Polymer Property : CTE, linear, Parallel to Flow = 3.33 µin/in-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 6.00 µm/m-°C

@Temperature -50.0 - 50.0 °C
3.33 µin/in-°F

@Temperature -58.0 - 122 °F
TMA; ASTM E831
Solvay Specialty Polymers AvaSpire® AV-722 CF30 Polyaryletherketone (PAEK)  (Unverified Data**)
AvaSpire AV-722 CF30 is a 30% carbon fiber reinforced version of AvaSpire AV-722. This formulation offers improved part economics relative to 30% carbon fiber reinforced PEEK while retaining most of..
CTE, linear, Parallel to Flow 6.00 µm/m-°C
3.33 µin/in-°F
Above Tg; ISO 11359
Victrex® PEEK 150CA30 30% Carbon Fiber Reinforced
Product Description: High performance thermoplastic material, 30% carbon fiber reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding, easy flow, FDA food contact c..
CTE, linear, Parallel to Flow 6.00 µm/m-°C

@Temperature -50.0 - 50.0 °C
3.33 µin/in-°F

@Temperature -58.0 - 122 °F
1
Solvay Specialty Polymers AvaSpire® AV-722 CF30 Polyaryletherketone (PAEK), 30% Carbon Fiber
AvaSpire® AV-722 CF30 is a 30% carbon fiber reinforced version of AvaSpire® AV-722. This formulation offers improved part economics relative to 30% carbon fiber reinforced PEEK while retaining..
CTE, linear, Parallel to Flow 6.00 µm/m-°C

@Temperature -30.0 - 30.0 °C
3.33 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D 696
SABIC Innovative Plastics LNP Stat-kon EE008E PEI
LNP STAT-KON* EE008E is a compound based on Polyetherimide resin containing Carbon Fiber. Added features of this material include: Easy Molding.This data was supplied by SABIC-IP for the Americas r..
CTE, linear, Parallel to Flow 6.00 µm/m-°C

@Temperature -30.0 - 30.0 °C
3.33 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP STAT-KON DEL359EF PC
LNP* STAT-KON* DEL359EF is a compound based on Polycarbonate containing 25% Carbon Fiber, 15% PTFE. Added features include: Flame Retardant. Electrically Conductive, Wear Resistant.
CTE, linear, Parallel to Flow 6.00 µm/m-°C

@Temperature 23.0 - 60.0 °C
3.33 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
SABIC Innovative Plastics LNP THERMOCOMP OC006 PPS - Linear (Europe-Africa-Middle East)
LNP* THERMOCOMP* OC006 is a compound based on PPS - Linear resin containing Carbon Fiber. Added features include : Electrically Conductive.
CTE, linear, Parallel to Flow 6.00 µm/m-°C

@Temperature 23.0 - 85.0 °C
3.33 µin/in-°F

@Temperature 73.4 - 185 °F
ISO 11359
Solvay TECHNYL® A 216 S30 PA66, 30% glass spheres, DRY
Description: Polyamide 66, reinforced with 30% of glass spheres, for injection molding.Available in: EuropeProduct Applications: TECHNYL® A 216 S30 is used in all sectors of industry, offering an..
CTE, linear, Parallel to Flow 6.00 µm/m-°C

@Temperature 23.0 - 85.0 °C
3.33 µin/in-°F

@Temperature 73.4 - 185 °F
ISO 11359
Solvay TECHNYL® A 216 S40 PA66, 40% glass spheres, DRY
Description: Polyamide 66, reinforced with 40% of glass spheres, for injection molding.Available in: EuropeProduct Applications: TECHNYL ® A 216 S40 is used in all sectors of industry, offering a..
CTE, linear, Parallel to Flow 6.00 µm/m-°C

@Temperature 55.0 - 160 °C
3.33 µin/in-°F

@Temperature 131 - 320 °F
ISO 11359-1/-2
DuPont Performance Polymers Rynite® 940 BK505 Polyethylene Terephthalate (PET)  (Unverified Data**)
40% Glass/Mineral Reinforced Polyethylene Terephthalate Rynite 940 BK505 is a 40% mica/glass reinforced modified polyethylene terephthalate with greater strength stiffness and low warpage.Informatio..