Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 27.0 µm/m-°C @Temperature -40.0 - 95.0 °C |
15.0 µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® FL920 PC Various weight reductions at .250"" (6.35 mm) wall, 20% GR. Excellent flex mod, high tensile strength/heat resistance. V-0/5V at .250"" (6.35mm). |
|||
CTE, linear, Parallel to Flow | 27.0 µm/m-°C | 15.0 µin/in-°F | ASTM D696 |
Ravago Manufacturing Americas Hylon® N1213HL BK Nylon 6/6 Available in North America Filler: Glass Fiber Reinforcement, 13% Filler by WeightAdditive: Heat Stabilizer and Lubricant Features: Lubricated and Heat StabilizedRoHS CompliantForm: Pellets Proces.. |
|||
CTE, linear, Parallel to Flow | 27.0 µm/m-°C @Temperature -40.0 - 95.0 °C |
15.0 µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® FL920 PC (Asia Pacific) Various weight reductions at .250"" (6.35 mm) wall, 20% GR. Excellent flex mod, high tensile strength/heat resistance. V-0/5V at .250"" (6.35mm). |
|||
CTE, linear, Parallel to Flow | 27.0 µm/m-°C | 15.0 µin/in-°F | ASTM D696 |
Solvay Specialty Polymers Mindel® B-322 Polysulfone, Modified (PSU, Modified)
(discontinued **) Mindel B-322 is a glass filled, modified polysulfone developed specifically for molded electrical connector applications requiring excellent dimensional stability and resistance to warpage. This mat.. |
|||
CTE, linear, Parallel to Flow | 27.0 µm/m-°C @Temperature 20.0 °C |
15.0 µin/in-°F @Temperature 68.0 °F |
|
Cookson Group Plaskon® 3100 Novolac Epoxy Molding Compound
(discontinued **) Test specimens were transfer molded and post cured 4 hours at 175°C.A flame retardant, novolac-hardened epoxy molding compound recommended for semiconductor packages that are not stress sensitive. |
|||
CTE, linear, Parallel to Flow | 27.0 µm/m-°C @Temperature 23.0 - 85.0 °C |
15.0 µin/in-°F @Temperature 73.4 - 185 °F |
ISO 11359 |
Solvay TECHNYL® A 218 V25 Black 21 N PA66, 25% glass fiber, DRY Description: TECHNYL® A 218 V25 is a polyamide 66, reinforced with 25% of glass fiber, heat stabilized, for injection molding. This product is available in natural and black colors.Benefits: The .. |
|||
CTE, linear, Parallel to Flow | 27.0 µm/m-°C @Temperature 23.0 - 85.0 °C |
15.0 µin/in-°F @Temperature 73.4 - 185 °F |
ISO 11359 |
Solvay TECHNYL® A 218 V25 Natural B PA66, 25% glass fiber, DRY Description: Polyamide 66, reinforced with 25% of glass fiber, specially stabilized to improve its resistance to oils and greases, for injection molding.Available in: EuropeProduct Applications: Thi.. |
|||
CTE, linear, Parallel to Flow | 27.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
15.0 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP LUBRICOMP QFL36 PA6.10 (Europe-Africa-Middle East) LNP*Lubricomp* QFL36 is a compound based on PA 6/10 resin containing Glass Fiber, PTFE. Added features include: Internally Lubricated. |
|||
CTE, linear, Parallel to Flow | 27.0 µm/m-°C | 15.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill FR® PBT GF30 FR-S AS 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 30% Filler by WeightAdditive: AntistaticFeatures: Flame Retardant, Antistatic and Non-BloomingProcessing Method: Injection.. |
|||
CTE, linear, Parallel to Flow | 27.0 µm/m-°C | 15.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill FR® TPX-HTN-01031 35% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 35% Filler by WeightAdditive: Heat Stabilizer Features: Flame Retardant, Heat Stabilized and High Temperature Strength UL .. |
|||
CTE, linear, Parallel to Flow | 27.0 µm/m-°C | 15.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill® PET GF/M35 35% Glass/Mineral Fiber Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass/Mineral, 35% Filler by WeightInformation provided by TP Composites, Inc. |
