Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 25.2 µm/m-°C @Temperature -40.0 - 95.0 °C |
14.0 µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E 831 |
SABIC Innovative Plastics NORYL SE1GFN3 PPE+PS PPE+PS blend. 30% Glass reinforced. Non-brominated, non-chlorinated FR system. UL94 V1 listing. RTI 110/105/110. Dielectric strength. Dimensional stability. Suitable for E/E applications. |
|||
CTE, linear, Parallel to Flow | 25.2 µm/m-°C @Temperature -40.0 - 95.0 °C |
14.0 µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E 831 |
SABIC Innovative Plastics NORYL SE1GFN3 PPE+PS (Asia Pacific) GR 30%. 275F (135C) DTUL. UL94 V-1 rated. Halogen free flame retardant. For electrical construction market. |
|||
CTE, linear, Parallel to Flow | 25.2 µm/m-°C @Temperature -40.0 - 40.0 °C |
14.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP LUBRICOMP Lexan_LF1530A PC (Europe-Africa-Middle East) LNP* Lubricomp* Lexan_FL1530 compound is a 30% glass reinforced, 15% PTFE filled PC. Flame retardant and wear resistant. Tight tolerances. |
|||
CTE, linear, Parallel to Flow | 25.2 µm/m-°C @Temperature -20.0 - 150 °C |
14.0 µin/in-°F @Temperature -4.00 - 302 °F |
ASTM E 831 |
SABIC Innovative Plastics ULTEM 2200 PEI 20% Glass fiber filled, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing. NSF 51 listing, WRAS certification in recognized colors. |
|||
CTE, linear, Parallel to Flow | 25.2 µm/m-°C @Temperature -20.0 - 150 °C |
14.0 µin/in-°F @Temperature -4.00 - 302 °F |
ASTM E 831 |
SABIC Innovative Plastics ULTEM 2200 PEI (Asia Pacific) 20% Glass fiber filled, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing. NSF 51 listing, WRAS certification in recognized colors. |
|||
CTE, linear, Parallel to Flow | 25.2 µm/m-°C | 14.0 µin/in-°F | ASTM D696 |
Techmer ES Elastoblend® PBT GF33 IM 33% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: Impact ModifierFeatures: Impact ModifiedInformation provided by TP Composites,.. |
|||
CTE, linear, Parallel to Flow | 25.2 µm/m-°C @Temperature -40.0 - 40.0 °C |
14.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP THERMOCOMP DF0049 PC LNP THERMOCOMP* DF0049 is a compound based on Polycarbonate resin containing 20% Glass Fiber. Added features of this material include: Flame Retardant. |
|||
CTE, linear, Parallel to Flow | 25.2 µm/m-°C @Temperature -40.0 - 40.0 °C |
14.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP THERMOCOMP DF0049 PC (Asia Pacific) LNP* THERMOCOMP* DF0049 is a compound based on Polycarbonate resin containing Flame Retardant, Glass Fiber. Added features of this material include: Flame Retardant. |
|||
CTE, linear, Parallel to Flow | 25.2 µm/m-°C | 14.0 µin/in-°F | ASTM D696 |
Techmer ES Luriblend® PA6/6 GF30 TS1 BK 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 30% Filler by WeightAdditive: Heat Stabilizer, Silicone Lubricant and PTFE Lubricant(15%)Features: Lubricated, Good Wear R.. |
|||
CTE, linear, Parallel to Flow | 25.2 µm/m-°C | 14.0 µin/in-°F | ASTM D696 |
Techmer ES Luriblend® PA6/6 GF40 ML2 HS 40% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 40% Filler by WeightAdditive: Heat Stabilizer and Molybdenum Disulfide Lubricant(2%)Features: Lubricated and Heat Stabiliz.. |
|||
CTE, linear, Parallel to Flow | 25.2 µm/m-°C | 14.0 µin/in-°F | ASTM D696 |
Techmer ES Luriblend® PA6/6 GF40 ML2 HS BK 40% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 40% Filler by WeightAdditive: Heat Stabilizer and Molybdenum Disulfide Lubricant(5%)Features: Lubricated and Heat Stabiliz.. |
|||
CTE, linear, Parallel to Flow | 25.2 µm/m-°C | 14.0 µin/in-°F | ASTM D696 |
Techmer ES Luriblend® PA6/6 GF43 ML2 43% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 43% Filler by WeightAdditive: Molybdenum Disulfide Lubricant(2%)Features: LubricatedInformation provided by TP Composites,.. |
|||
CTE, linear, Parallel to Flow | 25.2 µm/m-°C | 14.0 µin/in-°F | ASTM D696 |
Techmer ES Luriblend® PA6/6 GF43 ML2 BK 43% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 43% Filler by WeightAdditive: Molybdenum Disulfide Lubricant(2%)Features: Lubricated Appearance: BlackTPCI# 8047101Informa.. |
|||
CTE, linear, Parallel to Flow | 25.2 µm/m-°C @Temperature -40.0 - 40.0 °C |
14.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP THERMOCOMP ECF62 PEI LNP* THERMOCOMP* ECF62 is a compound based on Polyetherimide resin containing 30% Glass Fiber, 10% Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
CTE, linear, Parallel to Flow | 25.2 µm/m-°C @Temperature -30.0 - 30.0 °C |
14.0 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP THERMOCOMP RX06421S PA 66 LNP* Thermocomp* RX06421S is a compound based on Nylon 66 resin containing Glass Fiber. Added features of this material include: Easy Molding. |
|||
CTE, linear, Parallel to Flow | 25.2 µm/m-°C | 14.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill® PBT GF/M40 BK 40% Glass/Mineral Filler Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass/Mineral, 40% Filler by WeightAppearance: BlackInformation provided by TP Composites, Inc. |
|||
CTE, linear, Parallel to Flow | 25.2 µm/m-°C | 14.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill® PBT GF20 20% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 20% Filler by WeightInformation provided by TP Composites, Inc. |
|||
CTE, linear, Parallel to Flow | 25.2 µm/m-°C | 14.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill® TPX-PBT-98010 BN069 Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/ReinforFeatures: High DensityAppearance: Light BeigeProcessing Method: Injection MoldingInformation provided by TP C.. |
|||
CTE, linear, Parallel to Flow | 25.2 µm/m-°C @Temperature 20.0 °C |
14.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
PlastxWorld CEVIAN® SKG20 20% GF ABS Glass fiber reinforced, heat resistant and flame retarded ABS.These are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by Plast.. |
|||
CTE, linear, Parallel to Flow | 25.2 µm/m-°C | 14.0 µin/in-°F | ASTM D696 |
Ensinger TECAPEI® 20% Glass Reinforced, made from Ultem® 2200 PEI TECAPEI™ is an amorphous thermoplastic polyetherimide (PEI) made from Sabic Innovative Plastics' Ultem® 1000 and 2000 series resins. The unreinforced 1000 series materials are translucent amber in.. |
|||
CTE, linear, Parallel to Flow | 25.2 µm/m-°C | 14.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill FR® PA6/6 GF20 FR 20% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 20% Filler by WeightFeatures: Flame RetardantInformation provided by TP Composites, Inc. |