Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 72.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
40.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Cycoloy® C1000HF PC+ABS High flow PC+ABS. |
|||
CTE, linear, Parallel to Flow | 72.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
40.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Cycoloy® C1200 PC+ABS (Asia Pacific) PC+ABS, excellent impact/high heat resistance. Low temperature ductility. For automotive, appliance and electrical components. |
|||
CTE, linear, Parallel to Flow | 72.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
40.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Cycoloy® C1950 PC+ABS Low viscosity injection molding resin.This data was supplied by SABIC-IP for the Americas region. |
|||
CTE, linear, Parallel to Flow | 72.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
40.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Cycoloy® C2951 PC+ABS (Asia Pacific) CYCOLOY C2951 is a flame retardant PC+ABS free from chlorinated or brominated flame retardant additives. High heat resistance is offered for demanding electrical applications, whilst maintaining exc.. |
|||
CTE, linear, Parallel to Flow | 72.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
40.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Cycoloy® FXC630SK PC+ABS Color package may affect performance. PC+ABS, ECO-conforming flame retardant with diamond sparkle appearance. |
|||
CTE, linear, Parallel to Flow | 72.0 µm/m-°C @Temperature -20.0 - 150 °C |
40.0 µin/in-°F @Temperature -4.00 - 302 °F |
ASTM E 831 |
SABIC Innovative Plastics Cycoloy® LG9000 PC+ABS (Asia Pacific) PC+ABS blend, low gloss and UV-stable, suitable for automotive interior applications. |
|||
CTE, linear, Parallel to Flow | 72.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
40.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Cycoloy® MC1300 PC+ABS (Asia Pacific) Cycoloy MC1300 resin is an injection moldable PC/ABS blend featuring excellent flow and impact performance. It is designed for plating applications mostly used in automotive industry. |
|||
CTE, linear, Parallel to Flow | 72.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
40.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Cycoloy® MC8002 PC+ABS AUTOMOTIVE. Low viscosity, high impact and ductility. |
|||
CTE, linear, Parallel to Flow | 72.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
40.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Cycoloy® MC8002 PC+ABS (Asia Pacific) AUTOMOTIVE. Low viscosity, high impact and ductility. |
|||
CTE, linear, Parallel to Flow | 72.0 µm/m-°C @Temperature -20.0 - 150 °C |
40.0 µin/in-°F @Temperature -4.00 - 302 °F |
ASTM E 831 |
SABIC Innovative Plastics GELOY XP4034 ASA+PC Available in a wide range of colors. Recommended for unpainted exterior/high heat/high impact applications. |
|||
CTE, linear, Parallel to Flow | 72.0 µm/m-°C @Temperature -20.0 - 150 °C |
40.0 µin/in-°F @Temperature -4.00 - 302 °F |
ASTM E 831 |
SABIC Innovative Plastics GELOY XP4034 ASA+PC (Asia Pacific) Weatherable, injection moldable ASA+PC blend. In a wide range of colors. Recommended for unpainted exterior/high heat applications. |
|||
CTE, linear, Parallel to Flow | 72.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
40.0 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics Lexan® ML7689 PC Copolymer (Europe-Africa-Middle East) Lexan* ML7689 polycarbonate (PC) siloxane copolymer resin IS a high viscosity injection molding (IM) grade WITH good processability, offering opportunities FOR shorter IM CYCLE times compared TO sta.. |
|||
CTE, linear, Parallel to Flow | 72.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
40.0 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics Cycoloy® C1110HF PC+ABS High impact and ductility at 73F and -20F. For thin-wall applications. |
|||
CTE, linear, Parallel to Flow | 72.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
40.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Cycoloy® FXC1200E PC+ABS (Asia Pacific) Visual Fx PC/ABS for strong fluorescent bright colors with good flow, impact and heat resistance characteristics. Consumer electronic and appliance applications uses. |
|||
CTE, linear, Parallel to Flow | 72.0 µm/m-°C @Temperature 20.0 °C |
40.0 µin/in-°F @Temperature 68.0 °F |
