Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 25.0 - 35.0 µm/m-°C @Temperature 50.0 - 150 °C |
13.9 - 19.4 µin/in-°F @Temperature 122 - 302 °F |
ISO 11359-2 |
Raschig Group DECAL® 5431 Phenolic Organically and inorganically filled phenolic molding compound. This product meets the allowed upper limits for heavy metals and PCAs and also conforms to the requirements of the EU directives 2002/.. |
|||
CTE, linear, Parallel to Flow | 25.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
13.9 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP LUBRICOMP DFL34XXP PC (Europe-Africa-Middle East) LNP* Lubricomp* DFL-4034 HP is a compound based on Polycarbonate resin containing Glass Fiber, PTFE. |
|||
CTE, linear, Parallel to Flow | 25.0 µm/m-°C @Temperature 20.0 °C |
13.9 µin/in-°F @Temperature 68.0 °F |
ISO data |
BASF Capron® GR20 20% Glass-Filled Nylon 6 (Dry)
(discontinued **) Capron GR20 is a 20% glass reinforced polyamide 6 injection molding compound possessing a balance of engineering properties combined with excellent processability and surface aesthetics. It is also.. |
|||
CTE, linear, Parallel to Flow | 25.0 µm/m-°C @Temperature 23.0 - 55.0 °C |
13.9 µin/in-°F @Temperature 73.4 - 131 °F |
ASTM E831 |
Lavergne VYPET VNT 840 HY PET 40% Glass-Mineral Reinforced Vypet VNT 840 HY is a 40% glass/mineral reinforced PET high strength injection molding compound with improved hydrolysis stability designed for electrical and structural applications, with High Diel.. |
|||
CTE, linear, Parallel to Flow | 25.0 µm/m-°C @Temperature 23.0 - 85.0 °C |
13.9 µin/in-°F @Temperature 73.4 - 185 °F |
ISO 11359 |
Solvay TECHNYL® A 218 V30 BK 34 NG-K PA66, 33% glass fiber, DRY Description: TECHNYL® A 218 V30 Black 34 NG-K is a polyamide 66, reinforced with 30% of glass fiber, heat stabilized, for injection molding. The product is available in black color. Benefits: Thi.. |
|||
CTE, linear, Parallel to Flow | 25.0 µm/m-°C @Temperature 23.0 - 150 °C |
13.9 µin/in-°F @Temperature 73.4 - 302 °F |
ISO 11359-2 |
SABIC Innovative Plastics ULTEM 2200 PEI (Europe-Africa-Middle East) 20% Glass fiber filled, standard flow Polyetherimide (Tg 217C). Resin is RoHS compliant. UL94 V0 and 5VA listing. |
|||
CTE, linear, Parallel to Flow | 25.0 µm/m-°C @Temperature 23.0 - 150 °C |
13.9 µin/in-°F @Temperature 73.4 - 302 °F |
ISO 11359-2 |
SABIC Innovative Plastics ULTEM 2200R PEI (Europe-Africa-Middle East) 20% Glass fiber filled, standard flow Polyetherimide (Tg 217C) with internal mold release. Resin is RoHS compliant. UL94 V0 and 5VA listing. |
|||
CTE, linear, Parallel to Flow | 25.0 µm/m-°C @Temperature 23.0 - 150 °C |
13.9 µin/in-°F @Temperature 73.4 - 302 °F |
ISO 11359-2 |
SABIC Innovative Plastics ULTEM 2210F PEI (Europe-Africa-Middle East) 20% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). Resin is RoHS compliant. US FDA and European Food Contact approved. Effective June, 2007 this grade will no longer be supported with b.. |
|||
CTE, linear, Parallel to Flow | 25.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
13.9 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics Valox® V9260DCS PET (Europe-Africa-Middle East) Color Stable Glass Filled PET (for Dark colors only) |
|||
CTE, linear, Parallel to Flow | 25.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
13.9 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP STAT-KON ZEF061XC PPO (Europe-Africa-Middle East) LNP* STATKON* ZEF061XC is a compound based on Polyphenyleneoxide resin containing Glass Fiber, Milled Carbon Fiber and Flame Retardant. Added Features include: Electrically Conductive |
|||
CTE, linear, Parallel to Flow | 25.0 µm/m-°C @Temperature 20.0 °C |
13.9 µin/in-°F @Temperature 68.0 °F |
ASTM E-831 |
Sumitomo Bakelite North America E 8353-706R-1 Hardware Grade Epoxy Fiberglass and mineral reinforced epoxy molding compound with excellent dimensional stability and good strength at elevated temperatures.Information provided by Vyncolit, a Sumitomo Bak Group |
|||
CTE, linear, Parallel to Flow | 25.0 µm/m-°C @Temperature 20.0 °C |
13.9 µin/in-°F @Temperature 68.0 °F |
ASTM E-831 |
Sumitomo Bakelite North America RX® 3-1-501N-P Mineral Filled Diallyl Phthalate Mineral filled, flame retardant, diallyl ortho-phthalate molding compound which meets the requirements of ASTM D5948 Type MDG-F.Information provided by Vyncolit, a Sumitomo Bak Group |
|||
CTE, linear, Parallel to Flow | 25.0 - 35.0 µm/m-°C @Temperature 20.0 °C |
13.9 - 19.4 µin/in-°F @Temperature 68.0 °F |
TMA |
