Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 70.0 µm/m-°C | 38.9 µin/in-°F | ASTM D696 |
PolyOne Geon™ Vinyl Rigid Extrusion 87556 Polyvinyl Chloride, Rigid (PVC, Rigid) The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne |
|||
CTE, linear, Parallel to Flow | 70.0 µm/m-°C @Temperature 20.0 °C |
38.9 µin/in-°F @Temperature 68.0 °F |
|
Polycasa Acryl® G 55 Acrylic, Injection Molding Grade Injection molding grade for very long flow paths, as well as thin-walled parts.Data was collected by ISO methods.Quinn Manufacturing Group rebranded its Plastics Division as Polycasa in 2013. |
|||
CTE, linear, Parallel to Flow | 70.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
38.9 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Cycoloy® XCY620S PC+ABS (Asia Pacific) PC+ ABS Automotive applications |
|||
CTE, linear, Parallel to Flow | 70.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
38.9 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics Lexan® 241R PC (Europe-Africa-Middle East) LEXAN 241R is a medium viscosity multi purpose grade and contains a release agent to ensure easy processing. This grade is UL94-V2 at 0.8 mm approved. |
|||
CTE, linear, Parallel to Flow | 70.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
38.9 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics Lexan® 923A PC (Europe-Africa-Middle East) LEXAN 923A is a medium viscosity flame retardant grade, UV-stabilized, especially suitable for electrical applications. |
|||
CTE, linear, Parallel to Flow | 70.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
38.9 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics Lexan® 945AU PC (Europe-Africa-Middle East) Lexan* 945AU Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has a V0 UL rating and is UV stabilized, providing additiona.. |
|||
CTE, linear, Parallel to Flow | 70.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
38.9 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics Lexan® FXD101R PC (Europe-Africa-Middle East) Transparent/translucent PC for light diffusion special effects. Thicker sections without sinks. Internal mold release. Pigment package may affect properties. Application testing always recommended.. |
|||
CTE, linear, Parallel to Flow | 70.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
38.9 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics Lexan® FXE141R PC (Europe-Africa-Middle East) LEXAN FXE141R is a medium viscosity multi purpose UV stabilized grade for visual effects in ""energy"". The material contains a release agent to ensure easy processing. |
|||
CTE, linear, Parallel to Flow | 70.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
38.9 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics Lexan® FXE163R PC (Europe-Africa-Middle East) LEXAN FXE163R is a transparent/translucent UV stabilized, medium viscosity grade for special effects with fluorescent appearance. Color package may affect performance. LEXAN FXE163R contains a relea.. |
|||
CTE, linear, Parallel to Flow | 70.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
38.9 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Lexan® IFX2420Z PC (Asia Pacific) Lexan* IFX2420Z is a medium viscosity, release containing, injection moldable polycarbonate grade suitable for use in industry protective eye-ware applications specifically for welding. This grades .. |
|||
CTE, linear, Parallel to Flow | 70.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
38.9 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Lexan® XHT1143 PC (Asia Pacific) XHT1143 is a high flow, UV stabilized, high heat polycarbonate copolymer. It is the lowest heat, UV stabilized product in the LEXAN* XHT portfolio. It is available in a range of opaque and limited .. |
|||
CTE, linear, Parallel to Flow | 70.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
38.9 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics Lexan® 925 PC (Europe-Africa-Middle East) Lexan* 925A Polycarbonate (PC) resin is a non-filled, injection moldable grade of non-chlorinated, non-brominated flame retardant systems that has an UL-94 V0 rating. Lexan 925A is available in tran.. |
|||
CTE, linear, Parallel to Flow | 70.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
38.9 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics Lexan® 925AU PC (Europe-Africa-Middle East) Lexan* 925AU Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating and is UV stabilized, providing addit.. |
|||
CTE, linear, Parallel to Flow | 70.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
38.9 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics Lexan® 945 PC (Europe-Africa-Middle East) Lexan* 945 Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating and is available in various opaque color.. |
|||
CTE, linear, Parallel to Flow | 70.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
38.9 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics Lexan® 950 PC (Europe-Africa-Middle East) LEXAN 950 is a high viscosity flame retardant grade, especially suitable for electrical applications. |
|||
CTE, linear, Parallel to Flow | 70.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
