Capron® 8233G 33% Glass-Filled Nylon 6 (Dry)
(discontinued **) Capron 8233G is a 33% glass fiber reinforced polyamide 6 molding compound offering excellent strength, stiffness, high temperature performance and dimensional stability. It is also available in he.. |
|||
CTE, linear, Parallel to Flow | 21.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
11.7 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP THERMOCOMP DX07408 PC LNP* THERMOCOMP* DX07408 is a compound based on Polycarbonate containing Proprietary Filler(s). Added feature of this grade is: UL Rated. |