Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 56.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
31.1 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP COLORCOMP G1000 PSU LNP* COLORCOMP* G1000 is an unfilled Polysulfone resin. Added feature of this grade is: Transparent. |
|||
CTE, linear, Parallel to Flow | 56.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
31.1 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP LUBRICOMP DFI14 PC LNP* Lubricomp* DFI14 is a compound based on Polycarbonate resin containing 20% Glass Fiber and 2% Silicone. Added features include: Internally Lubricated. |
|||
CTE, linear, Parallel to Flow | 56.0 µm/m-°C | 31.1 µin/in-°F | ASTM D696 |
Solvay Specialty Polymers Udel® P-1700 Polysulfone (PSU)
(Unverified Data**) Udel P-1700 polysulfone (PSU) is a tough, rigid, high-strength thermoplastics suitable for continuous use up to 300°F (149°C). It is resistant to oxidation and hydrolysis and withstand prolonged e.. |
|||
CTE, linear, Parallel to Flow | 56.0 µm/m-°C | 31.1 µin/in-°F | ASTM D696 |
Solvay Specialty Polymers Udel® P-1700 LCD Polysulfone (PSU)
(Unverified Data**) Udel P-1700 LCD polysulfone is especially well suited for the fabrication of porous membranes for filtration applications. The membranes are usually in the form of hollow fibers, but tube, plate or .. |
|||
CTE, linear, Parallel to Flow | 56.0 µm/m-°C | 31.1 µin/in-°F | ASTM D696 |
Solvay Specialty Polymers Udel® P-1710 Polysulfone (PSU)
(Unverified Data**) Udel P-1710 polysulfone (PSU) is a tough, rigid, high-strength thermoplastic that is suitable for continuous use up to 300°F (149°C). The resin is resistant to oxidation and hydrolysis and withsta.. |
|||
CTE, linear, Parallel to Flow | 56.0 µm/m-°C | 31.1 µin/in-°F | ASTM D696 |
Solvay Specialty Polymers Udel® P-3500 LCD MB Polysulfone (PSU)
(Unverified Data**) Udel polysulfone is a tough, rigid, high-strength thermoplastic with outstanding hydrolytic resistance. Udel P-3500 LCD MB series polymers are particularly well suited for the fabrication of porous .. |
|||
CTE, linear, Parallel to Flow | 56.0 µm/m-°C | 31.1 µin/in-°F | ASTM D696 |
Solvay Specialty Polymers Udel® P-3700 HC Polysulfone (PSU)
(Unverified Data**) Udel P-3700 HC is a high-clarity grade of polysulfone (PSU) that is nearly water-white in color. This grade was designed to eliminate the yellow cast and provide design flexibility and improved aest.. |
|||
CTE, linear, Parallel to Flow | 56.0 µm/m-°C | 31.1 µin/in-°F | ASTM D696 |
Solvay Specialty Polymers Udel® P-3703 Polysulfone (PSU)
(Unverified Data**) Udel P-3703 is a high-flow grade of polysulfone intended for injection molding applications with thin walls or long flow lengths. This grade has higher flow than Udel P-1700 and a slightly greater t.. |
|||
CTE, linear, Parallel to Flow | 56.0 µm/m-°C | 31.1 µin/in-°F | ASTM D696 |
Solvay Specialty Polymers Udel® P-1800 Polysulfone (PSU)
(discontinued **) Udel P-1800 is a powdered grade of polysulfone with molecular weight similar to that of Udel P-1700 polysulfone. It is well suited for the fabrication of porous membranes that can be made into hollo.. |
|||
CTE, linear, Parallel to Flow | 56.0 µm/m-°C | 31.1 µin/in-°F | ASTM D696 |
Solvay Specialty Polymers Udel® P-1835 Polysulfone (PSU)
(discontinued **) Udel P-1835 polysulfone is a powdered grade well suited for the fabrication of porous membranes. The membranes can be made into hollow fibers, tubes, plates, or spiral wound elements. They are used .. |
