Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 20.0 µm/m-°C | 11.1 µin/in-°F | Z Direction |
Premix Premi-Glas® 2206-22 CR-SX Fiberglass Reinforced Thermoset SMC Premi-Glas® 2206-22 CR-SX is a fiberglass reinforced thermoset sheet molding compound for electrical, flame retardant and HVAC applications.Key features and benefits are:Non-Halogen FR technology f.. |
|||
CTE, linear, Parallel to Flow | 20.0 - 30.0 µm/m-°C @Temperature 50.0 - 100 °C |
11.1 - 16.7 µin/in-°F @Temperature 122 - 212 °F |
ISO 11359-2 |
Raschig Group AMPLA® 2000 melamine-modified polyester Halogen-free, organically and inorganically filled melamine-modified Polyester molding compound. Low post-shrinkage, very good electrical values, high heat resistance, very good sliding behavior, ve.. |
|||
CTE, linear, Parallel to Flow | 20.0 - 25.0 µm/m-°C @Temperature 50.0 - 150 °C |
11.1 - 13.9 µin/in-°F @Temperature 122 - 302 °F |
ISO 11359-2 |
Raschig Group DECAL® 666/8 Phenolic Glass-fiber reinforced phenolic molding compound with mineral fillers. High heat resistance, reduced mould shrinkage and post-shrinkage, good chemical resistance and mechanical properties. This prod.. |
|||
CTE, linear, Parallel to Flow | 20.0 µm/m-°C | 11.1 µin/in-°F | ASTM D696 |
Kuraray Genestarâ„¢ G1301A-M61 Nylon, 30% Glass Filled 30% Glass reinforced and impact modified injection grade.Main Features:Higher elongation and impact strengthHeat resistanceChemical resistanceExample of applications:Quick connector |
|||
CTE, linear, Parallel to Flow | 20.0 µm/m-°C | 11.1 µin/in-°F | ISO 11359-1,-2 |
Lanxess Durethan® BKV 230 H3.0 000000 Nylon 6-Copolymer, 30% Glass Fibers PA 6-Copolymer, 30% glass fibers, injection molding, impact modified, heat-ageing stabilized |
|||
CTE, linear, Parallel to Flow | 20.0 µm/m-°C | 11.1 µin/in-°F | ISO 11359-1/-2 |
Lanxess Pocan® B 4235 Z 000000 PBT, 30% Glass Fiber PBT, 30% glass fibers, injection molding, flame retardant, impact modified |
|||
CTE, linear, Parallel to Flow | 20.0 µm/m-°C @Temperature 23.0 - 55.0 °C |
11.1 µin/in-°F @Temperature 73.4 - 131 °F |
ISO 11359-1, -2 |
Lanxess Durethan® BKV 30 H2.0 EF 000000 Nylon 6, Glass Fiber Reinforced PA 6, 30% glass fibers, injection molding, improved flowability, heat-aging stabilizedInformation provided by LANXESS. |
|||
CTE, linear, Parallel to Flow | 20.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
11.1 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP LUBRICOMP Lexan_LF0335 PC (Europe-Africa-Middle East) LNP* Lubricomp* LEXAN_LF0335 compound is a 35% glass fiber, milled glass reinforced PC injection moulding resin with improved wear resistance and reduced friction. |
|||
CTE, linear, Parallel to Flow | 20.0 µm/m-°C @Temperature 23.0 - 85.0 °C |
11.1 µin/in-°F @Temperature 73.4 - 185 °F |
ISO 11359 |
Solvay TECHNYL® C 216 V45 PA6, 45% glass fiber, DRY Description: Polyamide PA6, reinforced with 45% of glass fiber, for injection molding.Available in: EuropeProduct Applications: TECHNYL C 216 V45 has been optimized to have high impact strength, a n.. |
|||
CTE, linear, Parallel to Flow | 20.0 µm/m-°C @Temperature 23.0 - 150 °C |
11.1 µin/in-°F @Temperature 73.4 - 302 °F |
ISO 11359-2 |
SABIC Innovative Plastics ULTEM 2300 PEI (Europe-Africa-Middle East) 30% Glass fiber filled, standard flow Polyetherimide (Tg 217C). Resin is RoHS compliant. UL94 V0 and 5VA listing. |