|||
CTE, linear, Parallel to Flow | 27.0 µm/m-°C | 15.0 µin/in-°F | ASTM D696 |
Techmer ES Luriblend® PA4/6 CF30 TL15 30% Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber, 30% Filler by WeightAdditive: PTFE Lubricant(15%)Features: Lubricated, Good Wear Resistance and Low FrictionInformation p.. |
|||
CTE, linear, Parallel to Flow | 27.0 µm/m-°C | 15.0 µin/in-°F | ASTM D696 |
Techmer ES Luriblend® PA6/10 GF30 TS15 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 30% Filler by WeightAdditive: Heat Stabilizer and PTFE+ Silicone LubricantFeatures: Lubricated, Heat Stabilizer and Good W.. |
|||
CTE, linear, Parallel to Flow | 27.0 µm/m-°C | 15.0 µin/in-°F | ASTM D696 |
Techmer ES Luriblend® PA6/6 GF30 IM TL15 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 30% Filler by WeightAdditive: Heat Stabilizer, Impact Modifier and PTFE Lubricant(15%)Features: Lubricated, Good Wear Resi.. |
|||
CTE, linear, Parallel to Flow | 27.0 µm/m-°C | 15.0 µin/in-°F | ASTM D696 |
Techmer ES Luriblend® PA6/6 GF30 TL5 LE 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 30% Filler by WeightAdditive: PTFE Lubricant(15%)Features: Lubricated, Good Wear Resistance, Low Friction and Low Extracta.. |
|||
CTE, linear, Parallel to Flow | 27.0 µm/m-°C | 15.0 µin/in-°F | ASTM D696 |
Techmer ES Luriblend® PPA CF30 TL15 30% Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber, 30% Filler by WeightAdditive: PTFE Lubricant(15%)Features: Lubricated, Good Wear Resistance, High Heat Resistance and Low.. |
|||
CTE, linear, Parallel to Flow | 27.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
15.0 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP THERMOCOMP Lexan_LGK3020 PC LNP* Thermocomp* Lexan_LGK3020 compound is a glass reinforced. Flame retardant. |
|||
CTE, linear, Parallel to Flow | 27.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
15.0 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP THERMOCOMP Lexan_LGK3020 PC (Europe-Africa-Middle East) LNP* Thermocomp* Lexan_LGK3020 compound is a glass reinforced, flame retardant material. |
|||
CTE, linear, Parallel to Flow | 27.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
15.0 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP THERMOCOMP RF0069SZ PA 66 LNP* THERMOCOMP* RF0069SZ is a compound based on Nylon 66 resin containing 30% Glass Fiber. Added features of th is grade include: Flame Retardant, Heat Stabilized. |
|||
CTE, linear, Parallel to Flow | 27.0 µm/m-°C | 15.0 µin/in-°F | ASTM E831 |
Sumitomo Bakelite North America E 2748-9641D Short Glass Fiber Reinforced Epoxy E 2748-9641D is a mineral and short fiberglass filled epoxy molding compound.Information provided by Sumitomo Bak North America, Inc. |
|||
CTE, linear, Parallel to Flow | 27.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
15.0 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP THERMOCOMP LX97024 PEEK (Europe-Africa-Middle East) LNP* LUBRICOMP* LX97024 is a compound based on Polyetheretherketone containing Glass Fiber, PTFE. Added features include: Internally Lubricated, Easy Molding. |
|||
CTE, linear, Parallel to Flow | 27.0 µm/m-°C | 15.0 µin/in-°F | ASTM D696 |
Techmer ES Luriblend® PPA CF30 TL10 30% Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber, 30% Filler by WeightAdditive: PTFE Lubricant(10%)Features: Lubricated, Good Wear Resistance, High Heat Resistance and Low.. |
|||
CTE, linear, Parallel to Flow | 27.0 µm/m-°C | 15.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill FR® PBT GF30 FR X 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 30% Filler by WeightFeatures: Flame RetardantUL File Number: E157318TPCI# 1006011Information provided by TP Composites, In.. |