|||
CTE, linear, Parallel to Flow | 56.0 µm/m-°C | 31.1 µin/in-°F | ASTM D696 |
Solvay Specialty Polymers Udel® M-2300 MR Polysulfone (PSU), Mold Release
(discontinued **) Udel M-2300 MR is an injection-moldable, low-color grade of polysulfone that is nearly water white in color. This material contains a mold release which aids part ejection when parts with low draft .. |
|||
CTE, linear, Parallel to Flow | 56.0 µm/m-°C | 31.1 µin/in-°F | ASTM D696 |
LG Chemical LUMID GP3200A(W) PA6+MF20%, General Purpose Feature: Injection Molding, PA6+MF23%, High ImpactPA6+MF15%, General PurposeApplication: E&E (Rice Cooer Housing)CAS No. 25038-54-4 and 9010-79-1Information provided by LG Chemical |
|||
CTE, linear, Parallel to Flow | 56.0 µm/m-°C | 31.1 µin/in-°F | ASTM D696 |
Kuraray Genestarâ„¢ N1006A-M41 Nylon Impact modified unreinforced injection grade. Main Features:High elongationHigh impact strengthExamples of applications are:Retainers for quick connectorFlexible band |
|||
CTE, linear, Parallel to Flow | 56.0 µm/m-°C @Thickness 3.18 mm |
31.1 µin/in-°F @Thickness 0.125 in |
|
Solvay Specialty Polymers Ajedium™ Films -- Radel® R-5100 NT15 Polyphenylsulfone (PPSU) Radel® polyphenylsulfone is an amorphous thermoplastic material that offers exceptional hydrolytic stability, and toughness superior to other commercially available, high-temperature films. PPSU .. |
|||
CTE, linear, Parallel to Flow | 56.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
31.1 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP LUBRILOY DF206XXH PC LNP* LUBRILOY* DF206XXH is a compound based on Polycarbonate containing 30% Glass Fiber, Proprietary Lubricant. Added features of this grade include: Wear Resistant, Healthcare. |
|||
CTE, linear, Parallel to Flow | 56.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
31.1 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP LUBRILOY RF203AXH PA 66 LNP* LUBRILOY* RF203AXH is a compound based on Nylon 66 resin containing 15% Glass Fiber, Proprietary Lubricant. Added features of this material include: Wear Resistant, Healthcare. |
|||
CTE, linear, Parallel to Flow | 56.0 µm/m-°C @Thickness 3.18 mm |
31.1 µin/in-°F @Thickness 0.125 in |
|
Solvay Specialty Polymers Radel® R-5000 Polyphenylsulfone (PPSU) Radel® R-5000 is a transparent polyphenylsulfone (PPSU) which offers exceptional hydrolytic stability, and toughness superior to other commercially-available, high-temperature engineering resins... |
|||
CTE, linear, Parallel to Flow | 56.0 µm/m-°C @Thickness 3.18 mm |
31.1 µin/in-°F @Thickness 0.125 in |
|
Solvay Specialty Polymers Radel® R-5500 Polyphenylsulfone (PPSU) Radel® R-5500 is a general purpose extrusion grade of polyphenylsulfone (PPSU), offering exceptional hydrolytic stability and better toughness than most commercially available high-temperature po.. |
|||
CTE, linear, Parallel to Flow | 56.0 µm/m-°C @Thickness 3.18 mm |
31.1 µin/in-°F @Thickness 0.125 in |
|
Solvay Specialty Polymers Radel® R-5600 Polyphenylsulfone (PPSU) Radel® R-5600 is a very high melt flow grade of Radel® polyphenylsulfone (PPSU). It is especially well-suited for parts requiring long flow length with thin walls. Radel® resins offer excep.. |
|||
CTE, linear, Parallel to Flow | 56.0 µm/m-°C @Thickness 3.18 mm |
31.1 µin/in-°F @Thickness 0.125 in |
|
