Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 40.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
22.2 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics Lexan® 500RS PC (Europe-Africa-Middle East) LEXAN 500RS is a medium viscosity, glass reinforced, flame retardant grade. |
|||
CTE, linear, Parallel to Flow | 40.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
22.2 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP FARADEX ES003E PEI LNP* FARADEX* ES003E is a Polyetherimide resin containing 15% Stainless Steel Fibers. Added feature of this grade is: EMI/RFI Shielding. |
|||
CTE, linear, Parallel to Flow | 40.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
22.2 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics Lexan® HF500R PC (Europe-Africa-Middle East) LEXAN HF500R is an easy flow, 9% glass reinforced, flame retardant grade, especially designed for applications requiring high rigidity together with high heat resistance and impact performance. |
|||
CTE, linear, Parallel to Flow | 40.0 - 50.0 µm/m-°C @Temperature 50.0 - 100 °C |
22.2 - 27.8 µin/in-°F @Temperature 122 - 212 °F |
ISO 11359-2 |
Raschig Group RALUPOL® 8601 UP Glass-fiber reinforced polyester molding compound. Mold shrinkage similar to phenolic moulding compounds, low post-shrinkage, good electrical values, excellent heat resistance, good mechanical stren.. |
|||
CTE, linear, Parallel to Flow | 40.0 µm/m-°C | 22.2 µin/in-°F | ASTM D696 |
LG Chemical LUMID LW4403A(W) PA66+GF/MF40%, Low Warpage Feature: Injection Molding, PA66+GF/MF40%, Low WarpageApplication: Automotive (Timing Belt Cover)CAS No. 25038-54-4, 13983-17-0 and 65997-17-3Information provided by LG Chemical |
|||
CTE, linear, Parallel to Flow | 40.0 µm/m-°C @Temperature 20.0 °C |
22.2 µin/in-°F @Temperature 68.0 °F |
ISO 11359-1/-2 |
Mitsubishi Xantar® MX 1081 Polycarbonate-10% Glass Reinforced Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
CTE, linear, Parallel to Flow | 40.0 µm/m-°C @Temperature 23.0 - 55.0 °C |
22.2 µin/in-°F @Temperature 73.4 - 131 °F |
ISO 11359-1, -2 |
Lanxess Durethan® BKV 215 000000 Nylon 6-Copolymer, Glass Fiber Reinforced, Impact Modified PA 6-Copolymer, 15% glass fibers, injection molding impact modifiedInformation provided by LANXESS. |
|||
CTE, linear, Parallel to Flow | 40.0 µm/m-°C | 22.2 µin/in-°F | ISO 11359-1/-2 |
Lanxess Durethan® BKV 215 901510 Copolyamide, 15% Glass Fiber CoPA, injection molding grade, 15% glass fibers, elastomer-modified, higher impact and notched impact strength and also higher energy absorption under biaxial impact load than BKV 115, conditioning .. |
|||
CTE, linear, Parallel to Flow | 40.0 µm/m-°C | 22.2 µin/in-°F | ISO 11359-1/-2 |
Lanxess Durethan® BKV 215 H2.0 901510 Copolyamide, 15% Glass Fiber CoPA, injection molding grade, 15% glass fibers, elastomer-modified, higher impact and notched impact strength and also higher energy absorption under biaxial impact load than BKV 115, conditioning .. |
|||
CTE, linear, Parallel to Flow | 40.0 µm/m-°C @Temperature 23.0 - 55.0 °C |
22.2 µin/in-°F @Temperature 73.4 - 131 °F |
ISO 11359-1, -2 |
Lanxess Durethan® DP 2-2240/15 H2.0 901510 Nylon 66, 15% Glass Fiber PA 66, 15% glass fibers, blow molding, heat-aging stabilized, hydrolysis stabilizedInformation provided by LANXESS. |
|||
CTE, linear, Parallel to Flow | 40.0 µm/m-°C | 22.2 µin/in-°F | ISO 11359-1/-2 |
Lanxess Pocan® B 7616 000000 PBT + PC, 15% Glass Fiber PBT+PC, 15% glass fibers, injection molding, low tendency to warp, improved surface finish |
|||
CTE, linear, Parallel to Flow | 40.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
22.2 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP LUBRICOMP RFN14 PA 66 LNP* LUBRICOMP* RFN14 is a compound based on Nylon 66 containing 20% Glass Fiber, 5% MOS2. Added features of this grade include: Wear Resistant. |
|||
CTE, linear, Parallel to Flow | 40.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
22.2 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics Xenoy® 1760T PBT+PC (Europe-Africa-Middle East) XENOY 1760T is developed as a easy flow material, for applications such as doorhandles and mirror housings. It is a 11% glass reinforced material with excellent strength and dimensional stability.Th.. |
|||
CTE, linear, Parallel to Flow | 40.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
22.2 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP THERMOCOMP RFB53XXZ PA 66 LNP* THERMOCOMP* RFB53XXZ is a compound based on Nylon 66 resin containing 15% Glass Fiber, 25% Glass Bead. |