|||
CTE, linear, Parallel to Flow | 20.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
11.1 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics NORYL PPX PPX630 PPE+PP (Europe-Africa-Middle East) PPX630 is a 30% glass filled alloy of PP and PPO providing design freedom for applications requiring a wide range of stiffness, toughness and temperature. Generic identification acc. ISO11469: PP+PP.. |
|||
CTE, linear, Parallel to Flow | 20.0 - 30.0 µm/m-°C @Temperature 20.0 °C |
11.1 - 16.7 µin/in-°F @Temperature 68.0 °F |
TMA |
Vyncolit 3640 CG Novolac Phenolic Graphite filled phenolic molding compound with excellent dimensional stability. Self-lubricating and has a low coefficient of friction. Not suitable for electrical applications.USES: Gas meter par.. |
|||
CTE, linear, Parallel to Flow | 20.0 - 30.0 µm/m-°C @Temperature 20.0 °C |
11.1 - 16.7 µin/in-°F @Temperature 68.0 °F |
|
Vyncolit G885 Novolac Phenolic Glass fiber and mineral filled phenolic molding compound with excellent mechanical and thermal properties. Information provided by Vyncolit, a Sumitomo Bak Group |
|||
CTE, linear, Parallel to Flow | 20.0 - 30.0 µm/m-°C @Temperature 20.0 °C |
11.1 - 16.7 µin/in-°F @Temperature 68.0 °F |
TMA |
Vyncolit X681 Novolac Phenolic Glass fiber filled phenolic molding compound with excellent mechanical properties and a low coefficient of friction. Tribological compound with PTFE additive.USES: Water pump seals and self-lubrica.. |
|||
CTE, linear, Parallel to Flow | 20.0 µm/m-°C | 11.1 µin/in-°F | dry; ISO 11359-1/-2 |
DSM Akulon® K224-G6-FC BK00001 PA6-GF30 30% Glass Reinforced, Food Contact Grade |
|||
CTE, linear, Parallel to Flow | 20.0 µm/m-°C @Temperature 20.0 °C |
11.1 µin/in-°F @Temperature 68.0 °F |
ISO 11359-1/-2 |
DSM Akulon® K224-G6U (Dry) 33% Glass Reinforced Nylon 6 (North America) Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis.. |
|||
CTE, linear, Parallel to Flow | 20.0 µm/m-°C @Temperature 20.0 °C |
11.1 µin/in-°F @Temperature 68.0 °F |
ISO 11359-1/-2 |
DSM Akulon® S223-HPG5 Impact Modified Nylon 66-25% Glass Reinforced (European Grade) (Dry) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
CTE, linear, Parallel to Flow | 20.0 µm/m-°C | 11.1 µin/in-°F | ISO 11359-1/-2 |
EMS-Grivory Grivory® BG-30 S PA6-GF30 Product description: Grilon BG-30 S is a heat stabilized PA6 injection molding grade with 30% glass fibers. Grilon BG-30 S has the following important properties: Excellent surface finishEasy flowin.. |
|||
CTE, linear, Parallel to Flow | 20.0 µm/m-°C | 11.1 µin/in-°F | ISO 11359-1/-2 |
EMS-Grivory Grivory® BG-40 S PA6-GF40 Product description: Grilon BG-40 S is a normal viscosity PA 6 injection molding type with 40% glass fibers. Grilon BG-40 S has the following important properties: High stiffnessExcellent surface fi.. |
|||
CTE, linear, Parallel to Flow | 20.0 µm/m-°C @Temperature 20.0 °C |
11.1 µin/in-°F @Temperature 68.0 °F |
ISO 11359-1/-2 |
DSM Stanyl® TW271F6 Nylon 46-30% Glass Reinforced (European and Asian Grade) (Dry) Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper.. |
|||
CTE, linear, Parallel to Flow | 20.0 µm/m-°C | 11.1 µin/in-°F | ISO 11359-1/-2 |