Solvay Specialty Polymers Radel® R-5800 Polyphenylsulfone (PPSU) Radel® R-5800 is a high melt flow grade of Radel® polyphenylsulfone (PPSU). It is especially well-suited for parts requiring long flow length with thin walls. Radel® resins offer exceptiona.. |
|||
CTE, linear, Parallel to Flow | 56.0 µm/m-°C @Thickness 3.18 mm |
31.1 µin/in-°F @Thickness 0.125 in |
|
Solvay Specialty Polymers Radel® R-5900 Polyphenylsulfone (PPSU) Radel® R-5900 polyphenylsulfone (PPSU) offers medium melt viscosities for long flow lengths and greater injection molding ease. It also provides exceptional hydrolytic stability and toughness tha.. |
|||
CTE, linear, Parallel to Flow | 56.0 µm/m-°C | 31.1 µin/in-°F | |
Solvay Specialty Polymers Udel® P-1700 LCD Polysulfone (PSU) Udel® P-1700 LCD polysulfone is especially well suited for the fabrication of porous membranes for filtration applications. The membranes are usually in the form of hollow fibers, but tube, plate.. |
|||
CTE, linear, Parallel to Flow | 56.0 µm/m-°C | 31.1 µin/in-°F | |
Solvay Specialty Polymers Udel® P-1710 Polysulfone (PSU) Udel® P-1710 polysulfone (PSU) is a tough, rigid, high-strength thermoplastic that is suitable for continuous use up to 300°F (149°C). The resin is resistant to oxidation and hydrolysis and.. |
|||
CTE, linear, Parallel to Flow | 56.0 µm/m-°C | 31.1 µin/in-°F | |
Solvay Specialty Polymers Udel® P-3500 LCD MB Polysulfone (PSU) Udel® polysulfone is a tough, rigid, high-strength thermoplastic with outstanding hydrolytic resistance. Udel® P-3500 LCD MB series polymers are particularly well suited for the fabrication of.. |
|||
CTE, linear, Parallel to Flow | 56.0 µm/m-°C | 31.1 µin/in-°F | |
Solvay Specialty Polymers Udel® P-3700 HC Polysulfone (PSU) Udel® P-3700 HC is a high-clarity grade of polysulfone (PSU) that is nearly water-white in color. This grade was designed to eliminate the yellow cast and provide design flexibility and improved .. |
|||
CTE, linear, Parallel to Flow | 56.0 µm/m-°C | 31.1 µin/in-°F | |
Solvay Specialty Polymers Udel® P-3703 Polysulfone (PSU) Udel® P-3703 is a high-flow grade of polysulfone intended for injection molding applications with thin walls or long flow lengths. This grade has higher flow than Udel® P-1700 and a slightly g.. |
|||
CTE, linear, Parallel to Flow | 56.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
31.1 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP THERMOCOMP AF004XXY ABS LNP* Thermocomp* AF004XXY is a compound based on ABS containing 20% glass fiber. |
|||
CTE, linear, Parallel to Flow | 56.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
31.1 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP THERMOCOMP AX02749 ABS LNP* THERMOCOMP* AX02749 is a compound based on ABS containing proprietary fillers. |
|||
CTE, linear, Parallel to Flow | 56.0 µm/m-°C | 31.1 µin/in-°F | |
Solvay Specialty Polymers Udel® P-1700 Polysulfone (PSU) Udel® P-1700 polysulfone (PSU) is a tough, rigid, high-strength thermoplastics suitable for continuous use up to 300°F (149°C). It is resistant to oxidation and hydrolysis and withstand pro.. |
|||
CTE, linear, Parallel to Flow | 56.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
31.1 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics XYLEX EXXX0292 PC+POLYESTER (Europe-Africa-Middle East) XYLEX* EXXX0292 is a transparent copolyester/polycarbonate blend with high flow, V2 UL94 rating at 1.5mm and Tg of 108 C |