|||
CTE, linear, Parallel to Flow | 40.0 µm/m-°C | 22.2 µin/in-°F | ASTM E831 |
Sumitomo Bakelite North America E 16521A Electrical Encapsulation Grade Epoxy E-16521A is an encapsulation grade epoxy molding compound suitable for electrical applications such as coils.Information provided by Sumitomo Bak North America, Inc. |
|||
CTE, linear, Parallel to Flow | 40.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
22.2 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP Thermocomp ZM3242 PPE+PS (Asia Pacific) Modified PPO* 30% mineral filled products, Non Halogenated Flame Retardant V-1 products.Supper low warpage series, HDT 110degCThis data was supplied by SABIC-IP for the Asia Pacific region. |
|||
CTE, linear, Parallel to Flow | 40.0 µm/m-°C | 22.2 µin/in-°F | ISO 11359-1/-2 |
Covestro Bayblend® T90 MF-20* Polycarbonate + ABS, Mineral Filled Developmental productInjection molding grade20 % mineral filledvery good flowreduced coefficient of thermal dilatationtensile modulus = 5200 MPaVicat/B 120 = 130 °CPreprocessingMax. Water content |
|||
CTE, linear, Parallel to Flow | 40.0 µm/m-°C @Temperature 20.0 °C |
22.2 µin/in-°F @Temperature 68.0 °F |
ISO 11359-1/-2 |
DSM Arnite® TV4 230 SF PBT-15% Glass Reinforced (European and Asian Grade) Arnite resins are engineered to provide specific performance in applications where DSM technology can offer value.Arnite Molding resins: Standard Unfilled and Reinforced materialsHigh modulus Flame .. |
|||
CTE, linear, Parallel to Flow | 40.0 µm/m-°C | 22.2 µin/in-°F | ISO 11359-1/-2 |
DSM Arnite® TZ4 254 S PBT-(GF+MD)25 FR(17) Glass/Mineral Reinforced, Flame Retardant |
|||
CTE, linear, Parallel to Flow | 40.0 µm/m-°C @Temperature 20.0 °C |
22.2 µin/in-°F @Temperature 68.0 °F |
|
Covestro Makrolon® 8025 Polycarbonate High viscosity extrusion and injection molding grade with 20% short glass fibers and easy mold release, low anisotropy, for stiff moldings requiring good dimensional stability.Information provided b.. |
|||
CTE, linear, Parallel to Flow | 40.0 µm/m-°C | 22.2 µin/in-°F | dry; ISO 11359-1/-2 |
DSM EcoPaXX® Q-X07209 PA410-I-GF40 % Glass Reinforced, Impact Modified |
|||
CTE, linear, Parallel to Flow | 40.0 µm/m-°C | 22.2 µin/in-°F | ISO 11359-1/-2 |
EMS-Grivory Grivory® AG-25 HM PA66-GF25 Product description: Grilon AG-25 HM is a heat stabilized, normal viscosity, and adhesion modified PA66 injection molding grade with 25% glass fibers. Grilon AG-25 HM has the following important pro.. |
|||
CTE, linear, Parallel to Flow | 40.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
22.2 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
Eurostar Starflam AFR560B1 PA66, Mineral/Glass Fiber Reinforced, Flame Retardant, Injection Molding Starflam AFR560B1 is a Flame Retardant, Mineral Filled and Glass Fiber Reinforced Polyamide 66, Injection Molding ResinInformation provided by Eurostar. |
|||
CTE, linear, Parallel to Flow | 40.0 µm/m-°C @Temperature 20.0 °C |
22.2 µin/in-°F @Temperature 68.0 °F |
ISO 11359-1/-2 |
DSM Akulon® S223-HM8 Nylon 66-40% Mineral Reinforced (European and Asian Grade) (Dry) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
CTE, linear, Parallel to Flow | 40.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
22.2 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
Eurostar Staramide BG4ST43 PA6, Glass Fiber Filled, Impact Modified, Injection Molded Staramide BG4ST43 is an Impact Modified and Glass Fiber Reinforced, Polyamide 6, Injection Molding ResinInformation provided by Eurostar. |
|||
CTE, linear, Parallel to Flow | 40.0 µm/m-°C @Temperature 20.0 °C |
22.2 µin/in-°F @Temperature 68.0 °F |
|
Arkema Group Rilsan® ASR 30 Nylon 12, 30% Carbon Fiber Filled (Conditioned) Designation ISO 1874-PA12,M,16-120,CF30Rigid grade with carbon fiber filler (30%) for injection molding. Available color: black.Very high rigidity. High strength-to-weight ratio. Very low shrinkage:.. |
|||
CTE, linear, Parallel to Flow | 40.0 µm/m-°C | 22.2 µin/in-°F | ISO 11359-1/-2 |
DSM Arnite® TV4 241 SL PBT-GF20 FR(17) 20% Glass Reinforced, Flame Retardant, UV Stabilized |
|||
CTE, linear, Parallel to Flow | 40.0 µm/m-°C | 22.2 µin/in-°F | ISO 11359-1/-2 |
DSM Arnite® TV6 241 SN PBT-GF20 FR(17) 20% Glass Reinforced, Flame Retardant |
|||
CTE, linear, Parallel to Flow | 40.0 µm/m-°C | 22.2 µin/in-°F | ISO 11359-1/-2 |
DSM Arnite® TZ6 280 PBT-(GF+GB)40 20% Glass Reinforced, 20% Glass Beads Reinforced |