38.9 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics Lexan® FXE143R PC (Europe-Africa-Middle East) LEXAN FXE143R is a medium viscosity multi purpose UV stabilized grade for visual effects in "energy". The material contains a release agent to ensure easy processing.This data was supplied by SABIC-.. |
|||
CTE, linear, Parallel to Flow | 70.0 µm/m-°C @Temperature 20.0 °C |
38.9 µin/in-°F @Temperature 68.0 °F |
|
Polimeri Europa KOBLEND PCA 839F PC+ABS
(discontinued **) Symbol according to ISO 1043/1: PC+ABSUnfilled. Suitable for Injection Molding. Supplied as pellets.ISO data. Information provided by EnichemPolimeri Europa now has Enichem's plastics businesses... |
|||
CTE, linear, Parallel to Flow | 70.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
38.9 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics NORYL SE100 PPE+HIPS (Europe-Africa-Middle East) NORYL® SE100 is an unfilled, flame retardant material with a Vicat B/120 of 120°C. It has a UL-94 flammability rating V1 @ 1.47 mm, and is halogen free according to VDE/DIN 472 part 815. |
|||
CTE, linear, Parallel to Flow | 70.0 µm/m-°C @Temperature 23.0 - 85.0 °C |
38.9 µin/in-°F @Temperature 73.4 - 185 °F |
ISO 11359 |
Solvay TECHNYL® A 402H1 Natural PA66, DRY Description: TECHNYL® A 402H1 is an unreinforced polyamide 66, very high viscosity, heat stabilized, for extrusion and injection molding. This product is available in natural color.Benefits: The .. |
|||
CTE, linear, Parallel to Flow | 70.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
38.9 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics NORYL PX1181 PPE+HIPS (Europe-Africa-Middle East) Noryl* PX1181 PolyPhenylene Oxide (PPO*) + Polystyrene (PS) resin is an unfilled , injection moldable grade, with improved impact performances, an ISO 306 Vicat B/120 temperature of 120 deg C and a .. |
|||
CTE, linear, Parallel to Flow | 70.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
38.9 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics NORYL N110 PPE+HIPS (Europe-Africa-Middle East) NORYL N110 is an unfilled material, with a Vicat B/120 of 115 °C according ISO 306. NORYL N110 has medium temperature resistance and good |
|||
CTE, linear, Parallel to Flow | 70.0 µm/m-°C @Temperature 20.0 °C |
38.9 µin/in-°F @Temperature 68.0 °F |
|
Covestro Apec® HT KU 1-9371 High-Heat Polycarbonate Transparent and opaque shades possible.Applications: Lighting, automotive and household goods, light covers.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was separated .. |
|||
CTE, linear, Parallel to Flow | 70.0 µm/m-°C @Temperature 23.0 - 55.0 °C |
38.9 µin/in-°F @Temperature 73.4 - 131 °F |
ISO 11359-1,-2 |
Covestro Bayblend® M850 XF PC/ABS Blend Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Injection molding• Eas.. |
|||
CTE, linear, Parallel to Flow | 70.0 µm/m-°C @Temperature 20.0 °C |
38.9 µin/in-°F @Temperature 68.0 °F |
|
Covestro Makrolon® 2803 Polycarbonate, Injection Grade Medium flowing injection molding grade with UV stabilizer.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name .. |
|||
CTE, linear, Parallel to Flow | 70.0 µm/m-°C @Temperature 20.0 °C |
38.9 µin/in-°F @Temperature 68.0 °F |
|
Covestro Makrolon® 2805 Polycarbonate, Injection Grade Medium flowing injection molding grade with easy mold release, Makrolon grade 2858 for food contact applications.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was separ.. |
|||
CTE, linear, Parallel to Flow | 70.0 µm/m-°C @Temperature 20.0 °C |
38.9 µin/in-°F @Temperature 68.0 °F |
|
Covestro Makrolon® 3103 Polycarbonate Injection molding and extrusion grade with high viscosity, UV stabilized, special grade for sheets.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was separated from Baye.. |
|||
CTE, linear, Parallel to Flow | 70.0 µm/m-°C | 38.9 µin/in-°F | ISO 11359-1/-2 |
Covestro Makrolon® T7855 Polycarbonate, Impact Grade ISO 7391-PC,MPR,(,,)-18-9Global gradeMVR (300 °C/1.2 kg) 12 cm3/10 minImpact modifiedMedium viscosityEasy releaseInjection molding - Melt temperature 280 - 320 °CAvailable in opaque colors onlyPre.. |
|||
CTE, linear, Parallel to Flow | 70.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
38.9 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
Eurostar Staramide B40 PA6, Extrusion Staramide B40 is High Viscosity, Unreinforced Polyamide 6, Extrusion ResinInformation provided by Eurostar. |
|||
CTE, linear, Parallel to Flow | 70.0 µm/m-°C @Temperature 20.0 °C |
38.9 µin/in-°F @Temperature 68.0 °F |
|
Covestro Apec® 1805 Polycarbonate
(discontinued **) Key Features:Release agentUnfilledSuitable processing methods:Injection moldingFilm extrusionProfile extrusionSheet extrusionCoatingBlow moldingCalanderingTransfer moldingThermoformingInformation pr.. |
|||
CTE, linear, Parallel to Flow | 70.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
38.9 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-1/-2 |
Styrolution Luran® 368 R Crystal Clear Transparent 77851 SAN Description: General-purpose grade with well-balanced properties, suitable for injection molding and extrusion. Especially for applications where highest transparency and low natural color is requir.. |