Vyncolit 2923 W Novolac Phenolic Mineral filled phenolic molding compound with excellent heat resistance and dimensional stability.Information provided by Vyncolit, a Sumitomo Bak Group |
|||
CTE, linear, Parallel to Flow | 25.0 µm/m-°C | 13.9 µin/in-°F | ISO 11359-1/-2 |
DSM Arnite® AV2 370 XL-T PET-GF35 35% Glass Reinforced, Low Outgassing, Thermal conductive material |
|||
CTE, linear, Parallel to Flow | 25.0 µm/m-°C | 13.9 µin/in-°F | ISO 11359-1/-2 |
EMS-Grivory Grivory® BG-25 S PA6-GF25 Product description: Grilon BG-25 S is a heat stabilized PA6 injection molding grade with 25 % glass fibers. Grilon BG-25 S has the following important properties: Excellent surface finishEasy flowi.. |
|||
CTE, linear, Parallel to Flow | 25.0 µm/m-°C | 13.9 µin/in-°F | ISO 11359-1/-2 |
EMS-Grivory Grivory® BG-35 S PA6-GF35 Information provided by EMS Grivory |
|||
CTE, linear, Parallel to Flow | 25.0 µm/m-°C | 13.9 µin/in-°F | dry; ISO 11359-1/-2 |
DSM Stanyl® TC153 PA46 FR(17) Thermal conductive material, Flame Retardant, Heat Stabilized |
|||
CTE, linear, Parallel to Flow | 25.0 µm/m-°C | 13.9 µin/in-°F | dry; ISO 11359-1/-2 |
DSM Stanyl® TW271B3 (PA46+PTFE)-CF15 15% Carbon Reinforced, Heat Stabilized, Wear and Friction Modified |
|||
CTE, linear, Parallel to Flow | 25.0 µm/m-°C | 13.9 µin/in-°F | dry; ISO 11359-1/-2 |
DSM Stanyl® TW272B6 (PA46+PTFE)-CF30 30% Carbon Reinforced, Heat Stabilized, Wear and Friction Modified |
|||
CTE, linear, Parallel to Flow | 25.0 µm/m-°C | 13.9 µin/in-°F | ISO 11359-1/-2 |
EMS-Grivory Grivory® TSG-25/4 PA666-GF25 Information provided by EMS Grivory |
|||
CTE, linear, Parallel to Flow | 25.0 µm/m-°C | 13.9 µin/in-°F | ISO 11359-1/-2 |
DuPont Performance Polymers Rynite® 940 NC010 Polyethylene Terephthalate (PET)
(Unverified Data**) 40% Glass/Mineral Reinforced Polyethylene TerephthalateInformation provided by DuPont Performance Polymers |
|||
CTE, linear, Parallel to Flow | 25.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
13.9 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
Eurostar Staramide AG6K PA66, 30% Glass Filled, Injection Molded AG6 is a Heat and Hydrolytically Stabilized, 30% Glass Fiber Reinforced Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive suppli.. |
|||
CTE, linear, Parallel to Flow | 25.0 µm/m-°C | 13.9 µin/in-°F | ISO 11359-1/-2 |
DSM Arnite® AV2 370 XT PET-GF35 35% Glass Reinforced, Applications with extremely narrow tolerances |
|||
CTE, linear, Parallel to Flow | 25.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
13.9 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
Eurostar Staramide BG6 PA6, 30% Glass Filled, Injection Molded BG6 is a 30% Glass Fiber Reinforced Polyamide 6 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
CTE, linear, Parallel to Flow | 25.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
13.9 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
Eurostar Staramide RF006XXP PA66, 30% Glass Fiber Filled, Injection Molded Staramide RF006XXP is a 30% Glass Fiber Reinforced Polyamide 66 Injection Molding Resin (also known as RF1006)Information provided by Eurostar. |
|||
CTE, linear, Parallel to Flow | 25.0 µm/m-°C | 13.9 µin/in-°F | ISO 11359 |
BASF Ultradur B 4040 G10 High Speed BK15029 50% Glass Filled PBT/PET Ultradur B 4040 G10 High Speed BK15029 is a high flow, fast cycling with low warpage, 50% glass filled, injection molding PBT for industrial parts, rigid tough and dimensional stable applications. |
|||
CTE, linear, Parallel to Flow | 25.0 µm/m-°C @Temperature 20.0 °C |
13.9 µin/in-°F @Temperature 68.0 °F |
ISO data |
BASF Capron® GR30 HS 30% Glass-Filled Nylon 6 (Dry)
(discontinued **) Capron GR30 HS is a heat stabilized 30% glass reinforced polyamide 6 injection molding compound possessing a balance of engineering properties combined with excellent processability and surface aest.. |
|||
CTE, linear, Parallel to Flow | 25.0 µm/m-°C @Temperature 20.0 °C |
13.9 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Sumitomo Bakelite North America FS-6 CAF Mineral Filled Diallyl Phthalate Isophthalate DAP Resin Isomer. Used for critical, high-performance military and commercial electrical components where long-term reliability is demanded.Meets the requirements of ASTM D5948 Type MI.. |
|||
CTE, linear, Parallel to Flow | 25.0 µm/m-°C @Temperature 20.0 °C |
13.9 µin/in-°F @Temperature 68.0 °F |
ASTM E-831 |
Sumitomo Bakelite North America RX® 1-501N Mineral Filled Diallyl Phthalate Mineral filled diallyl ortho-phthalate molding compound which meets the requirements of ASTM D5948 Type MDG.Information provided by Vyncolit, a Sumitomo Bak Group |