Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 26.0 µm/m-°C @Temperature 23.0 - 55.0 °C |
14.4 µin/in-°F @Temperature 73.4 - 131 °F |
ASTM E831 |
Lavergne VYPET VNT 840 PET 40% Glass-Mineral Reinforced Vypet VNT 840 is a 40% glass/mineral reinforced PET injection molding compound designed for electrical and structural applications, with High Dielectric Strength Features: High temperature performan.. |
|||
CTE, linear, Parallel to Flow | 26.0 µm/m-°C @Temperature 23.0 - 85.0 °C |
14.4 µin/in-°F @Temperature 73.4 - 185 °F |
ISO 11359 |
Solvay TECHNYL® B 218L V30 Black 44 N PA66, 30% glass fiber, DRY Description: Copolyamide 66/6, reinforced with 30% of glass fiber, for injection molding, heat stabilized with improved UV ageing resistance.Available in: Asia Pacific, Europe and Latin AmericaProdu.. |
|||
CTE, linear, Parallel to Flow | 26.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
14.4 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP LUBRICOMP RFG16 PA 66 (Europe-Africa-Middle East) LNP* LUBRICOMP* RFG16 is a compound based on PA 66 resin containing Glass Fiber, Graphite. Added features include: Internally Lubricated. |
|||
CTE, linear, Parallel to Flow | 26.0 µm/m-°C @Temperature 23.0 - 150 °C |
14.4 µin/in-°F @Temperature 73.4 - 302 °F |
ISO 11359-2 |
SABIC Innovative Plastics ULTEM 2100 PEI (Europe-Africa-Middle East) 10% Glass fiber filled, standard flow Polyetherimide (Tg 217C). Resin is RoHS compliant. UL94 V0 and 5VA listing. |
|||
CTE, linear, Parallel to Flow | 26.0 µm/m-°C @Temperature 23.0 - 150 °C |
14.4 µin/in-°F @Temperature 73.4 - 302 °F |
ISO 11359-2 |
SABIC Innovative Plastics ULTEM 2100R PEI (Europe-Africa-Middle East) 10% Glass fiber filled, standard flow Polyetherimide (Tg 217C) with internal mold release. Resin is RoHS compliant. UL94 V0 and 5VA listing. |
|||
CTE, linear, Parallel to Flow | 26.0 µm/m-°C @Temperature 23.0 - 150 °C |
14.4 µin/in-°F @Temperature 73.4 - 302 °F |
ISO 11359-2 |
SABIC Innovative Plastics ULTEM 2110 PEI (Europe-Africa-Middle East) 10% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). Resin is RoHS compliant. UL94 V0 and 5VA listing. |
|||
CTE, linear, Parallel to Flow | 26.0 µm/m-°C @Temperature 23.0 - 150 °C |
14.4 µin/in-°F @Temperature 73.4 - 302 °F |
ISO 11359-2 |
SABIC Innovative Plastics Ultem 2110F PEI (Europe-Africa-Middle East) 10% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). US FDA and European Food Contact approved. Effective June, 2007 this grade will no longer be supported with biocompatibility informati.. |
|||
CTE, linear, Parallel to Flow | 26.0 µm/m-°C @Temperature 23.0 - 150 °C |
14.4 µin/in-°F @Temperature 73.4 - 302 °F |
ISO 11359-2 |
SABIC Innovative Plastics ULTEM 2110R PEI (Europe-Africa-Middle East) 10% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C) with internal mold release. Resin is RoHS compliant. UL94 V0 and 5VA listing. |
|||
CTE, linear, Parallel to Flow | 26.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
14.4 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP LUBRICOMP WFL36 PBT (Europe-Africa-Middle East) LNP* Lubricomp* WFL36 is a compound based on Polybutylene Terephalate resin containing Glass Fiber, PTFE. |
|||
CTE, linear, Parallel to Flow | 26.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
14.4 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP STAT-KON DE002 PC (Asia Pacific) LNP* Stat-Kon* DE002 is a Polycarbonate containing Carbon Fiber. |
|||
CTE, linear, Parallel to Flow | 26.0 µm/m-°C @Temperature 23.0 - 150 °C |
14.4 µin/in-°F @Temperature 73.4 - 302 °F |
ISO 11359-2 |
SABIC Innovative Plastics ULTEM PW2100 PEI (Europe-Africa-Middle East) 10% Glass fiber filled, standard flow Polyetherimide (Tg 217°C). Specific grade-colors are designed and certified for use in Potable Water applications. KTW, WRAS, ACS, NSF-61 and W270 certified... |
|||
CTE, linear, Parallel to Flow | 26.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
14.4 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP THERMOCOMP JX97000 PES (Europe-Africa-Middle East) LNP* Thermocomp* JX97000 is a compound based on Polyethersulfone resin containing Glass Fiber. Added features of this material include: Mold Release. |
|||
CTE, linear, Parallel to Flow | 26.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
14.4 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP THERMOCOMP OF008A PPS (Asia Pacific) LNP* Thermocomp* OF008A is a compound based on PPS - Branched resin containing Glass Fiber.This product is also known as Thermocomp* OF-1008. |