|
Ineos ABS Centrex® 601 ASA+AES Blend
(discontinued **) Key Features:UnfilledHigh impact or high impact modifiedLight stabilized or stable to lightU.V. stabilized or stable to weatherSuitable processing methods:Profile extrusionSheet extrusionInformation.. |
|||
CTE, linear, Parallel to Flow | 72.0 µm/m-°C | 40.0 µin/in-°F | ASTM D696 |
Techmer ES Electrablend® PC C BK Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/Reinfor.Features: ConductiveAppearance: BlackInformation provided by TP Composites, Inc. |
|||
CTE, linear, Parallel to Flow | 72.0 µm/m-°C | 40.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill FR® PBT FR X Availability: North AmericaForms: PelletsAdditive: Mold ReleaseFeatures: Flame RetardantProcessing Method: Injection MoldingInformation provided by TP Composites, Inc. |
|||
CTE, linear, Parallel to Flow | 72.0 µm/m-°C | 40.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill® HDPE GF10 CC 10% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 10% Filler by WeightFeatures: Chemically CoupledInformation provided by TP Composites, Inc. |
|||
CTE, linear, Parallel to Flow | 72.0 µm/m-°C | 40.0 µin/in-°F | ASTM D696 |
Techmer ES Plastiblend® PC/ABS 1950 Availability: North AmericaForms: PelletsInformation provided by TP Composites, Inc. |
|||
CTE, linear, Parallel to Flow | 72.0 µm/m-°C | 40.0 µin/in-°F | ASTM D696 |
Techmer ES Plastiblend® PC/ABS 8800 Availability: North AmericaForms: PelletsFeatures: High Impact Resistance and High Temperature StrengthProcessing Method: Profile ExtrusionInformation provided by TP Composites, Inc. |
|||
CTE, linear, Parallel to Flow | 72.0 µm/m-°C | 40.0 µin/in-°F | ASTM D696 |
Techmer ES Plastiblend® PC/ABS FR 6209 Availability: North AmericaForms: PelletsFeatures: Flame RetardantInformation provided by TP Composites, Inc. |
|||
CTE, linear, Parallel to Flow | 72.0 µm/m-°C @Temperature 0.000 - 100 °C |
40.0 µin/in-°F @Temperature 32.0 - 212 °F |
ASTM E 831 |
SABIC Innovative Plastics NORYL PX1265 PPE+PS Automotive applications. Exterior mirror and cluster housings, speaker grilles, cowl tops, exterior trim. 270F (132C) DTUL. |
|||
CTE, linear, Parallel to Flow | 72.0 µm/m-°C | 40.0 µin/in-°F | ASTM D696 |
Techmer ES Electrablend® HDPE C BK Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/Reinfor.Features: ConductiveAppearance: BlackTPCI# 9411115Information provided by TP Composites, Inc. |
|||
CTE, linear, Parallel to Flow | 72.0 µm/m-°C | 40.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill FR® PA4/6 FR Availability: North AmericaForms: PelletsFeatures: Flame Retardant TPCI# 8277150Information provided by TP Composites, Inc. |
|||
CTE, linear, Parallel to Flow | 72.0 µm/m-°C @Temperature -29.0 - 100 °C |
40.0 µin/in-°F @Temperature -20.2 - 212 °F |
ASTM D696 |
Styron PULSEâ„¢ 2300 PT PC/ABS Engineering Resin Information provided by Styron |
|||
CTE, linear, Parallel to Flow | 72.0 µm/m-°C @Temperature 23.0 - 55.0 °C |
40.0 µin/in-°F @Temperature 73.4 - 131 °F |
ISO 11359-1,-2 |
Covestro Bayblend® FR3006 HF PC/ABS Blend Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Flame-retardant• Injec.. |
|||
CTE, linear, Parallel to Flow | 72.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
40.0 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP THERMOCOMP WF002I PBT LNP* THERMOTUF* WF006I is a compound based on PBT resin containing 10% Glass Fiber. Added feature of this grade is: High Impact. |
|||
CTE, linear, Parallel to Flow | 72.0 µm/m-°C | 40.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill FR® PBT FR Availability: North AmericaForms: PelletsFeatures: Flame RetardantProcessing Method: Injection MoldingInformation provided by TP Composites, Inc. |
|||
CTE, linear, Parallel to Flow | 72.0 µm/m-°C | 40.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill FR® PBT FR-C Availability: North AmericaForms: PelletsFeatures: Flame RetardantUL File Number: E157318Processing Method: Injection MoldingInformation provided by TP Composites, Inc. |
|||
CTE, linear, Parallel to Flow | 72.0 µm/m-°C | 40.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill® TPX-HTN-01043 A Availability: North AmericaForms: PelletsAdditive: Impact Modifier and LubricantFeatures: High Temperature Strength, Impact Modified and LubricatedUL File Number: E157318Information provided by TP C.. |