EMS-Grivory Grivory® LV-30H FWA nat PA12-GF30 Product description: Grilamid LV-30H FWA natural is a 30 % glass fiber reinforced, heat stabilized polyamide 12 injection molding grade with the following special features: Stiffness combined with h.. |
|||
CTE, linear, Parallel to Flow | 20.0 µm/m-°C | 11.1 µin/in-°F | ISO 11359-1/-2 |
EMS-Grivory Grivory® TSG-30/4 PA666-GF30 Product description: Grilon TSG-30/4 is a heat stabilized, normal viscosity PA66 + PA6 injection molding grade with 30% glass fibers. Grilon TSG-30/4 has the following important properties: Good flo.. |
|||
CTE, linear, Parallel to Flow | 20.0 µm/m-°C | 11.1 µin/in-°F | ISO 11359-1/-2 |
EMS-Grivory Grivory® TSGZ-30 PA666-GF30 Product description: Grilon TSGZ-30 is a heat stabilized, normal viscosity, and impact modified PA66 + PA6 injection molding grade with 30% glass fibers. Grilon TSGZ-30 has the following important p.. |
|||
CTE, linear, Parallel to Flow | 20.0 µm/m-°C | 11.1 µin/in-°F | ISO 11359-1/-2 |
EMS-Grivory Grivory® XE 4105 black 9992 PA610-GF50 Product description: Grilamid XE 4105 black 9992 is a 50% glass fiber reinforced, heat stabilized and UV resistant polyamide 610 (PA610) injection molding grade. This product is to a large extent ba.. |
|||
CTE, linear, Parallel to Flow | 20.0 µm/m-°C | 11.1 µin/in-°F | ISO 11359-1/-2 |
EMS-Grivory Grivory® XE 4174 black 9992 PA1010-GF30 Product description: Grilamid XE 4174 black 9992 is a 30% glass fiber reinforced, heat stabilized polyamide 1010 injection molding grade. The main features of Grilamid XE 4174 black 9992 are: PA1010.. |
|||
CTE, linear, Parallel to Flow | 20.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
11.1 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
Eurostar Staramide ACF3 PA66, 15% Carbon Fiber Reinforced, Heat stabilized, Injection Molding Staramide ACF3 is a 15% Carbon Fiber Reinforced Polyamide 66, Injection Molding ResinInformation provided by Eurostar. |
|||
CTE, linear, Parallel to Flow | 20.0 µm/m-°C | 11.1 µin/in-°F | ISO 11359-1/-2 |
EMS-Grivory Grivory® HT XE 4027 nat PA*-GF30 Product description: Grivory XE 4027 natural is a 30% glass-fiber reinforced flame retardant (UL 94 V-0) engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamid.. |
|||
CTE, linear, Parallel to Flow | 20.0 µm/m-°C | 11.1 µin/in-°F | ISO 11359-1/-2 |
EMS-Grivory Grivory® TRV-4X9 PAMACM12-GF40 Product description: Grilamid TRV-4X9 is an amorphous, cycloaliphatic polyamide with 40% glass fibre reinforcement. Grilamid TRV-4X9 characterises itself through the following features: Very low shr.. |
|||
CTE, linear, Parallel to Flow | 20.0 - 25.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
11.1 - 13.9 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-1/-2 |
BASF Ultramid® B3ZG6 30% Glass Filled PA6 (Dry) Ultramid B3ZG6 is an impact-modified, 30% glass fiber reinforced injection molding PA6 grade for industrial items having very high impact strength and rigidity. |
|||
CTE, linear, Parallel to Flow | 20.0 µm/m-°C @Temperature 20.0 °C |
11.1 µin/in-°F @Temperature 68.0 °F |
ISO 11359-1/-2 |
DSM Arnite® TV4 460 KL PBT/PET Blend-30% Glass Reinforced (European Grade) Arnite resins are engineered to provide specific performance in applications where DSM technology can offer value.Arnite Molding resins: Standard Unfilled and Reinforced materialsHigh modulus Flame .. |