|||
CTE, linear, Parallel to Flow | 26.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
14.4 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP THERMOCOMP OF008E PPS (Asia Pacific) LNP* Thermocomp* OF008E is a compound based on Polyphenylene Sulfide resin containing Glass Fiber. Added features of this material include: Easy Molding. |
|||
CTE, linear, Parallel to Flow | 26.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
14.4 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP THERMOCOMP RF007ES PA 66 LNP* THERMOCOMP* RF007ES is a compound based on Nylon 66 resin containing 35% Glass Fiber. Added features of this material include: Heat Stabilized, Easy Molding. |
|||
CTE, linear, Parallel to Flow | 26.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
14.4 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP THERMOCOMP RF009S PA 66 LNP* THERMOCOMP* RF009S is a compound based on Nylon 66 resin containing 45% Glass Fiber. Added features of this material include: Heat Stabilized. |
|||
CTE, linear, Parallel to Flow | 26.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
14.4 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP Thermocomp RF00ASXP PA6.6 (Europe-Africa-Middle East) LNP* THERMOCOMP* RF00ASXP is a compound based on PA 66 resin containing Glass Fiber. Added features include: Heat Stabilized.This data was supplied by SABIC-IP for the Europe-Africa-Middle East regi.. |
|||
CTE, linear, Parallel to Flow | 26.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
14.4 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP THERMOCOMP RF00ASXS PA6.6 (Europe-Africa-Middle East) LNP* Thermocomp* RF00ASXS is a compound based on PA 66 resin containing Glass Fiber. Added features include: Heat Stabilized. |
|||
CTE, linear, Parallel to Flow | 26.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
14.4 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP THERMOCOMP OF008A PPS - Branched LNP* THERMOCOMP* OF008A is a compound based on PPS - Branched resin containing 40% Glass Fiber. |
|||
CTE, linear, Parallel to Flow | 26.0 - 28.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
14.4 - 15.6 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP Verton RV008ESV PA 66 40% long glass fiber filled PA66 Verton Xtreme XCThis data was supplied by SABIC-IP for the Americas region. |
|||
CTE, linear, Parallel to Flow | 26.0 µm/m-°C | 14.4 µin/in-°F | DAM; ISO 11359-1/-2 |
DuPont Performance Polymers Zytel® 73G30HSL BK416 Nylon 6
(Unverified Data**) 30% Glass Reinforced Heat Stabilized Polyamide 6 Zytel 73G30HSL BK416 is a 30% glass fiber reinforced heat stabilized lubricated black polyamide 6 resin for injection molding.Information provided by.. |
|||
CTE, linear, Parallel to Flow | 26.0 µm/m-°C @Temperature -40.0 - 23.0 °C |
14.4 µin/in-°F @Temperature -40.0 - 73.4 °F |
DAM; ISO 11359-1/-2 |
DuPont Performance Polymers Zytel® FG77G33L NC010 Nylon 612 33% Glass Reinforced Polyamide 612 with Developed for Food Contact ApplicationsInformation provided by DuPont Performance Polymers |
|||
CTE, linear, Parallel to Flow | 26.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
14.4 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
Eurostar Staramide RF00ASXP PA66, 50% Glass Filled, Injection Molded Staramide RF00ASXP is a 50% Glass Fiber Reinforced Polyamide 66 Injection Molding Resin (also known as Staramide 66 G 50V S3)Information provided by Eurostar. |
|||
CTE, linear, Parallel to Flow | 26.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
14.4 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP LUBRICOMP DFL44 PC (Europe-Africa-Middle East) LNP* Lubricomp* DFL44 is a compound based on Polycarbonate resin containing Glass Fiber, PTFE. |
|||
CTE, linear, Parallel to Flow | 26.0 µm/m-°C @Temperature 20.0 °C |
14.4 µin/in-°F @Temperature 68.0 °F |
ASTM E831 |
Sumitomo Bakelite North America FM 3000 Cellulose Reinforced Phenolic Novolac FM 3000 is a self-lubricated cellulose reinforced phenolic molding compound, modified for applications requiring reduced friction and low wear. Information supplied by Sumitomo Bak North America... |
|||
CTE, linear, Parallel to Flow | 26.0 µm/m-°C @Temperature 20.0 °C |
14.4 µin/in-°F @Temperature 68.0 °F |
ASTM E-831 |
Sumitomo Bakelite North America TEM 9053C Hardware Grade Epoxy Short fiberglass and mineral filled, toughened epoxy molding compound with excellent dimensional stability and high strength properties.Information provided by Vyncolit, a Sumitomo Bak Group |